Manufacture and characterisation of a low cost carbon fibre reinforced C/SiC dual matrix composite

被引:65
|
作者
Odeshi, A. G. [1 ]
Mucha, H.
Wielage, B.
机构
[1] Univ Manitoba, Dept Mech & Mfg Engn, Winnipeg, MB R3T 5V6, Canada
[2] Tech Univ Chemnitz, Inst Composite Mat & Surface Technol, D-09107 Chemnitz, Germany
关键词
carbon composites; pyrolysis; dynamic mechanical thermal analysis; mechanical properties; DYNAMIC-MECHANICAL ANALYSIS; SILICON-CARBIDE; ROUTE;
D O I
10.1016/j.carbon.2006.01.025
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A porous two-dimensional C/C composite was produced via the polymer pyrolysis route using phenolic resin as the matrix precursor and polyacrilonitrile- (PAN-) or pitch-based carbon fibres as reinforcement. The resulting C/C composites were then densified using a modified polysilane followed by pyrolysis to convert the polymer into silicon carbide, sealing the pores in the C/C composite. Aiming to increase the ceramic yield of the infiltrated polysilane and to reduce its volumetric shrinkage during pyrolysis the polymer's curing behaviour was modified by catalytic addition of 0.1% dicobaltoctacarbonyl [Co-2(CO)(8)]. The densification procedure is very efficient in sealing cracks in the C/C composite with SiC. The obtained carbon fibre reinforced C/SiC dual matrix composites were subjected to flexural tests and dynamic mechanical analysis. The flexural and visco-clastic properties of the composite are dominated by the strength of the fibre/matrix interface rather than by the fibre strength or modulus. A correlation between the mechanical loss factor (tan delta) and the fracture behaviour of the composite is suggested. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1994 / 2001
页数:8
相关论文
共 50 条
  • [21] Preparation and tribological properties of C fibre reinforced C/SiC dual matrix composites fabrication by liquid silicon infiltration
    Li, Zhuan
    Xiao, Peng
    Xiong, Xiang
    Huang, Bo-yun
    SOLID STATE SCIENCES, 2013, 16 : 6 - 12
  • [22] Nanoindentation, microscratch, friction and wear studies of carbon-fibre reinforced SiC-Si matrix composite
    Fouquet, S
    Jouannigot, S
    Alexis, J
    Pailler, R
    Bourrat, X
    Guette, A
    Naslain, R
    EURO CERAMICS VIII, PTS 1-3, 2004, 264-268 : 917 - 920
  • [23] Damage Characterisation of Carbon Fibre Reinforced Composite Plate Using Acoustic Emission
    Mohammed, Bizuayehu Y.
    Tan, Chee K.
    Wilcox, Steven J.
    Chong, Alex Z. S.
    STRUCTURAL HEALTH MONITORING: RESEARCH AND APPLICATIONS, 2013, 558 : 184 - +
  • [24] Characterisation of voids in fibre reinforced composite materials
    Little, John Eric
    Yuan, Xiaowen
    Jones, Mark Ian
    NDT & E INTERNATIONAL, 2012, 46 : 122 - 127
  • [25] Fracture behaviour and toughness of a plane-woven SiC fibre-reinforced SiC matrix composite
    Goto, K
    Kagawa, Y
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 211 (1-2): : 72 - 81
  • [26] Effect of PIP cycles on fracture behaviour in unidirectional SiC fibre-reinforced SiC matrix composite
    Kakisawa, H.
    Kagawa, Y.
    Takeda, M.
    Imai, Y.
    Ichikawa, H.
    Advanced Composites Letters, 8 (03): : 109 - 115
  • [27] Fracture behaviour and toughness of a plane-woven SiC fibre-reinforced SiC matrix composite
    Univ of Tokyo, Tokyo, Japan
    Mater Sci Eng A Struct Mater Prop Microstruct Process, 1-2 (72-81):
  • [28] Effect of PIP cycles on fracture behaviour in unidirectional SiC fibre-reinforced SiC matrix composite
    Kakisawa, H
    Kagawa, Y
    Takeda, M
    Imai, Y
    Ichikawa, H
    ADVANCED COMPOSITES LETTERS, 1999, 8 (03) : 109 - 115
  • [29] Development and characterization of liquid carbon fibre reinforced aluminium matrix composite
    Shalu, T.
    Abhilash, E.
    Joseph, M. A.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (10) : 4809 - 4813
  • [30] Oxidation behaviour of carbon short fibre reinforced C/SiC composites
    Raether, Friedrich
    Meinhardt, Jurgen
    Kienzle, Andreas
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (2-3) : 1217 - 1221