Effect of tension on corrosive and thermal properties of Cu60Zr30Ti10 metallic glass

被引:9
|
作者
An, W. K. [1 ]
Cai, A. H. [1 ,2 ]
Xiong, X. [2 ]
Liu, Y. [2 ]
Zhou, G. J. [1 ]
Luo, Y. [1 ]
Li, T. L. [1 ]
Li, X. S. [1 ]
机构
[1] Hunan Inst Sci & Technol, Coll Mech Engn, Yueyang 414000, Peoples R China
[2] Cent S Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
关键词
Cu60Zr30Ti10 metallic glasses; Thermal property; Corrosion; CU-ZR-TI; MECHANICAL-PROPERTIES; FORMING ABILITY; CHLORIDE MEDIA; BEHAVIOR; RESISTANCE; ALLOY; STRESS; HF; PLASTICITY;
D O I
10.1016/j.jallcom.2013.01.187
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cu60Zr30Ti10 (at.%) glassy ribbon was prepared by melt spinning. The effect of the tension on its thermal and corrosive properties was investigated by differential scanning calorimetry and electrochemical polarization experiments, respectively. The glass transition temperature T-g, onset crystallization temperature T-x, and crystallization peak temperature T-p increase with increasing heating rate, but the increasing rate of these temperatures is larger for low heating rate (5-20 K min(-1)) than for rapid heating rate (20-80 K min(-1)) for the as-cast and tensile ribbons. The T-g for the tensile ribbon is smaller than that for the as-cast one in studied heating rates. The T-x and the T-p for the tensile ribbon are smaller than those for the a-cast ribbon when the heating rate is less than 80 K min(-1), while inversely when the heating rate reaches up to 80 K min(-1). There is a critical heating rate for the characteristic temperatures of the tensile ribbon surpassing those of the as-cast one. The heating rates are estimated to be 114.7 K min(-1) for T-g, 65.3 K min(-1) for T-x, and 64.9 K min(-1) for T-p, respectively. In addition, the activation energies for the glass transition and the crystallization decrease. On the other hand, the corrosion potential is larger in 0.5 M H2SO4 than in 1 M chloride-ion-containing solutions for the as-cast and tensile specimens. However, the corrosion current density is smaller in the former than in the latter for the tensile and as-cast specimens. After the tension, the corrosion potential sharply increases in 0.5 M H2SO4 and decreases in 1 M chloride-ion-containing solutions. The passive potential decreases and the pitting corrosion can be observed in 0.5 M H2SO4. The potential for the sharp decrease of the current density decreases in 1 M HCl, and maintains almost the same in 1 M NaCl. The corroded surface micrographs in all studied solutions are remarkably changed. In addition, the difference of corrosive behavior in 0.5 M H2SO4, 1 M HCl, and 1 M NaCl is also discussed. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:55 / 62
页数:8
相关论文
共 50 条
  • [21] Effects of annealing temperature on microstructure and hardness of (Cu60Zr30Ti10)98Y2 bulk metallic glass
    Zha Guilan
    Zhang Aisheng
    JOURNAL OF RARE EARTHS, 2010, 28 (02) : 243 - 245
  • [22] Crystallisation behaviour of CU60Zr30Ti10, bulk glassy alloy
    Kasai, M
    Matsubara, E
    Saida, J
    Nakayama, M
    Uematsu, K
    Zhang, T
    Inoue, A
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 375 : 744 - 748
  • [23] High pressure torsion of amorphous Cu60Zr30Ti10 alloy
    Hobor, Sandor
    Revesz, Adam
    Szabo, Peter J.
    Zhilyaev, Alex P.
    Kis, Viktoria Kovacs
    Labar, Janos L.
    Kovacs, Zsolt
    JOURNAL OF APPLIED PHYSICS, 2008, 104 (03)
  • [24] Influence of nanoprecipitation on strength of Cu60Zr30Ti10 glass containing μm-ZrC particle reinforcements
    Kato, H
    Yubuta, K
    Louzguine, DV
    Inoue, A
    Kim, HS
    SCRIPTA MATERIALIA, 2004, 51 (06) : 577 - 581
  • [25] Study on Crystallization Behavior in (Cu60Zr30Ti10)98Y2 Bulk Metallic Glass by Differential Scanning Calorimeter (DSC)
    Zhang, Aisheng
    Zha, Guilan
    ADVANCES IN CHEMISTRY RESEARCH II, PTS 1-3, 2012, 554-556 : 76 - 80
  • [26] 块状非晶合金Cu60Zr30Ti10的激光熔凝研究
    黄钧声
    杨元政
    陶平均
    吴启梁
    郑善
    包渠平
    林晓聪
    特种铸造及有色合金, 2007, (06) : 411 - 412+405
  • [27] Microstructure feature of bulk glassy Cu60Zr30Ti10 alloy in As-cast and annealed states
    Chen, YT
    Zhang, T
    Zhang, W
    Ping, DH
    Hono, K
    Inoue, A
    Sakurai, T
    MATERIALS TRANSACTIONS, 2002, 43 (10) : 2647 - 2650
  • [28] Dynamics of a bulk metallic glass CU60Zr20Hf10Ti10
    Agarwal, PC
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 404 (1-2): : 301 - 304
  • [29] Oxidation-induced copper segregation in Cu60Zr30 Ti10 bulk metallic glass
    Tam C.Y.
    Shek C.H.
    Journal of Materials Research, 2006, 21 (4) : 851 - 855
  • [30] Enhancement of solderability of Cu60Zr30Ti 10 bulk metallic glass by dealloying in hydrofluoric acid solution
    Naoi T.
    Nishikawa H.
    Takemoto T.
    Abe H.
    Fukuhara M.
    Inoue A.
    Yosetsu Gakkai Ronbunshu/Quarterly Journal of the Japan Welding Society, 2011, 29 (03): : 147s - 150s