Microstructure and Mechanical Properties of Selective Laser Melted Reduced Activation Ferritic/Martensitic Steel

被引:1
|
作者
Yuan, Zihao [1 ]
Xiao, Chenyu [1 ]
Liu, Hao [1 ]
Sun, Xuejing [1 ]
Zhao, Guangyi [1 ]
Liao, Hongbin [1 ]
Qian, Wei [1 ]
Yuan, Jingkun [2 ]
Lao, Changshi [2 ]
Wang, Huajie [1 ]
机构
[1] Southwestern Inst Phys, Huangjing Rd 5, Chengdu 610041, Peoples R China
[2] Shenzhen Univ, Addit Mfg Inst, Coll Mechatron & Control Engn, Shenzhen 518060, Peoples R China
关键词
CLF-1; steel; selective laser melting; process parameters; microstructure; mechanical properties; PRECIPITATION BEHAVIOR; COMPONENTS; PROGRESS;
D O I
10.3390/met12122044
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Cube and tensile samples of reduced activation ferritic/martensitic steel were formed at different laser powers and scanning velocities using a selective laser melting process; the microstructural characteristics and tensile properties of the cube and tensile samples were investigated in this study. The experimental results showed that the SLMed CLF-1 samples that formed with selected laser melting were near-fully dense, and the relative density of the SLMed CLF-1 samples exceeded 99%. Meanwhile, there were numerous nano-sized spherical and needle-like precipitate dispersions distributed in the grains and boundary of the grains, and the precipitates were mainly composed of M23C6 carbide and MX carbide. The microstructure was composed of columnar grains and equiaxed grains arranged in a sequence, and the smallest average size of the grains was 15 +/- 2.1 mu m when measured at 320 W of power and 800 mm/s scanning velocity. In addition, the sample at 320 W of power and 800 mm/s scanning velocity exhibited higher yield strength (875 +/- 6.0 MPa) and higher elongation (25.6 +/- 0.8%) than that of the sample at 200 W of power, 800 mm/s scanning velocity, yield strength of 715 +/- 1.5 MPa, and elongation of 22.6 +/- 1.2%.
引用
收藏
页数:9
相关论文
共 50 条
  • [31] Effects of yttrium and zirconium additions on inclusions and mechanical properties of a reduced activation ferritic/martensitic steel
    Zhan, Dong-ping
    Qiu, Guo-xing
    Li, Chang-sheng
    Qi, Min
    Jiang, Zhou-hua
    Zhang, Hui-shu
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2020, 27 (02) : 197 - 207
  • [32] Microstructure and mechanical properties of selective laser melted 18Ni300 steel
    Liang, Yan
    Qing, Luo
    Yu, He
    Huili, Zhao
    Yuxin, Wang
    Materials Science- Poland, 2022, 40 (03) : 64 - 71
  • [33] Effects of Y and Ti addition on microstructure stability and tensile properties of reduced activation ferritic/martensitic steel
    Qiu, Guoxing
    Zhan, Dongping
    Li, Changsheng
    Qi, Min
    Jiang, Zhouhua
    Zhang, Huishu
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2019, 51 (05) : 1365 - 1372
  • [34] Microstructure and mechanical properties of Selective Laser Melted 18Ni-300 steel
    Kempen, K.
    Yasa, E.
    Thijs, L.
    Kruth, J. -P.
    Van Humbeeck, J.
    LASERS IN MANUFACTURING 2011: PROCEEDINGS OF THE SIXTH INTERNATIONAL WLT CONFERENCE ON LASERS IN MANUFACTURING, VOL 12, PT A, 2011, 12 : 255 - 263
  • [35] Microstructure and mechanical properties of selective laser melted 18Ni300 steel
    Liang, Yan
    Qing, Luo
    Yu, He
    Huili, Zhao
    Yuxin, Wang
    MATERIALS SCIENCE-POLAND, 2022, 40 (03): : 64 - 71
  • [36] Microstructure and mechanical properties of laser beam welded joints of China low-activation ferritic/martensitic steel with cerium addition
    Gong, Jialin
    Wang, Xiaoyu
    Liao, Hongbin
    Zhang, Kuan
    FUSION ENGINEERING AND DESIGN, 2021, 170 (170)
  • [37] Thermal and mechanical behaviour of the reduced-activation-ferritic-martensitic steel EUROFER
    Lindau, R
    Möslang, A
    Schirra, M
    FUSION ENGINEERING AND DESIGN, 2002, 61-62 : 659 - 664
  • [38] Novel core-layer-shell structured nano-composite precipitates formed in selective laser melted reduced activation ferritic-martensitic steel
    Yang, Tao
    Chai, Linjiang
    Tang, Yi
    Wu, Yu
    Tan, Xiaolian
    Murty, Korukonda L.
    MATERIALS TODAY COMMUNICATIONS, 2024, 41
  • [39] Effect of irradiation on the microstructure and the mechanical properties of oxide dispersion strengthened low activation ferritic/martensitic steel
    Ramar, A.
    Baluc, N.
    Schaeublin, R.
    JOURNAL OF NUCLEAR MATERIALS, 2007, 367 : 217 - 221
  • [40] Effect of concentrations of Ta and Ti on microstructure and mechanical properties of 9Cr-1W reduced activation ferritic/martensitic steel
    Kim, Byoung-Hwan
    Moon, Joonoh
    Kim, Sung-Dae
    Jang, Jae-Hoon
    Lee, Tae-Ho
    Hong, Hyun-Uk
    Kim, Hyoung Chan
    Cho, Kyung-Mox
    Lee, Chang-Hoon
    FUSION ENGINEERING AND DESIGN, 2020, 151