High-temperature corrosion of martensitic and austenitic steels under on-tube oil shale ash deposits

被引:0
|
作者
Tallermo, H [1 ]
Klevtsov, I [1 ]
机构
[1] Tallinn Univ Technol, Dept Thermal Engn, EE-11712 Tallinn, Estonia
关键词
D O I
暂无
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Superheater surfaces in oil shale steam boilers, constructed from pearlitic or austenitic steels, are subject to intensive corrosion, primarily due to the presence of chlorine in external deposits. The applicability of martensitic steels ei-756, X10CrMoVNb9-1 and X20CrMoV12-1 for superheaters has been examined, and empirical equations for prediction of steel corrosion depth have been developed for the operational temperature range. An abnormal dependence of corrosion depth of martensitic steels on temperature is revealed, namely that corrosion in the presence of oil shale fly ash is more intensive at 580 degreesC than at 620 degreesC. On the basis of laboratory testing it was found that steel X10CrMoVNb9-1 is highly suitable for superheaters of boilers firing fossil fuels containing alkaline metals and chlorine.
引用
收藏
页码:19 / 33
页数:15
相关论文
共 50 条
  • [41] HIGH-TEMPERATURE AISI 310 AUSTENITIC STAINLESS STEELS.
    Ohmori, Y.
    Maehara, Y.
    Materials Science and Technology, 1986, 2 (06) : 595 - 602
  • [42] Temperature Dependence of Corrosion of Ferritic/Martensitic and Austenitic Steels in Liquid Lead-Bismuth Eutectic
    Kurata, Yuji
    Saito, Shigeru
    MATERIALS TRANSACTIONS, 2009, 50 (10) : 2410 - 2417
  • [43] INFLUENCE OF ALLOYING ON PROPERTIES AND STRUCTURE OF AUSTENITIC HIGH-TEMPERATURE STEELS
    LEVITIN, VV
    GRABOVSKII, VY
    KOROSTELEV, VF
    RYVKIN, YA
    STEEL IN THE USSR, 1978, 8 (10): : 580 - 582
  • [44] Structure and Properties of High-Temperature Austenitic Steels for Superheater Tubes
    Blinov, V. M.
    RUSSIAN METALLURGY, 2009, (06): : 478 - 487
  • [45] HIGH-TEMPERATURE OXIDATION OF COMMERCIAL AUSTENITIC STAINLESS-STEELS
    STOTT, FH
    WEI, FI
    MATERIALS SCIENCE AND TECHNOLOGY, 1989, 5 (11) : 1140 - 1147
  • [46] Characteristics of the high-temperature strength of austenitic steels strengthened with carbides
    Kositsyna, II
    Kochetkova, TN
    PHYSICS OF METALS AND METALLOGRAPHY, 2003, 96 (03): : 321 - 332
  • [47] High-temperature dynamic corrosion mechanisms of austenitic stainless and carbon steels in nitrates for concentrating solar power
    Yang, Pu
    Deng, Zhongyue
    Chen, Bingqing
    Wang, Yueshe
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2024, 266
  • [48] Enhanced high-temperature strength of austenitic steels by nanotwins and nanoprecipitates
    Liu, D. Y.
    Shen, Z. L.
    Ren, C. X.
    Li, Q.
    Tao, N. R.
    SCRIPTA MATERIALIA, 2024, 242
  • [49] HIGH-TEMPERATURE OXIDATION BEHAVIOR OF AUSTENITIC STAINLESS-STEELS
    HALES, R
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1978, 29 (06): : 393 - 399
  • [50] Laboratory tests of high-temperature corrosion of steels B-407, X8CrNiNb1613 and X8CrNiMoNb1616 under impact of ash formed at pulverized firing of oil shale
    Tallermo, H
    Klevtsov, I
    Bojarinova, T
    Dedov, A
    OIL SHALE, 2005, 22 (04) : 467 - 474