Formation of Fine Spheroidal Microstructure of Semi-Solid Al-Zn-Mg-Cu Alloy by Hyperthermally and Subsequent Isothermally Reheating

被引:8
|
作者
Chen, Gang [1 ]
Jiang, Jufu [1 ]
Du, Zhiming [1 ]
Cao, Qi [1 ]
Li, Hongwei [2 ,3 ]
Zhang, Xin [2 ,3 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Beijing North Vehicle Grp Corp, Inst Technol, Beijing 100072, Peoples R China
[3] Beijing Engn Res Ctr Adv Mfg & Elevat Special Veh, Beijing 100072, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-Zn-Mg-Cu alloys; Microstructure; Semisolid; Recrystallization; TENSILE MECHANICAL-PROPERTIES; AZ91D MAGNESIUM ALLOY; ALUMINUM-ALLOY; EVOLUTION; STATE; ECAE; 7075-ALUMINUM-ALLOY; RECRYSTALLIZATION; EXTRUSION;
D O I
10.1016/j.jmst.2013.05.008
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The high strength 7xxx series aluminium alloys are usually difficult to be prepared as semi-solid feedstock, because some dispersoid particles (soluble only in liquid) could pin at grain and subgrain boundary to make the alloy difficultly recrystallise. In this work, a novel multistep reheating regime is developed for recrystallisation and partial melting (RAP) route to prepare fine spheroidal microstructure of semi-solid Al-Zn-Mg-Cu alloy. After reheating to 665 degrees C, holding for 4 min and subsequent isothermally holding at 620 degrees C with total heating time of 15 min, fine spheroidal microstructures with grain size of similar to 40 mu m were prepared without remained unrecrystallised grains and directionality, which are much finer than the conventionally obtained microstructures (similar to 100 mu m).
引用
收藏
页码:979 / 982
页数:4
相关论文
共 50 条
  • [21] Microstructure of spray formed Al-Zn-Mg-Cu alloy with Mn addition
    Cai Yuan-hua
    Liang Rui-guang
    Su Zhan-pei
    Zhang Ji-shan
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (01) : 9 - 14
  • [22] Effect of Thermomechanical Treatment on Microstructure and Properties of Al-Zn-Mg-Cu Alloy
    Zhang, Weijian
    Su, Ruiming
    Li, Guanglong
    Qu, Yingdong
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2025, 78 (05)
  • [23] Microstructure of Al-Zn-Mg-Cu aluminum alloy strengthened by yttrium element
    Li G.
    Zhao Y.
    Li J.
    Wang H.
    Chen G.
    Jiangsu Daxue Xuebao (Ziran Kexue Ban) / Journal of Jiangsu University (Natural Science Edition), 2010, 31 (01): : 49 - 52
  • [24] Effect of microstructure on stress corrosion cracking of an Al-Zn-Mg-Cu alloy
    Puiggali, M
    Zielinski, A
    Olive, JM
    Renauld, E
    Desjardins, D
    Cid, M
    CORROSION SCIENCE, 1998, 40 (4-5) : 805 - 819
  • [25] Interactions between microstructure and plastic instabilities in Al-Zn-Mg-Cu alloy
    Thevenet, D
    Mliha-Touati, M
    Zeghloul, A
    ZEITSCHRIFT FUR ANGEWANDTE MATHEMATIK UND MECHANIK, 2000, 80 : S459 - S460
  • [26] Synthesis and microstructure of nanocrystalline Al-Zn-Mg-Cu alloy powders by cryomilling
    State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083, China
    不详
    Beijing Keji Daxue Xuebao, 2006, 9 (845-849):
  • [27] Influence of Zr on the microstructure and mechanical properties of an Al-Zn-Mg-Cu alloy
    Yang, Shoujie
    Xie, Youhua
    Dai, Shenglong
    Yan, Minggao
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 1069 - +
  • [28] Deformation and microstructure characterization during semi-solid extrusion of Al-4Cu-Mg alloy
    卢雅琳
    李淼泉
    李兴成
    TransactionsofNonferrousMetalsSocietyofChina, 2006, (S3) : 1606 - 1609
  • [29] Deformation and microstructure characterization during semi-solid extrusion of Al-4Cu-Mg alloy
    Lu Ya-lin
    Li Miao-quan
    Li Xing-cheng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1606 - S1609
  • [30] Semi-solid ZnAl 27 alloy and its microstructure after reheating
    Song, Jian-Li
    You, Xiao-Hong
    Li, Tian-You
    Lou, Shuai
    Jinshu Rechuli/Heat Treatment of Metals, 2002, 27 (10):