Fracture behaviour of laser-welded 2219-T6 aluminium alloy under pulsed Lorentz force

被引:16
|
作者
Zhu, Hui [1 ]
Huang, Liang [1 ]
Wang, Zeyu [1 ]
Li, Jianjun [1 ]
Ma, Huijuan [1 ,2 ]
Su, Hongliang [1 ]
机构
[1] Huazhong Univ Sci & Technol, State Key Lab Mat Proc & Die & Mould Technol, Sch Mat Sci & Engn, Wuhan 430074, Hubei, Peoples R China
[2] Wuhan Univ Technol, Hubei Key Lab Adv Technol Automot Components, Wuhan 430070, Hubei, Peoples R China
基金
中国国家自然科学基金;
关键词
ELECTRICAL-CONDUCTIVITY; FORMING LIMITS; STRAIN-RATE; MICROSTRUCTURE; FORMABILITY; MECHANISM; SHEET; COIL;
D O I
10.1007/s10853-019-03588-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Electromagnetic forming is a high-speed forming technology, using pulsed Lorentz force to make sheet metal deformed. The fracture behaviour of material during electromagnetic forming is a significant scientific issue in the development of this technology. In the current work, experimental methods are used to investigate the properties and microstructure of laser-welded 2219-T6 aluminium alloy and the fracture behaviour of the weld joint under pulsed Lorentz force. The results indicate that the hardness, strength, ductility, impact toughness of the laser-welded joint are all worse than that of the base metal because of the inhomogeneity of the microstructure and the existence of coarse brittle eutectic phases. This leads to the ductile fracture of laser-welded joint at the initial stage, followed by the sparking and partially melting breaking phenomena, under the pulsed Lorentz force. The molten structure is also observed on the fracture surface of the weld joint after electromagnetic tensile test rather than mechanical high-speed tensile test. During the fracture process under pulsed Lorentz force, local short circuits occur at the ductile crack tip of the weld joint due to the eddy current effect, resulting in the melting of the weld metal. The percentage reduction of area and the dimple sizes in the fracture morphology of the specimen under the conditions of high-speed deformation are larger than that under the condition of quasi-static tensile test, indicating the slight improvement in ductility of the laser-welded joint under high-speed deformation due to the inertial effect and the adiabatic temperature rise from the plastic work. Particularly, the above indicators are even larger under electromagnetic tensile test, revealing extra very slight increase in ductility compared with mechanical high-speed tensile test because of the body force and the additional temperature rise resulting from the Joule heat.
引用
收藏
页码:9857 / 9874
页数:18
相关论文
共 50 条
  • [41] Potentiodynamic Corrosion Behavior and Microstructural Characteristics of Pulsed CMT-Welded AA2014-T6 Aluminium Alloy Joints: Effect of PWHT
    Rao, A. Padma
    Hadi, Manzoor
    Rajendran, C.
    Tushar, Sonar
    Ivanov, Mikhail
    Kumar, P. Senthil
    Krishna, V. Murali
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2022, 2022
  • [42] Microstructure and Mechanical Properties of Laser Welded 6061-T6 Aluminum Alloy under High Strain Rates
    Nie, Jincheng
    Li, Shengci
    Zhong, Huilong
    Hu, Changjing
    Lin, Xiangsong
    Chen, Jiqiang
    Guan, Renguo
    METALS, 2020, 10 (09) : 1 - 13
  • [43] Effect of laser-arc hybrid welding on fracture and corrosion behaviour of AA6061-T6 alloy
    Zhang, Da-Quan
    Jin, Xin
    Gao, Li-Xin
    Joo, Hyung Goun
    Lee, Kang Yong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (06): : 2748 - 2754
  • [44] Effect of pre/post T6 heat treatment on the mechanical properties of laser welded SSM cast A356 aluminium alloy
    Akhter, R.
    Ivanchev, L.
    Burger, H. P.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 447 (1-2): : 192 - 196
  • [45] Fretting fatigue behaviour of a 2014-T6 aluminium alloy coated with an electroless nickel under rotating bending loading
    Sadeler, R.
    Atasoy, S.
    Altun, H.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2009, 47 (02): : 95 - 100
  • [46] Investigation of the Effect of Tool Temperature on Microstructure, Hardness, and Wear Behaviour of Aluminium 6061-T6 Alloy Welded by the Friction Stir Welding Process
    Pita M.
    Material Design and Processing Communications, 2023, 2023
  • [47] Comparative study on torsional strength, ductility and fracture characteristics of laser-welded α plus β Ti-6Al-7Nb alloy, CP Titanium and Co-Cr alloy dental castings
    Srimaneepong, Viritpon
    Yoneyama, Takayuki
    Kobayashi, Equo
    Doi, Hisashi
    Hanawa, Takao
    DENTAL MATERIALS, 2008, 24 (06) : 839 - 845
  • [48] Investigation of Parametric Influences During the Cutting of Contours in 6061-T6 Aluminium Alloy Sheet Using a Pulsed Nd:YAG Laser
    Joshi, P.
    Sharma, A.
    LASERS IN ENGINEERING, 2020, 45 (1-3) : 35 - 68
  • [49] Microstructure evolution and fracture behaviour of friction stir welded 6061-T6 thin plate joints under high rotational speed
    Liu, F. J.
    Fu, L.
    Chen, H. Y.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2018, 23 (04) : 333 - 343
  • [50] Flexural behaviour of 7A04-T6 high-strength aluminium alloy SHS and RHS beams under moment gradient
    Li, Beibei
    Wang, Yuanqing
    Zhang, Ying
    Yuan, Huanxin
    Zhi, Xinhang
    Baniotopoulos, Charalampos C.
    ENGINEERING STRUCTURES, 2022, 259