Experimental investigation into the size effect on the microscale fatigue behaviour of 316L stainless steel

被引:12
|
作者
Donnelly, E. [1 ]
Weafer, F. M. [1 ]
Connolley, T. [1 ]
McHugh, P. E. [1 ]
Bruzzi, M. S. [1 ]
机构
[1] Natl Univ Ireland Galway, Coll Engn & Informat, Galway, Ireland
关键词
Fatigue; Size effect; 316L stainless steel; Strain localization; COMPONENTS; STENTS;
D O I
10.1016/j.ijfatigue.2016.10.007
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This study focuses on the microscale fatigue properties of 316L stainless steel. This material is commonly used in the manufacture of medical devices such as stents, which, once implanted, are subjected to hundreds of millions of fatigue cycles. Fatigue testing was carried out on 50 gm, 75 mu m,100 gm and 150 gm 316L specimens with 60 gm thickness. A size effect was shown to exist in the form of a reduced fatigue endurance limit of the 50 gm specimens. In order to determine the cause of this size effect, the outer surfaces and fracture surfaces of failed test specimens were examined using Scanning Electron Microscopy (SEM) techniques. These SEM studies suggest that the process of strain localization was occurring in the specimens and was most pronounced in the 50 gm specimens. The experimentally established surface roughness of the test specimens, measured using white-light interferometry, further confirmed the SEM observation. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1 / 7
页数:7
相关论文
共 50 条
  • [31] Fatigue behavior of Austenitic Type 316L Stainless Steel
    Mohammad, K. A.
    Ali, Aidy
    Sahari, B. B.
    Abdullah, S.
    1ST INTERNATIONAL CONFERENCE ON MECHANICAL ENGINEERING RESEARCH 2011 (ICMER2011), 2012, 36
  • [32] Effect of hold-time on low cycle fatigue behaviour of nitrogen bearing 316L stainless steel
    Materials Development Group, Indira Gandhi Ctr. Atom. R., Kalpakkam, India
    不详
    Int. J. Press. Vessels Pip., 12 (863-870):
  • [33] Effect of surface carbonitriding by plasma immersion ion implantation on the fatigue behaviour of 316L austenitic stainless steel
    Obrtlík, K
    Jirásková, Y
    Man, J
    Polák, J
    COMPUTER METHODS AND EXPERIMENTAL MEASUREMENTS FOR SURFACE EFFECTS AND CONTACT MECHANICS VII, 2005, 49 : 13 - 22
  • [34] Corrosion behaviour of 316L stainless steel in PTA slurry
    Ju, P. F.
    Zuo, Y.
    Tang, J. L.
    Tang, Y. M.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2013, 48 (03) : 207 - 210
  • [35] Behaviour of 316L Stainless Steel in Simulated Physiological Fluids
    Poinescu, Aurora Anca
    Ion, Rodica-Mariana
    Ionita, Ionica
    Dulama, Ioana Daniela
    Chilian, Andrei
    REVISTA DE CHIMIE, 2014, 65 (11): : 1351 - 1356
  • [36] Grain growth behaviour of type 316L stainless steel
    Kashyap, B.P.
    Tangri, K.
    Materials Science and Engineering A, 1992, A149 (02)
  • [37] An experimental study of crevice corrosion behaviour of 316L stainless steel in artificial seawater
    Cai, Baoping
    Liu, Yonghong
    Tian, Xiaojie
    Wang, Fei
    Li, Hang
    Ji, Renjie
    CORROSION SCIENCE, 2010, 52 (10) : 3235 - 3242
  • [38] Strain hardening behaviour of 316L austenitic stainless steel
    Singh, KK
    MATERIALS SCIENCE AND TECHNOLOGY, 2004, 20 (09) : 1134 - 1142
  • [39] Experimental investigation of structural behavior of 316L stainless steel and carbon steel slit dampers
    Hwang, BoKyung
    Kim, TaeSoo
    Ahn, YongHan
    THIN-WALLED STRUCTURES, 2023, 186
  • [40] Low cycle fatigue behaviour of a nitrogen modified 316L stainless steel at 823 K
    Srinivasan, VS
    Valsan, M
    Rao, KBS
    Mannan, SL
    Sastry, DH
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 1996, 49 (04): : 489 - 495