In order to investigate the effect of texture variation on the delayed hydride cracking behavior in Zr-2.5%Nb plates, crack growth rate and K-IH tests have been carried out at temperature ranges varying from 415 to 506 K after texture modification by rolling. The texture variation of plates was achieved by direct-rolling and cross-rolling. Texture was measured through the determination of inverse pole figures, from which the basal pole components were calculated. The results have shown that the texture of a plate in which the basal poles are concentrated in the transverse direction can be changed significantly by cross-rolling. The crack growth rate increases exponentially with the basal pole component in the direction normal to the cracking plane. The increase in stress relieving temperature on cold worked material reduces crack growth rate. K-IH decreases linearly with the basal pole component, and a behavior of which could be explained by the uniformly dispersed aggregate composite theory. (C) 1999 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:52 / 59
页数:8
相关论文
共 50 条
  • [1] The effect of texture on delayed hydride cracking in Zr-2.5Nb alloy
    Levi, MR
    Sagat, S
    [J]. ENVIRONMENTAL DEGRADATION OF MATERIALS AND CORROSION CONTROL IN METALS, 1999, : 323 - 335
  • [2] Hydride morphology and striation formation during delayed hydride cracking in Zr-2.5% Nb
    Shek, GK
    Jovanovic, MT
    Seahra, H
    Ma, Y
    Li, D
    Eadie, RL
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1996, 231 (03) : 221 - 230
  • [3] Temperature dependence of the velocity of delayed hydride cracking in Zr-2.5% Nb Alloy
    Markelov V.A.
    Kotov P.V.
    Zheltkovskaya T.N.
    [J]. Inorganic Materials: Applied Research, 2010, 1 (3) : 217 - 224
  • [4] EFFECT OF HEAT-TREATMENT ON DELAYED HYDRIDE CRACKING IN ZR-2.5 WT PCT NB
    AMOUZOUVI, KF
    CLEGG, LJ
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1987, 18 (10): : 1687 - 1694
  • [5] The delayed hydride cracking avoidance manoeuvre for Zr-2.5 Nb pressure tube alloy
    Yan, D
    Sun, S
    Eadie, RL
    Shek, GK
    Seahra, H
    [J]. INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2000, 77 (09) : 531 - 538
  • [6] Crack initiation by delayed hydride cracking at sharp notches in Zr-2.5 NB alloys
    Sagat, S
    Newman, GW
    Scarth, DA
    [J]. HYDROGEN EFFECTS ON MATERIAL BEHAVIOR AND CORROSION DEFORMATION INTERACTIONS, 2003, : 289 - 299
  • [7] Metallographic and fractographic observations of hydrides during delayed hydride cracking in Zr-2.5% Nb alloy
    Jovanovic, MT
    Shek, GK
    Seahra, H
    Eadie, RL
    [J]. MATERIALS CHARACTERIZATION, 1998, 40 (01) : 15 - 25
  • [8] Threshold stress intensity factor for delayed hydride cracking in Zr-2.5%Nb pressure tube alloy
    Singh, R. N.
    Stahle, P.
    Chakravartty, J. K.
    Shmakov, A. A.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 112 - 117
  • [9] EFFECT OF HYDROGEN CONCENTRATION ON THE THRESHOLD STRESS INTENSITY FACTOR FOR DELAYED HYDRIDE CRACKING IN ZR-2.5 NB PRESSURE TUBES
    Shek, Gordon K.
    Metzger, Don R.
    [J]. PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, PVP 2011, VOL 6, A AND B, 2012, : 1287 - 1295
  • [10] Delayed hydride cracking of Zr-2.5%Nb pressure tube material due to partially constrained precipitates
    Murty, T. Narayana
    Singh, R. N.
    Stahle, P.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2019, 513 : 129 - 142