Delayed hydride cracking of Zr-2.5%Nb pressure tube material due to partially constrained precipitates

被引:21
|
作者
Murty, T. Narayana [1 ,2 ]
Singh, R. N. [1 ,2 ]
Stahle, P. [3 ]
机构
[1] Bhabha Atom Res Ctr, Mech Met Div, Bombay 400085, Maharashtra, India
[2] Homi Bhabha Natl Inst, Bombay 400094, Maharashtra, India
[3] Lund Univ, Div Solid Mech, S-22100 Lund, Sweden
关键词
Zr-25%Nb alloy; Hydride blister; Oxide nodule; Finite element method; Stress field; Delayed hydride cracking; STRESS INTENSITY FACTOR; TERMINAL SOLID SOLUBILITY; FINITE-ELEMENT-METHOD; THRESHOLD STRESS; ZIRCONIUM HYDRIDE; REORIENTATION; FRACTURE; TEMPERATURE; BLISTERS; MISFIT;
D O I
10.1016/j.jnucmat.2018.10.040
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Formation of partially constrained precipitates such as hydride blisters and oxide nodules have been reported on surfaces of Zr-alloy components of pressurised heavy water reactors and is associated with a large increase in volume. Such a change in volume imposes large stresses in the material surrounding the precipitate and may facilitate stable crack growth through delayed hydride cracking. In this work, the stress field of the partially constrained precipitates with different depth and aspect ratio has been computed using a finite element method. The computed stress field is used to predict the region in the matrix in which radial hydride is likely to form and fracture, by taking into consideration grain-size, texture and multi-axial state of stress. For a hypothetical crack just below the precipitate, stress intensity factors are estimated using material properties for both unirradiated and irradiated pressure tube materials. The results are compared with the threshold stress intensity factors required for crack growth due to delayed hydride cracking. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:129 / 142
页数:14
相关论文
共 50 条
  • [1] The delayed hydride cracking avoidance manoeuvre for Zr-2.5 Nb pressure tube alloy
    Yan, D
    Sun, S
    Eadie, RL
    Shek, GK
    Seahra, H
    [J]. INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2000, 77 (09) : 531 - 538
  • [2] Delayed hydride cracking in Zr-2.5Nb pressure tube material
    Singh, RN
    Kumar, N
    Kishore, R
    Roychaudhury, S
    Sinha, TK
    Kashyap, BP
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2002, 304 (2-3) : 189 - 203
  • [3] Indentation and hydride orientation in Zr-2.5%Nb pressure tube material
    Murty, T. Narayana
    Chandanshive, Sandeep A.
    Kumawat, Bhupender K.
    Singh, R. N.
    [J]. 2ND INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY AND EXHIBITION 2018 (SICE 2018), 2019, 14 : 664 - 667
  • [4] Threshold stress intensity factor for delayed hydride cracking in Zr-2.5%Nb pressure tube alloy
    Singh, R. N.
    Stahle, P.
    Chakravartty, J. K.
    Shmakov, A. A.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 112 - 117
  • [5] Effect of radial hydride on delayed hydride cracking behaviour of Zr-2.5Nb pressure tube material
    Sunil, Saurav
    Gopalan, Avinash
    Bind, A. K.
    Sharma, R. K.
    Murty, T. N.
    Singh, R. N.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2020, 542
  • [6] Effect of radial hydride on delayed hydride cracking behaviour of Zr-2.5Nb pressure tube material
    Sunil, Saurav
    Gopalan, Avinash
    Bind, A.K.
    Sharma, R.K.
    Murty, T.N.
    Singh, R.N.
    [J]. Journal of Nuclear Materials, 2021, 542
  • [7] Delayed hydride cracking in Zr-2.5Nb pressure tube material: influence of fabrication routes
    Singh, RN
    Roychowdhury, S
    Sinha, VP
    Sinha, TK
    De, PK
    Banerjee, S
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 374 (1-2): : 342 - 350
  • [8] Hydride morphology and striation formation during delayed hydride cracking in Zr-2.5% Nb
    Shek, GK
    Jovanovic, MT
    Seahra, H
    Ma, Y
    Li, D
    Eadie, RL
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1996, 231 (03) : 221 - 230
  • [9] Temperature dependence of the velocity of delayed hydride cracking in Zr-2.5% Nb Alloy
    Markelov V.A.
    Kotov P.V.
    Zheltkovskaya T.N.
    [J]. Inorganic Materials: Applied Research, 2010, 1 (3) : 217 - 224
  • [10] Precipitation of reoriented hydrides and textural change of α-zirconium grains during delayed hydride cracking of Zr-2.5%Nb pressure tube
    Kim, YS
    Perlovich, Y
    Isaenkova, M
    Kim, SS
    Cheong, YM
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2001, 297 (03) : 292 - 302