Effect of Ball Milling Parameters on the Refinement of Tungsten Powder

被引:22
|
作者
Wu, Zaoming [1 ]
Liang, Yanxia [1 ]
Fu, Engang [1 ]
Du, Jinlong [1 ]
Wang, Peipei [1 ]
Fan, Yong [1 ]
Zhao, Yunbiao [1 ]
机构
[1] Peking Univ, Sch Phys, State Key Lab Nucl Phys & Technol, Beijing 100871, Peoples R China
关键词
morphology and microstructure; nanocrystalline tungsten; refinement; milling speed; process control agent; PLASMA-FACING MATERIALS; MECHANICAL ATTRITION TREATMENT; MICROSTRUCTURAL EVOLUTION; RECRYSTALLIZATION BEHAVIOR; FABRICATION;
D O I
10.3390/met8040281
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The high-energy ball milling method was adopted to explore the influence of ball milling parameters, such as milling speed and additive amounts of process control agent (PCA) on tungsten powder. The morphology and microstructure of tungsten powder in the process of refinement were characterized by field-emission scanning electron microscope (FE-SEM), field-emission transmission electron microscope (FE-TEM), and X-ray diffractometer (XRD). Results revealed that the ball milling process and the refinement of tungsten particle and grain can be largely influenced by these two parameters. The milling efficiency was found to be highest with the milling speed of 700 rpm and additive amounts of 8% PCA. The mechanisms for the effect of these two parameters and milling time on the refinement process were discussed. Nanocrystalline tungsten powder with a particle size and grain size smaller than 100 nm was obtained, and the grain size of 5-15 nm was fabricated successfully under the highest milling efficiency conditions.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Cyclic solid-state transformations during ball milling of aluminum zirconium powder and the effect of milling speed
    El-Eskandarany, MS
    Aoki, K
    Sumiyama, K
    Suzuki, K
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (07): : 1877 - 1880
  • [42] Cyclic solid-state transformations during ball milling of aluminum zirconium powder and the effect of milling speed
    M. Sherif El-Eskandarany
    K. Aoki
    K. Sumiyama
    K. Suzuki
    [J]. Metallurgical and Materials Transactions A, 1999, 30 : 1877 - 1880
  • [43] Influence of ball milling on the sintering behaviour of ZnO powder
    Lao, Y. W.
    Kuo, S. T.
    Tuan, W. H.
    [J]. CERAMICS INTERNATIONAL, 2009, 35 (03) : 1317 - 1320
  • [44] Study of the Ball Milling Device for Synthesizing Nanocrystalline Powder
    Djilali, Zidane
    Said, Bergheul
    [J]. JOURNAL OF NANO RESEARCH, 2017, 47 : 60 - 70
  • [45] Surface modification of silica powder by mild ball milling
    Nakashima, Yuki
    Fukushima, Manabu
    Hyuga, Hideki
    [J]. COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2022, 652
  • [46] Structural changes in iron powder during ball milling
    Khatirkar, R. K.
    Murty, B. S.
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 2010, 123 (01) : 247 - 253
  • [47] Effect of high energy ball milling on spherical metallic powder particulates for additive manufacturing
    Ansell, Troy Y.
    Hanneman, Timothy
    Gonzalez-Perez, Andres
    Park, Chanman
    Nieto, Andy
    [J]. PARTICULATE SCIENCE AND TECHNOLOGY, 2021, 39 (08) : 981 - 989
  • [48] Effect of ball milling materials and methods on powder processing of Bi2223 superconductors
    Yavuz, M
    Maeda, H
    Vance, L
    Liu, HK
    Dou, SX
    [J]. SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1998, 11 (10): : 1153 - 1159
  • [49] Effect on wear resistance of nanoparticles addition to a powder polyester coating through ball milling
    María Fernández-Álvarez
    Francisco Velasco
    Asunción Bautista
    [J]. Journal of Coatings Technology and Research, 2018, 15 : 771 - 779
  • [50] Effect of ball to powder ratio on the ZrO2 phase transformations during milling
    Zakeri, M.
    Razavi, M.
    Rahimipour, M. R.
    Abbasi, B. Jamal
    [J]. PHYSICA B-CONDENSED MATTER, 2014, 444 : 49 - 53