On the Causes of Degradation in Bi2Sr2CaCu2O8+x Round Wires and Coils by Quenching at 4.2 K

被引:12
|
作者
Ye, Liyang [1 ]
Cruciani, Davide [1 ]
Effio, Timothy [2 ,3 ]
Hunte, Frank [1 ]
Schwartz, Justin [1 ]
机构
[1] N Carolina State Univ, Dept Mat Sci & Engn, Raleigh, NC 27695 USA
[2] Florida State Univ, Natl High Magnet Field Lab, Tallahassee, FL 32310 USA
[3] Florida State Univ, Dept Mech Engn, Tallahassee, FL 32310 USA
关键词
Critical current density; high temperature superconductors; mechanical behavior; NORMAL ZONE PROPAGATION; COATED CONDUCTORS; SUPERCONDUCTORS; MAGNETIZATION; GENERATION; STABILITY; BEHAVIOR;
D O I
10.1109/TASC.2013.2271255
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
One of the remaining challenges for the implementation of commercial Ag-alloy-sheathed Bi2Sr2CaCu2O8+x (Bi2212) wires in high-field superconducting magnets is quench protection. To develop an effective quench protection system, it is important to understand the conditions that must be avoided during a quench so that the conductor is not degraded. While these conditions are understood for NbTi and Nb3Sn, they are conductor specific and there remains a lack of data and understanding of the limiting conditions for Bi2212 wires. Here, quenches are induced in short strands and small coils of Bi2212 round wires at 4.2 K. The quench conditions are varied to identify the threshold conditions resulting in wire degradation. These conditions are quantified in terms of the maximum temperature, the maximum time rate of change of the temperature, and the maximum temperature spatial gradient along the length of the wire. It is found that the time rate of change of the temperature (thermal shock) is not a primary driver for degradation but that both the maximum temperature and its spatial gradient play a key role. It is not clear, however, whether the temperature gradient along the length of the wire, or radially from the center of the wire to the surface, dominates. It is also found that threshold values for these parameters vary between different Bi2212 wires and, thus, must be identified for the specific wire to be used in a magnet system. Implications of these results on quench protection are discussed.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] FLEXIBLE BI2SR2CACU2O8+X TAPES BY METALLOORGANIC DEPOSITION
    HUNG, LS
    CHATTERJEE, DK
    JOURNAL OF MATERIALS RESEARCH, 1991, 6 (03) : 459 - 466
  • [22] OXYGEN STOICHIOMETRY, STRUCTURE AND SUPERCONDUCTIVITY IN BI2SR2CACU2O8+X
    KRISHNARAJ, P
    LELOVIC, M
    EROR, NG
    BALACHANDRAN, U
    PHYSICA C, 1995, 246 (3-4): : 271 - 276
  • [23] ANGULAR SCALING OF THE MICROWAVE MAGNETODISSIPATION IN BI2SR2CACU2O8+X
    MARCON, R
    SILVA, E
    FASTAMPA, R
    GIURA, M
    SARTI, S
    PHYSICAL REVIEW B, 1994, 50 (18) : 13684 - 13687
  • [24] Atomic image of Bi2Sr2CaCu2O8+x cleaved surface
    Susla, B
    Giersig, M
    Czajka, R
    Kaminski, A
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2003, 387 (1-2): : 221 - 224
  • [25] Bi2Sr2CaCu2O8+x单晶的热导率测量
    王如竹,吴静怡
    低温工程, 1995, (03) : 43 - 47
  • [26] Needle-like microstructure in Bi2Sr2CaCu2O8+x
    Cabeza, O.
    Barca, O.
    Miguelez, F.
    Journal of low temperature physics, 1997, 107 (5 -6 pt 3): : 503 - 509
  • [27] Neutron depolarisation studies in Bi2Sr2CaCu2O8+x superconductors
    Univ of NSW, Kensington
    J Magn Magn Mater, pt 2 (1317-1318):
  • [28] Analysis of Critical Current Density in Bi2Sr2CaCu2O8+x Round Wire with Filament Fracture
    Donghui Liu
    Huadong Yong
    Youhe Zhou
    Journal of Superconductivity and Novel Magnetism, 2016, 29 : 2299 - 2309
  • [29] Doping dependence of electronic structure in Bi2Sr2CaCu2O8+x
    Onellion, M
    Christensen, S
    Frazer, B
    Gatt, R
    Kelley, RJ
    Misra, S
    Schmauder, T
    Berger, H
    Grioni, M
    Margaritondo, G
    Vobornik, I
    Zwick, F
    Möâle, M
    Kleiner, R
    Müller, P
    HIGH TEMPERATURE SUPERCONDUCTIVITY, 1999, 483 : 304 - 309
  • [30] MODULATED STRUCTURE OF BI2SR2CACU2O8+X SUPERCONDUCTING MONOCRYSTAL
    LEVIN, AA
    SMOLIN, YI
    SHEPELEV, YF
    ZHURNAL NEORGANICHESKOI KHIMII, 1993, 38 (11): : 1755 - 1766