Hot working behavior of a super high strength Cu-Ni-Si alloy

被引:29
|
作者
Lei, Q. [1 ]
Li, Z. [1 ,2 ]
Wang, J. [1 ]
Xie, J. M. [1 ]
Chen, X. [1 ]
Li, S. [3 ]
Gao, Y. [1 ]
Li, L. [1 ]
机构
[1] Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
[3] Minist Educ, Key Lab Nonferrous Met Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
INDUCED PLASTICITY STEEL; DEFORMATION-BEHAVIOR; HIGH-CONDUCTIVITY; MICROSTRUCTURE; EVOLUTION;
D O I
10.1016/j.matdes.2013.05.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hot working behavior of a novel super high strength Cu-6.0Ni-1.0Si-0.5Al-0.15 Mg-0.1Cr alloy has been studied systematically. Experiment of hot compression deformation with temperature ranging from 750 degrees C to 900 degrees C and strain rate from 0.001 s(-1) to 1 s(-1) indicated that both strain rate and deforming temperature affect the flow stress. Flow stress increased to a peak value, and then decreased with increase of deformation time, showing continuous dynamic recrystallization behavior. In the deformation temperature zone of 750-800 degrees C, nucleation of the recrystallization grains occurred in the interior grains at special locations such as deformation bands and shear bands. At the high temperature zone (850-900 degrees C), nucleation of the recrystallization grains occurred both at the grain boundaries and inside the grains of the matrix. Three typical textures appeared after hot compressive deformation and the order of the texture intensity from largest to smallest was: Copper texture of {112}< 111 >, S texture of {123}< 634 >, Gauss texture of {011}< 100 >. On the basis of established processing map, appropriate hot working temperature range was 850-875 degrees C. With the optimised hot working parameters and appropriate thermal mechanical treatment, the designed alloy has achieved excellent properties: hardness 341 HV, tensile strength 1090 MPa, yield strength 940 MPa, elongation 3.5%, electrical conductivity 26.5% IACS, and the stress relaxation rate 8.52% as tested at 150 degrees C for 100 h. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1104 / 1109
页数:6
相关论文
共 50 条
  • [41] CU-NI-SI ALLOY SPRING FOR WIRE SPRING RELAYS
    TOMITA, Y
    YAMADA, Y
    NISHIHATA, M
    SAITOH, T
    SATOH, A
    YOSHIZAWA, H
    KUMAKURA, Y
    [J]. REVIEW OF THE ELECTRICAL COMMUNICATIONS LABORATORIES, 1971, 19 (5-6): : 735 - +
  • [42] Influence of Zinc on Coarsening of δ-Ni2Si Particles, Aging Behavior and Hardness in a Cu-Ni-Si Alloy
    Wei Chen
    Zhou Li
    Hu Xie
    Yanlin Jia
    Mingpu Wang
    [J]. Journal of Materials Engineering and Performance, 2017, 26 : 2459 - 2464
  • [43] Influence of Zinc on Coarsening of δ-Ni2Si Particles, Aging Behavior and Hardness in a Cu-Ni-Si Alloy
    Chen, Wei
    Li, Zhou
    Xie, Hu
    Jia, Yanlin
    Wang, Mingpu
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (06) : 2459 - 2464
  • [44] Effect of Ni/Si mass ratio on microstructure and properties of Cu-Ni-Si alloy
    Tao, Shiping
    Lu, Zhenlin
    Jia, Lei
    Xie, Hui
    Zhang, Jinlong
    [J]. MATERIALS RESEARCH EXPRESS, 2020, 7 (06)
  • [45] Microstructural changes of Cu-Ni-Si alloy during aging
    Dong, Qiming
    Zhao, Dongmei
    Liu, Ping
    Kang, Buxi
    Huang, Jinliang
    [J]. Journal of Materials Science and Technology, 2004, 20 (01): : 99 - 102
  • [46] Microstructural changes of Cu-Ni-Si alloy during aging
    Dong, QM
    Zhao, DM
    Liu, P
    Kang, BX
    Huang, JL
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2004, 20 (01) : 99 - 102
  • [47] Microstructural Changes of Cu-Ni-Si Alloy during Aging
    Qiming DONG
    [J]. Journal of Materials Science & Technology, 2004, (01) : 99 - 102
  • [48] Dynamic embrittlement during fatigue of a Cu-Ni-Si alloy
    Sun, Z.
    Laitem, C.
    Vincent, A.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (19-20): : 6334 - 6337
  • [49] Deformation Behavior of Pure Cu and Cu-Ni-Si Alloy Evaluated by Micro-Tensile Testing
    Yanagida, Sari
    Araki, Akiyoshi
    Chang, Tso-Fu Mark
    Chen, Chun-Yi
    Nagoshi, Takashi
    Kobayashi, Equo
    Hosoda, Hideki
    Sato, Tatsuo
    Sone, Masato
    [J]. MATERIALS TRANSACTIONS, 2016, 57 (11) : 1897 - 1901
  • [50] Corrosion behavior of novel Cu-Ni-Al-Si alloy with super-high strength in 3.5% NaCl solution
    Zhu, Jia-jun
    Li, San-hua
    Shen, Lei-nuo
    Yang, Wu-lin
    Li, Zhou
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2017, 27 (05) : 1096 - 1104