Indium-induced changes in GaN(0001) surface morphology

被引:142
|
作者
Northrup, JE
Neugebauer, J
机构
[1] Xerox Corp, Palo Alto Res Ctr, Palo Alto, CA 94304 USA
[2] Max Planck Gesell, Fritz Haber Inst, D-14195 Berlin, Germany
来源
PHYSICAL REVIEW B | 1999年 / 60卷 / 12期
关键词
D O I
10.1103/PhysRevB.60.R8473
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
First-principles calculations of the energetics of the In-terminated GaN(0001), (000 (1) under bar), (10 (1) under bar 1), and (10 (1) under bar (1) under bar) surfaces indicate that In has a substantial effect on the relative energies of formation of these surfaces. Indium-induced changes in the surface energetics enable the formation of inverted hexagonal pyramid defects having (10 (1) under bar 1) facets at the termination of threading defects on the (0001) surface of pseudomorphic InxGa1-xN films. For dislocations terminating on the InxGa1-xN(000 (1) under bar) surface, the calculations predict that large ( 10 (1) under bar (1) under bar) faceted defects are not energetically favorable.
引用
收藏
页码:R8473 / R8476
页数:4
相关论文
共 50 条
  • [31] Surface morphology and optical properties of InGaN/GaN multiple quantum wells grown on freestanding GaN (0001) substrates
    Zhou, Kun
    Ren, Huaijin
    Liu, Jianping
    Ikeda, Masao
    Ma, Yi
    Gao, Songxin
    Tang, Chun
    Yang, Hui
    SUPERLATTICES AND MICROSTRUCTURES, 2016, 100 : 968 - 972
  • [32] Theoretical adlayer surface morphology of wurtzite 2x2 reconstructions of the GaN(0001) surface
    Timon, V
    Brand, S
    Clark, SJ
    Abram, RA
    JOURNAL OF PHYSICS-CONDENSED MATTER, 2005, 17 (01) : 17 - 26
  • [33] Origins of GaN(0001) surface reconstructions
    Vézian, S
    Semond, F
    Massies, J
    Bullock, DW
    Ding, Z
    Thibodo, PM
    SURFACE SCIENCE, 2003, 541 (1-3) : 242 - 251
  • [34] Vacancy structures on the GaN(0001) surface
    Packard, WE
    Dow, JD
    Doverspike, K
    Kaplan, R
    Nicolaides, R
    JOURNAL OF MATERIALS RESEARCH, 1997, 12 (03) : 646 - 650
  • [35] Vacancy structures on the GaN(0001) surface
    William E. Packard
    John D. Dow
    Kathleen Doverspike
    Ray Kaplan
    Ruth Nicolaides
    Journal of Materials Research, 1997, 12 : 646 - 650
  • [36] Polarization modulation of nanotrenches in GaN (0001)/(0001′) by surface hydrogenation
    Yayama, Tomoe
    Gao, Yanlin
    Okada, Susumu
    Chikyow, Toyohiro
    Japanese Journal of Applied Physics, 2017, 56 (11)
  • [37] NEUTRON-ACTIVATION ANALYSIS OF INDIUM-INDUCED TERATOGENESIS IN GOLDEN-HAMSTER
    MURNANE, JM
    HILBELINK, DR
    TERATOLOGY, 1978, 17 (02) : A22 - A22
  • [38] Structure determination of the indium-induced Si(111)-(4 x 1) reconstruction by surface x-ray diffraction
    Bunk, O
    Falkenberg, G
    Zeysing, JH
    Lottermoser, L
    Johnson, RL
    Nielsen, M
    Berg-Rasmussen, F
    Baker, J
    Feidenhans'l, R
    PHYSICAL REVIEW B, 1999, 59 (19): : 12228 - 12231
  • [39] Structure determination of indium-induced Si(111)-In-4x1 surface by LEED Patterson inversion
    Wang, J
    Wu, HS
    So, R
    Liu, Y
    Xie, MH
    Tong, SY
    PHYSICAL REVIEW B, 2005, 72 (24)
  • [40] Structure determination of the indium-induced Ge(103)-(1 × 1) reconstruction by surface X-ray diffraction
    Bunk, O.
    Falkenberg, G.
    Zeysing, J.H.
    Lottermoser, L.
    Johnson, R.L.
    Nielsen, M.
    Berg-Rasmussen, F.
    Feidenhans'L, R.
    Applied Surface Science, 1999, 142 (01): : 88 - 93