Structural changes in carbon aerogels with high temperature treatment

被引:127
|
作者
Hanzawa, Y
Hatori, H
Yoshizawa, N
Yamada, Y
机构
[1] Natl Inst Adv Ind Sci & Technol, Tsukuba, Ibaraki 3058569, Japan
[2] Japan Sci & Technol Corp, Kawaguchi, Saitama 3320012, Japan
基金
日本学术振兴会;
关键词
carbon aerogel; heat treatment; adsorption; porosity; textures;
D O I
10.1016/S0008-6223(01)00150-6
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The structural change of carbon aerogels at high temperatures up to 2800 degreesC has been investigated. Change in microtexture of fine particles, which constitute carbon aerogels derived from phenolic resin, was of atypical non-graphitized carbon. The microporosity decreased with an increase of heat-treatment temperature, and disappeared at 2000 degreesC. The mesoporosity still remained even after heat-treatment up to 2800 degreesC, though 50% of mesopore volume was lost because of the fusion of the particles with the change of carbon microtexture. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:575 / 581
页数:7
相关论文
共 50 条
  • [21] High temperature treatment and characterization of carbon nanotubes
    Wang, Y
    Huang, W
    Wei, F
    Luo, GH
    Yu, H
    Aihemai, TJ
    [J]. CHEMICAL JOURNAL OF CHINESE UNIVERSITIES-CHINESE, 2003, 24 (06): : 953 - 957
  • [22] HIGH TEMPERATURE THERMOMECHANICAL TREATMENT OF CARBON STEELS
    ZAYMOVSK.VA
    BERNSHTE.ML
    [J]. RUSSIAN METALLURGY, 1966, (02): : 35 - &
  • [23] Printing Porous Carbon Aerogels for Low Temperature Supercapacitors
    Yao, Bin
    Peng, Huarong
    Zhang, Haozhe
    Kang, Junzhe
    Zhu, Cheng
    Delgado, Gerardo
    Byrne, Dana
    Faulkner, Soren
    Freyman, Megan
    Lu, Xihong
    Worsley, Marcus A.
    Lu, Jennifer Q.
    Li, Yat
    [J]. NANO LETTERS, 2021, 21 (09) : 3731 - 3737
  • [24] Thermal Conductivity of Carbon Aerogels as a Function of Pyrolysis Temperature
    M. Wiener
    G. Reichenauer
    F. Hemberger
    H. -P. Ebert
    [J]. International Journal of Thermophysics, 2006, 27 : 1826 - 1843
  • [25] High surface area carbon aerogels for supercapacitors
    Saliger, R
    Fischer, U
    Herta, C
    Fricke, J
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 1998, 225 (1-3) : 81 - 85
  • [26] Textural characterization of high temperature silica aerogels
    Casu, M
    Casula, MF
    Corrias, A
    Paschina, G
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 2003, 315 (1-2) : 97 - 106
  • [27] ALUMINUM SILICATE AEROGELS WITH HIGH TEMPERATURE STABILITY
    Trifu, Roxana
    Rhine, Wendell
    Melnikova, Irene
    White, Shannon
    Hurwitz, Frances
    [J]. ADVANCES IN BIOCERAMICS AND POROUS CERAMICS II, 2010, 30 (06): : 301 - +
  • [28] Progress on Polyimide Aerogels with High Temperature Resistance
    Zhang, Sizhao
    Liu, Chun
    Jiang, Yonggang
    Feng, Jian
    [J]. Cailiao Daobao/Materials Reports, 2024, 38 (13):
  • [29] STRUCTURAL CHANGES OF ZSM-5 MOLECULAR SIEVES, AFTER HIGH TEMPERATURE STEAM TREATMENT.
    Zhang, Wanjing
    Yu, Qin
    Wei, Guoxiang
    Wang, Shuju
    Liu, Zhengyi
    Lin, Bingxion
    [J]. Shiyou Xuebao/Acta Petrolei Sinica, 1985, 1 (01): : 41 - 51
  • [30] Effect of high temperature treatment on tribological properties of carbon/carbon composites
    Luo, Ruiying
    Yang, Zheng
    Li, Hejun
    Kang, Mokuang
    [J]. Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 1996, 13 (04): : 47 - 52