摘要
In this study, the effects of coarse initial grain size with varying heat inputs on microstructure and mechanical properties of weld metal and heat-affected zone (HAZ) were investigated. In the welding experiments, SAE 1020 steel specimens in hot-rolled and in grain-coarsened conditions were used. The specimens taken from the hot-rolled steel (original) plate were heat treated at 1100 degrees C for 45 min and then cooled in a furnace in order to obtain a coarse initial grain size. The original and grain-coarsened specimens were welded using a submerged are welding machine with heat inputs of 0.5, 1 and 2 kJ/mm. Following the welding, microstructure, hardness and toughness of weld metals and HAZs were investigated. From the results, we tried to establish a relationship between initial grain size, microstructure, hardness and toughness of weld metals and HAZs. From the results of the toughness tests, it was seen that the weld metals of coarse initial grain sized specimens and original specimens exhibited nearly the same toughness values with the same heat input, whereas different HAZ toughness values were obtained with the same heat input. Maximum toughness of HAZ of the coarse initial grain sized specimen was achieved with a high input, while maximum toughness of original specimen was obtained with a medium heat input. As a result, considering the heat input, it was observed that the coarse initial grain size had a great influence on the microstructure, hardness and toughness of HAZ of a low carbon steel. Thus, taking into consideration the plate thickness, a higher heat input should be used with respect to the maximum toughness of the HAZ in the welding of grain-coarsened low carbon steels. (C) 1999 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:59 / 66
页数:8
相关论文
共 50 条
  • [31] Influence of grain size on mechanical properties of aluminium GTA weld metal
    P. Schempp
    C. E. Cross
    R. Häcker
    A. Pittner
    M. Rethmeier
    Welding in the World, 2013, 57 : 293 - 304
  • [32] Resistance spot welding of martensitic stainless steel: Effect of initial base metal microstructure on weld microstructure and mechanical performance
    Shirmohammadi, Davood
    Movahedi, Mojtaba
    Pouranvari, Majid
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 703 : 154 - 161
  • [33] Influence of zirconium and boron on low carbon steel weld metal microstructure
    Oh, D.W.
    Olson, D.L.
    Frost, R.H.
    Journal of engineering for industry, 1994, 116 (01): : 26 - 31
  • [34] Effect of Microalloying Additions on the Microstructure and Mechanical Properties of Low Carbon Steel
    Eissa, Mamdouh
    Abd El-Aziz, Ahmed
    Ghali, Saeed
    Halfa, Hossam
    Saber, Shady
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2011, 18 : 246 - 251
  • [35] Effect of Thermomechanical Processing on the Microstructure and Mechanical Properties of Low Carbon Steel
    Shao Zhenyao
    Wang Zhichao
    Li Zhuang
    Wang Shuai
    Wang Jijie
    PROCEEDINGS OF THE 5TH INTERNATIONAL CONFERENCE ON ADVANCED DESIGN AND MANUFACTURING ENGINEERING, 2015, 39 : 1984 - 1989
  • [36] Effect of Microalloying Additions on the Microstructure and Mechanical Properties of Low Carbon Steel
    EISSA Mamdouh
    ABD El-Aziz Ahmed
    GHALI Saeed
    HALFA Hossam
    SABER Shady
    Journal of Iron and Steel Research(International), 2011, 18 (S1) : 246 - 251
  • [37] Effect of Initial Austenite Grain Size on Microstructure Development and Mechanical Properties in a Medium-carbon Steel Treated with One-step Quenching and Partitioning
    Tsuchiyama, Toshihiro
    Amano, Yoshinori
    Uranaka, Shohei
    Masumura, Takuro
    ISIJ INTERNATIONAL, 2021, 61 (02) : 537 - 545
  • [38] Effect of Initial Austenite Grain Size on Microstructure Development and Mechanical Properties in a Medium-carbon Steel Treated with One-step Quenching and Partitioning
    Tsuchiyama, Toshihiro
    Amano, Yoshinori
    Uranaka, Shohei
    Masumura, Takuro
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2023, 109 (04): : 344 - 353
  • [39] Microstructure and Mechanical Properties of a Dissimilar Friction Stir Weld between Austenitic Stainless Steel and Low Carbon Steel
    Jafarzadegan, M.
    Abdollah-Zadeh, A.
    Feng, A. H.
    Saeid, T.
    Shen, J.
    Assadi, H.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2013, 29 (04) : 367 - 372
  • [40] Microstructure and Mechanical Properties of a Dissimilar Friction Stir Weld between Austenitic Stainless Steel and Low Carbon Steel
    M Jafarzadegan
    A.Abdollah-zadeh
    A.H.Feng
    T.Saeid
    J.Shen
    H.Assadi
    Journal of Materials Science & Technology, 2013, 29 (04) : 367 - 372