Reduction Kinetics and Microscopic Properties Transformation of Boron-Bearing Iron Concentrate-Carbon-Mixed Pellets

被引:12
|
作者
Gao, Peng [1 ]
Li, Guofeng [2 ]
Gu, Xiaotian [1 ]
Han, Yuexin [1 ]
机构
[1] Northeastern Univ, Coll Resources & Civil Engn, Shenyang 110819, Liaoning, Peoples R China
[2] North China Univ Sci & Technol, Coll Min Engn, Tangshan, Peoples R China
基金
中国国家自然科学基金;
关键词
Boron-bearing iron concentrate; reduction kinetics; phase transformation; microstructure; COAL-BASED REDUCTION; THERMAL-ANALYSIS; METALLIC IRON; ORE; SEPARATION; DUSTINESS; HEMATITE; STRENGTH; BINDER;
D O I
10.1080/08827508.2019.1598403
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Selective reduction followed by magnetic or melting separation is an innovative and effective method for the comprehensive utilization of boron-bearing iron concentrate. As the raw material of boron products, the reserve of szaibelyite ore is significantly depleted. Therefore, the comprehensive utilization of boron-bearing iron ore resources becomes more and more important. To study the reduction kinetics in depth, a boron-bearing iron concentrate containing 52.18% total iron and 5.50% B2O3 was reduced isothermally with coke as the reductant. The results showed that both the reduction degree and the maximum reduction rate increased with temperature and C/O molar ratio (fixed carbon in the coke to oxygen in iron oxides in the ore). 98.00% reduction degree and 0.00414 s(-1) maximum reduction rate were achieved at 1523K of reduction temperature and 1.4 of C/O molar ratio. The reduction kinetics can be best described by Avrami-Erofeev model, g(alpha) = [-ln(1-alpha)](3/2). The apparent activation energy and pre-exponential factor were 264.565 kJ center dot mol(-1) and 1.87 x 10(7) s(-1), respectively. The phase transformation observed by XRD agreed well with the results of reduction degree analysis. The micro-structure evolution behavior of the pellets was analyzed by SEM and EDS. As the reduction time increased from 0 to 600 s, most of the iron oxides were reduced to metallic iron, leaving other major elements in the slag phase. The slag phase mainly consisted of the solid solution of Mg2SiO4 and Mg3B2O6. With further increase to 1200 s, the metallic iron particles migrated and flocculated together forming bigger particles.
引用
收藏
页码:162 / 170
页数:9
相关论文
共 50 条
  • [21] Mechanism of Strength Improvement of Magnetite Pellet by Adding Boron-bearing Iron Concentrate
    Hong-wei GUO
    Jun-li BAI
    Jian-liang ZHANG
    Hong-ge LI
    Journal of Iron and Steel Research(International), 2014, 21 (01) : 9 - 15
  • [22] Mechanism of Strength Improvement of Magnetite Pellet by Adding Boron-bearing Iron Concentrate
    Guo, Hong-wei
    Bai, Jun-li
    Zhang, Jian-liang
    Li, Hong-ge
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2014, 21 (01) : 9 - 15
  • [23] Mechanism of Strength Improvement of Magnetite Pellet by Adding Boron-bearing Iron Concentrate
    Hong-wei Guo
    Jun-li Bai
    Jian-liang Zhang
    Hong-ge Li
    Journal of Iron and Steel Research International, 2014, 21 : 9 - 15
  • [24] Fluidized Reduction Kinetics of Boron-Bearing Iron Concentrate by Hydrogen at Low Temperatures Based on Model-Fitting and Model-Free Methods
    Li, Peiyu
    Yu, Jianwen
    Li, Yanjun
    Gao, Peng
    Han, Yuexin
    ACS OMEGA, 2024, 9 (17): : 19679 - 19689
  • [25] Effects of copper on structure and properties of boron-bearing ductile iron
    He, Jiangai
    Liu, Yue
    Liu, Yunqiu
    Wang, Yuwei
    Zhan, Kehui
    Dongbei Daxue Xuebao/Journal of Northeastern University, 1998, 19 (03): : 224 - 226
  • [26] Boron-Iron Separation and Boron Enrichment from Boron-Bearing Iron Concentrate at Low-Temperature Enhanced by Supergravity
    Li, Yu
    Gao, Jintao
    Lan, Xi
    Guo, Zhancheng
    ISIJ INTERNATIONAL, 2022, 62 (09) : 1760 - 1767
  • [27] Growth of metallic iron particles during reductive roasting of boron-bearing magnetite concentrate
    Zhang, Xin
    Li, Guang-hui
    Rao, Ming-jun
    Mi, Huan-peng
    Liang, Bin-jun
    You, Jin-xiang
    Peng, Zhi-wei
    Jiang, Tao
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2020, 27 (05) : 1484 - 1494
  • [28] Reduction Characteristics and Kinetics of Bayanobo Complex Iron Ore Carbon Bearing Pellets
    Yin-gui Ding
    Jing-song Wang
    Xue-feng She
    Guang Wang
    Qing-guo Xue
    Journal of Iron and Steel Research International, 2013, 20 : 28 - 33
  • [29] Kinetics and catastrophic swelling during reduction of iron ore in carbon bearing pellets
    Nascimento, R.C.
    Mourão, M.B.
    Capocchi, J.D.T.
    Ironmaking and Steelmaking, 1999, 26 (03): : 182 - 186
  • [30] Reduction Characteristics and Kinetics of Bayanobo Complex Iron Ore Carbon Bearing Pellets
    DING Yin-gui
    WANG Jing-song
    SHE Xue-feng
    WANG Guang
    XUE Qing-guo
    Journal of Iron and Steel Research(International), 2013, 20 (05) : 28 - 33