Reduction Kinetics and Microscopic Properties Transformation of Boron-Bearing Iron Concentrate-Carbon-Mixed Pellets

被引:12
|
作者
Gao, Peng [1 ]
Li, Guofeng [2 ]
Gu, Xiaotian [1 ]
Han, Yuexin [1 ]
机构
[1] Northeastern Univ, Coll Resources & Civil Engn, Shenyang 110819, Liaoning, Peoples R China
[2] North China Univ Sci & Technol, Coll Min Engn, Tangshan, Peoples R China
基金
中国国家自然科学基金;
关键词
Boron-bearing iron concentrate; reduction kinetics; phase transformation; microstructure; COAL-BASED REDUCTION; THERMAL-ANALYSIS; METALLIC IRON; ORE; SEPARATION; DUSTINESS; HEMATITE; STRENGTH; BINDER;
D O I
10.1080/08827508.2019.1598403
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Selective reduction followed by magnetic or melting separation is an innovative and effective method for the comprehensive utilization of boron-bearing iron concentrate. As the raw material of boron products, the reserve of szaibelyite ore is significantly depleted. Therefore, the comprehensive utilization of boron-bearing iron ore resources becomes more and more important. To study the reduction kinetics in depth, a boron-bearing iron concentrate containing 52.18% total iron and 5.50% B2O3 was reduced isothermally with coke as the reductant. The results showed that both the reduction degree and the maximum reduction rate increased with temperature and C/O molar ratio (fixed carbon in the coke to oxygen in iron oxides in the ore). 98.00% reduction degree and 0.00414 s(-1) maximum reduction rate were achieved at 1523K of reduction temperature and 1.4 of C/O molar ratio. The reduction kinetics can be best described by Avrami-Erofeev model, g(alpha) = [-ln(1-alpha)](3/2). The apparent activation energy and pre-exponential factor were 264.565 kJ center dot mol(-1) and 1.87 x 10(7) s(-1), respectively. The phase transformation observed by XRD agreed well with the results of reduction degree analysis. The micro-structure evolution behavior of the pellets was analyzed by SEM and EDS. As the reduction time increased from 0 to 600 s, most of the iron oxides were reduced to metallic iron, leaving other major elements in the slag phase. The slag phase mainly consisted of the solid solution of Mg2SiO4 and Mg3B2O6. With further increase to 1200 s, the metallic iron particles migrated and flocculated together forming bigger particles.
引用
收藏
页码:162 / 170
页数:9
相关论文
共 50 条
  • [1] Reduction–melting behaviors of boron-bearing iron concentrate/carbon composite pellets with addition of CaO
    Guang Wang
    Qing-guo Xue
    Xue-feng She
    Jing-song Wang
    International Journal of Minerals, Metallurgy, and Materials, 2015, 22 : 926 - 932
  • [2] Effect of carbon species on the reduction and melting behavior of boron-bearing iron concentrate/carbon composite pellets
    Wang, Guang
    Ding, Yin-gui
    Wang, Jing-song
    She, Xue-feng
    Xue, Qing-guo
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2013, 20 (06) : 522 - 528
  • [3] Reduction–melting behaviors of boron-bearing iron concentrate/carbon composite pellets with addition of CaO
    Guang Wang
    Qing-guo Xue
    Xue-feng She
    Jing-song Wang
    International Journal of Minerals,Metallurgy and Materials, 2015, 22 (09) : 926 - 932
  • [4] Effect of carbon species on the reduction and melting behavior of boron-bearing iron concentrate/carbon composite pellets
    Guang Wang
    Yin-gui Ding
    Jing-song Wang
    Xue-feng She
    Qing-guo Xue
    International Journal of Minerals, Metallurgy, and Materials, 2013, 20 : 522 - 528
  • [5] Effect of carbon species on the reduction and melting behavior of boron-bearing iron concentrate/carbon composite pellets
    Guang Wang
    Yin-gui Ding
    Jing-song Wang
    Xue-feng She
    Qing-guo Xue
    International Journal of Minerals,Metallurgy and Materials, 2013, 20 (06) : 522 - 528
  • [6] Reduction-melting behaviors of boron-bearing iron concentrate/carbon composite pellets with addition of CaO
    Wang, Guang
    Xue, Qing-guo
    She, Xue-feng
    Wang, Jing-song
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2015, 22 (09) : 926 - 932
  • [7] Reduction of boron-bearing iron ore concentrate/coal composite pellet and kinetics analysis
    Wang, G.
    Xue, Q. G.
    Wang, J. S.
    IRONMAKING & STEELMAKING, 2016, 43 (02) : 153 - 162
  • [8] New approach to reduce carbon emissions by hydrogen reduction of boron-bearing iron concentrate in a fluidized bed: Reduction kinetics and microstructure analysis
    Li, Peiyu
    Yu, Jianwen
    Li, Yanjun
    Gao, Peng
    Han, Yuexin
    MINERALS ENGINEERING, 2024, 212
  • [9] Experimental study on preparation of oxidized Barun iron ore pellets with boron-bearing iron concentrate addition
    School of Materials and Metallurgy, Northeastern University, Shenyang
    110819, China
    Dongbei Daxue Xuebao, 1 (52-56):
  • [10] Carbothermal Reduction of Boron-bearing Iron Concentrate and Melting Separation of the Reduced Pellet
    Wang, Guang
    Xue, Qingguo
    She, Xuefeng
    Wang, Jingsong
    ISIJ INTERNATIONAL, 2015, 55 (04) : 751 - 757