Friction Stir Welded AZ31 Magnesium Alloy: Microstructure, Texture, and Tensile Properties

被引:64
|
作者
Chowdhury, S. H. [1 ]
Chen, D. L. [1 ]
Bhole, S. D. [1 ]
Cao, X. [2 ]
Wanjara, P. [2 ]
机构
[1] Ryerson Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
[2] Natl Res Council Canada, Aerosp Mfg Technol Ctr, Montreal, PQ H3T 2B2, Canada
基金
加拿大自然科学与工程研究理事会; 加拿大创新基金会;
关键词
AL-ZN ALLOYS; STRAIN-HARDENING BEHAVIOR; HIGH-STRENGTH STEEL; MG ALLOY; GRAIN-SIZE; WELDING BEHAVIOR; FATIGUE BEHAVIOR; RATE SENSITIVITY; HOT DEFORMATION; ALUMINUM-ALLOY;
D O I
10.1007/s11661-012-1382-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study was aimed at characterizing the microstructure, texture and tensile properties of a friction stir welded AZ31B-H24 Mg alloy with varying tool rotational rates and welding speeds. Friction stir welding (FSW) resulted in the presence of recrystallized grains and the relevant drop in hardness in the stir zone (SZ). The base alloy contained a strong crystallographic texture with basal planes (0002) largely parallel to the rolling sheet surface and < 11 (2) over bar0 > directions aligned in the rolling direction (RD). After FSW the basal planes in the SZ were slightly tilted toward the TD determined from the sheet normal direction (or top surface) and also slightly inclined toward the RD determined from the transverse direction (or cross section) due to the intense shear plastic flow near the pin surface. The prismatic planes (10 (1) over bar0) and pyramidal planes (10 (1) over bar1) formed fiber textures. After FSW both the strength and ductility of the AZ31B-H24 Mg alloy decreased with a joint efficiency in-between about 75 and 82 pct due to the changes in both grain structure and texture, which also weakened the strain rate dependence of tensile properties. The welding speed and rotational rate exhibited a stronger effect on the YS than the UTS. Despite the lower ductility, strain-hardening exponent and hardening capacity, a higher YS was obtained at a higher welding speed and lower rotational rate mainly due to the smaller recrystallized grains in the SZ arising from the lower heat input. DOI: 10.1007/s11661-012-1382-3 (C) The Minerals, Metals & Materials Society and ASM International 2012
引用
收藏
页码:323 / 336
页数:14
相关论文
共 50 条
  • [31] Refill friction stir spot welding of AZ31 magnesium alloy sheets: metallurgical features, microstructure, texture and mechanical properties
    Liu, Zhe
    Fan, Zhiyu
    Liu, Li
    Miao, Shu
    Lin, Zhicheng
    Wang, Chungui
    Zhao, Yunqiang
    Xin, Renlong
    Dong, Chunlin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 23 : 3337 - 3350
  • [32] Microstructure Distribution and Tensile Anisotropy of Dissimilar Friction Stir Welded AM60 and AZ31 Magnesium Alloys
    Jun-Lei Zhang
    Han Liu
    Yu-Lu Xie
    Guang-Sheng Huang
    Xiang Chen
    Bin Jiang
    Ai-Tao Tang
    Fu-Sheng Pan
    Acta Metallurgica Sinica (English Letters), 2020, 33 : 1487 - 1504
  • [33] The Influence of Friction Stir Welding of Dissimilar AZ31 and AZ91 Magnesium Alloys on the Microstructure and Tensile Properties
    Mohamed, N. S.
    Alias, J.
    INTERNATIONAL JOURNAL OF AUTOMOTIVE AND MECHANICAL ENGINEERING, 2019, 16 (02) : 6675 - 6683
  • [34] Microstructure Distribution and Tensile Anisotropy of Dissimilar Friction Stir Welded AM60 and AZ31 Magnesium Alloys
    Zhang, Jun-Lei
    Liu, Han
    Xie, Yu-Lu
    Huang, Guang-Sheng
    Chen, Xiang
    Jiang, Bin
    Tang, Ai-Tao
    Pan, Fu-Sheng
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2020, 33 (11) : 1487 - 1504
  • [35] Microstructure Distribution and Tensile Anisotropy of Dissimilar Friction Stir Welded AM60 and AZ31 Magnesium Alloys
    Jun-Lei Zhang
    Han Liu
    Yu-Lu Xie
    Guang-Sheng Huang
    Xiang Chen
    Bin Jiang
    Ai-Tao Tang
    Fu-Sheng Pan
    ActaMetallurgicaSinica(EnglishLetters), 2020, 33 (11) : 1487 - 1504
  • [36] Microstructure and Texture Evolution during Friction Stir Processing of AZ31 Mg Alloy
    Xin, Renlong
    Li, Bo
    Liu, Qing
    PRICM 7, PTS 1-3, 2010, 654-656 : 1195 - 1200
  • [37] Friction Stir Extrusion of AZ31 Magnesium Alloy Rod
    Al-Buainain, Maryam
    Shunmugasamy, Vasanth C.
    Mansoor, Bilal
    MAGNESIUM TECHNOLOGY 2022, 2022, : 207 - 212
  • [38] Friction stir processing of commercial AZ31 magnesium alloy
    Darras, B. M.
    Khraisheh, M. K.
    Abu-Farha, F. K.
    Omar, M. A.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 191 (1-3) : 77 - 81
  • [39] Submerged friction stir processing of AZ31 Magnesium alloy
    Darras, Basil
    Kishta, Emad
    MATERIALS & DESIGN, 2013, 47 : 133 - 137
  • [40] The weldability of AZ31 magnesium alloy by friction stir welding
    Aydin, M.
    Bulut, R.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2010, 48 (02): : 97 - 103