The experimental study on friction and wear characteristics of 25Cr12Ni5Mo hot work die steels at high temperature

被引:0
|
作者
Wang Xingguo [1 ]
Xu Jiujun [2 ]
机构
[1] Jingdezhen Ceram Inst, Sch Mech & Elect Engn, Jingdezhen 333403, Peoples R China
[2] Dalian Maritime Univ, Dalian 116026, Peoples R China
关键词
Hot work die steels; High temperature wear; Wear loss; Load;
D O I
10.4028/www.scientific.net/AMM.157-158.286
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
High temperature pin-on-disk tester heated by middle frequency induction was designed. Friction test of hot work die steels with the same composition treated under three different heat treatment conditions was carried out by the pin-on-disk tester at high temperature. The experimental temperature were 200 degrees C, 300 degrees C, 400 degrees C, 500 degrees C, applied loads were 1 kg, 1.5kg, 2kg, 2.5kg, respectively, pin-on-disk circumrotating speed was 1000r/min for all the experiments. Morphology of worn surface and sub-surface structure were observed by optical microscope. Experimental results indicat that wear loss decrease with temperature increasing. Meanwhile, there are various growing rule under different loads, wear loss increase slightly under low load, but increase rapidly with load increasing, especially increment become larger at low temperature. Morphology of worn surface show that the two-body abrasive wear are mainly mechanism under low temperature and low load condition, oxidation wear and adherence abrasive wear are mainly mechanism under high temperature and high load condition.
引用
收藏
页码:286 / +
页数:2
相关论文
共 48 条
  • [1] Study on thermal fatigue damage characteristics of 25Cr12Ni5Mo steel
    Dhi. Dcw Group Co. Ltd., Dalian 116020, China
    不详
    不详
    Cailiao Rechuli Xuebao, 2007, SUPPL. (49-52):
  • [2] High temperature friction and wear properties of two hot work die steels
    Bai Z.-X.
    Zuo P.-P.
    Ji J.
    Wu X.-C.
    Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2019, 41 (07): : 906 - 913
  • [3] High-Temperature Oxidation Behavior of Cr-Ni-Mo Hot-Work Die Steels
    Zhang, Yuqi
    Zhang, Cheng
    Li, Fei
    Wang, Zhou
    Wang, Xiaodong
    Wang, Changji
    Zhang, Chen
    Huang, Jinfeng
    Mao, Feng
    Chen, Chong
    Jiang, Tao
    Wei, Shizhong
    Xiong, Mei
    Hu, Jinmeng
    MATERIALS, 2022, 15 (15)
  • [4] Effect of Mo on the high-temperature oxidation behavior of Cr-Ni-Mo hot-work die steels
    Zhang, Cheng
    Zhang, Yuqi
    Hu, Jinmeng
    Wang, Zhou
    Xue, Jun
    Yu, Hua
    Zhang, Cheng
    Wang, Xiaodong
    Cai, Qiaochu
    Wang, Changji
    Jiang, Tao
    Wei, Shizhong
    Pan, Kunming
    CORROSION SCIENCE, 2023, 224
  • [5] 25Cr12Ni5Mo钢热疲劳损伤特性研究
    郭冰峰
    樊永军
    刘宪东
    王兴国
    郝海
    周文龙
    徐久军
    材料热处理学报, 2007, (S1) : 49 - 52
  • [6] A comparison of wear resistance of two types hot-work die steels at high temperature
    Li S.
    Chen S.
    He X.
    Wu X.
    Wu, Xiaochun (pirateshuang@shu.edu.cn), 1600, Science Press (37): : 59 - 67
  • [7] High-temperature oxidation wear performance and mechanism of Cr-Mo (W)-V hot-work die steel
    Shi, Yuanji
    Yu, Linhui
    Guo, Xunzhong
    Cheng, Cheng
    Zuo, Pengpeng
    Dai, Yunzhong
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2022, 113 (01) : 12 - 32
  • [8] Wear Characteristics of Mo-W-Type Hot-Work Steel at High Temperature
    Shuang Li
    Xiaochun Wu
    Xinxin Li
    Junwan Li
    Xijuan He
    Tribology Letters, 2016, 64
  • [9] Wear Characteristics of Mo-W-Type Hot-Work Steel at High Temperature
    Li, Shuang
    Wu, Xiaochun
    Li, Xinxin
    Li, Junwan
    He, Xijuan
    TRIBOLOGY LETTERS, 2016, 64 (02)
  • [10] High temperature wear characteristics of a new hot work die steel CH95
    Cheng Xianhua
    Shangguan
    Qianqian
    Wu Ju
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2006, 21 (03): : 7 - 11