High-Temperature Oxidation Behavior of Cr-Ni-Mo Hot-Work Die Steels

被引:11
|
作者
Zhang, Yuqi [1 ,2 ]
Zhang, Cheng [2 ]
Li, Fei [1 ,2 ]
Wang, Zhou [1 ,2 ]
Wang, Xiaodong [1 ,2 ]
Wang, Changji [1 ,2 ]
Zhang, Chen [3 ]
Huang, Jinfeng [3 ]
Mao, Feng [1 ,2 ]
Chen, Chong [1 ,2 ]
Jiang, Tao [1 ,2 ]
Wei, Shizhong [2 ]
Xiong, Mei [1 ,2 ]
Hu, Jinmeng [1 ,2 ]
机构
[1] Henan Univ Sci & Technol, Sch Mat Sci & Engn, Luoyang 471003, Peoples R China
[2] Henan Univ Sci & Technol, Natl Joint Engn Res Ctr Abras Control & Molding M, Luoyang 471003, Peoples R China
[3] Univ Sci & Technol Beijing, State Key Lab Adv Met & Mat, 30 Xueyuan Rd, Beijing 100083, Peoples R China
基金
国家重点研发计划;
关键词
oxidation; steels; microstructure; grain boundaries; AUSTENITIC STAINLESS-STEEL; WEAR; MOLYBDENUM; RESISTANCE; MECHANISM; SUPERALLOY; GROWTH;
D O I
10.3390/ma15155145
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The oxidation of 3Cr3Mo2NiW and 3CrNi3Mo steels was studied at 600 degrees C in air, and the test results suggest that the parabolic rate law fitted the oxidation kinetics of both steels. The microstructure, morphology, structure, and phase composition of the oxide film cross-sectional layers of the two Cr-Ni-Mo hot-work die steels were analyzed using scanning electron microscopy (SEM), energy-dispersive spectrometry (EDS), and X-ray diffraction (XRD). The influences of Cr, Ni, and Mo on the high-temperature oxidation resistance of the two Cr-Ni-Mo hot-work die steels are discussed, and the oxidation mechanism is summarized. Heat-treated samples were analyzed using electron backscattered diffraction (EBSD) to obtain inverse pole figures (IPFs) and average sample grain sizes, and the percentages of twin grain boundaries (TGBs) (theta = 60 degrees) were also measured. After heat treatment, recrystallization was observed in both steels with a large portion of twin grain boundaries. After 10 h of oxidation, the dense chromium-rich oxide layer that formed in the inner oxide layer of 3Cr3Mo2NiW steel effectively prevented the continuation of oxidation. The inner oxide layer in 3CrNi3Mo steel formed an adhesion layer with a network structure composed mainly of Ni- and Cr-rich spinel oxide, without forming a barrier to prevent oxidation.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Effect of Mo on the high-temperature oxidation behavior of Cr-Ni-Mo hot-work die steels
    Zhang, Cheng
    Zhang, Yuqi
    Hu, Jinmeng
    Wang, Zhou
    Xue, Jun
    Yu, Hua
    Zhang, Cheng
    Wang, Xiaodong
    Cai, Qiaochu
    Wang, Changji
    Jiang, Tao
    Wei, Shizhong
    Pan, Kunming
    CORROSION SCIENCE, 2023, 224
  • [2] HIGH-TEMPERATURE OXIDATION OF FOUR HOT-WORK TOOL STEELS
    Balasko, Tilen
    Burja, Jaka
    Medved, Jozef
    MATERIALI IN TEHNOLOGIJE, 2018, 52 (06): : 775 - 780
  • [3] High-temperature oxidation wear performance and mechanism of Cr-Mo (W)-V hot-work die steel
    Shi, Yuanji
    Yu, Linhui
    Guo, Xunzhong
    Cheng, Cheng
    Zuo, Pengpeng
    Dai, Yunzhong
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2022, 113 (01) : 12 - 32
  • [4] Thermomechanical fatigue behavior of Cr-Ni-Mo cast hot work die steel
    Jiang, QC
    Fang, JR
    Guan, QF
    SCRIPTA MATERIALIA, 2001, 45 (02) : 199 - 204
  • [5] Thermomechanical fatigue behavior of Cr-Ni-Mo casting hot work die steel
    Fang, Jian-Ru
    Zhang, Rui-Qing
    Zhao, Yu-Qian
    Jiang, Qi-Chuan
    2003, Science Press (28):
  • [6] Microstructures and thermal fatigue behavior of Cr-Ni-Mo hot work die steel modified by rare earth
    Guan, QF
    Jiang, QC
    Fang, JR
    Jiang, H
    ISIJ INTERNATIONAL, 2003, 43 (05) : 784 - 789
  • [7] Simultaneous thermal analysis of the high-temperature oxidation behaviour of three hot-work tool steels
    Balasko, Tilen
    Voncina, Maja
    Medved, Jozef
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2023, 148 (04) : 1251 - 1264
  • [8] Simultaneous thermal analysis of the high-temperature oxidation behaviour of three hot-work tool steels
    Tilen Balaško
    Maja Vončina
    Jožef Medved
    Journal of Thermal Analysis and Calorimetry, 2023, 148 : 1251 - 1264
  • [9] High-temperature properties and microstructural stability of hot-work tool steels
    Medvedeva, A.
    Bergstrom, J.
    Gunnarsson, S.
    Andersson, J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 39 - 46
  • [10] AN APPROACH TO DEVELOPING A HOT-WORK DIE STEEL FOR HIGH-TEMPERATURE APPLICATION
    XIE, CS
    SUN, PZ
    ZHAO, JS
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1990, 124 (02): : 203 - 209