Evolution of interphase and intergranular stresses in Zr-2.5Nb during room temperature deformation

被引:39
|
作者
Cai, S. [1 ]
Daymond, M. R. [1 ]
Holt, R. A. [1 ]
Gharghouri, M. A. [2 ]
Oliver, E. C. [3 ]
机构
[1] Queens Univ, Dept Mech & Mat Engn, Kingston, ON K7L 3N6, Canada
[2] Canadian Neutron Beam Ctr, NRC, Chalk River, ON K0J 1J0, Canada
[3] Rutherford Appleton Lab, ISIS, Didcot OX11 0QX, Oxon, England
关键词
Interphase; Intergranular strain; Neutron diffraction; Asymmetric yielding; Strength differential; Zr-2.5Nb; WT-PERCENT-NB; PRESSURE TUBE MATERIAL; IN-REACTOR DEFORMATION; ZIRCONIUM ALLOYS; IRRADIATION GROWTH; RIETVELD REFINEMENT; MECHANICAL RESPONSE; TEXTURE DEVELOPMENT; RESIDUAL-STRESSES; ROD TEXTURE;
D O I
10.1016/j.msea.2008.10.016
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Both in situ tension and compression tests have been carried out on textured Zr-2.5Nb plate material at room temperature. Deformation along all the three principle plate directions has been studied and the evolution of interphase and intergranular strains along the loading and the principle Poisson's directions has been investigated by neutron diffraction. The evolution of interphase and intergranular strain was determined by the relative phase properties, crystal properties and texture distribution. The average phase behaviors are similar during tension and compression, where the P-phase in this material is stronger than the (x-phase. The asymmetric yielding of the alpha-{0 0 2) grain family results in a relatively large intergranular strain in the loading direction during compression and different dependence of strength during tension and compression on texture. The combination of the thermal residual stress and the asymmetric CRSS in the (c) axis gives the {0 0 0 2} grain family a higher strength in compression than in tension. (c) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:166 / 181
页数:16
相关论文
共 50 条
  • [41] Mechanism of deuterium pickup in Zr-2.5Nb alloy
    Ploc, RA
    MATERIALS AT HIGH TEMPERATURES, 2000, 17 (01) : 29 - 34
  • [42] Modelling of the Zr-2.5Nb alloy properties with hydrides
    Lithuanian Energy Institute, 3 Breslaujos str., 44403 Kaunas, Lithuania
    不详
    Mechanika, 2007, 2 (23-26):
  • [43] Microtexture analysis of Zr-2.5Nb pressure tubing
    Griffiths, M
    Holt, RA
    Li, J
    Saimoto, S
    ANALYSIS OF IN-SERVICE FAILURES AND ADVANCES IN MICROSTRUCTURAL CHARACTERIZATION, 1999, 26 : 293 - 302
  • [44] Corrosion Fatigue Crack Initiation in Zr-2.5Nb
    Nordin, H. M.
    Phillion, A. J.
    Karlsen, T. M.
    Persaud, S.
    PROCEEDINGS OF THE 18TH INTERNATIONAL CONFERENCE ON ENVIRONMENTAL DEGRADATION OF MATERIALS IN NUCLEAR POWER SYSTEMS - WATER REACTORS, VOL 2, 2018, : 525 - 541
  • [45] Evolution of dislocation structure of an alloy of Zr-2.5Nb under a stretching in a ultrasonic field
    Karasevs'ka, O. P.
    Mordyuk, B. M.
    Rudoy, P. Eh.
    Skyba, I. O.
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 2006, 28 : 59 - 66
  • [46] Internal friction peaks associated with hydrides in Zr and Zr-2.5Nb
    Pan, Z.L.
    Puls, M.P.
    Journal De Physique. IV : JP, 1996, 6 (08): : 31 - 34
  • [47] Tensile creep and rupture behavior along with evolution of microstructure in a Zr-2.5Nb alloy
    Guguloth, Krishna
    Ghosh, M.
    Swaminathan, J.
    Mitra, Rahul
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 791
  • [48] Effect of β-Zr decomposition on the solubility limits for H in Zr-2.5Nb
    Khatamian, D
    JOURNAL OF ALLOYS AND COMPOUNDS, 2003, 356 : 22 - 26
  • [49] Internal friction peaks associated with hydrides in Zr and Zr-2.5Nb
    Pan, ZL
    Puls, MP
    JOURNAL DE PHYSIQUE IV, 1996, 6 (C8): : 31 - 34
  • [50] OXIDATION BEHAVIOR OF THE β-Nb PHASE PRECIPITATED IN Zr-2.5Nb ALLOY
    Li Qiang
    Liang Xue
    Peng Jianchao
    Liu Renduo
    Yu Kang
    Zhou Bangxin
    ACTA METALLURGICA SINICA, 2011, 47 (07) : 893 - 898