Phase diagram calculation on Sn-Zn-Ga solders

被引:17
|
作者
Zhang, Y [1 ]
Liang, TX
Jusheng, MA
机构
[1] Tsinghua Univ, Inst Nucl Energy Technol, Beijing 100084, Peoples R China
[2] Tsinghua Univ, Dept Mat Sci & Engn, Beijing 100084, Peoples R China
关键词
D O I
10.1016/j.jnoncrysol.2004.01.013
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Sn-Zn eutectic system is one of the most promising lead-free solders with the advantages of low melting points, excellent mechanical properties and acceptable costs, whereas its poor wetting ability confines its applications in many substrates. In this paper, gallium (Ga) was added to the Sn-Zn eutectic system in order to improve its melting properties and wetting abilities. Piecing binary phase diagram method was employed to calculate the uncharted Sn-Zn-Ga ternary phase diagram and the eutectic point of this ternary system. Differential scanning calorimeter (DSC) method was used to exam the melting point of the solder system. The SnZn6Ga solder has a melting point of 174.4degreesC, with wetting rate of 48.9%, while the melting point of Sn-Zn alloy is 198.5degreesC and melting rate is only about 20%. In addition, the method of piecing binary phase diagrams proves to be feasible to clarify certain unknown ternary phase systems. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:153 / 156
页数:4
相关论文
共 50 条
  • [41] Determination and calculation of the Cd-Pb-Sn ternary phase diagram
    Zhou, Weiya, 1600, Elsevier Sequoia SA, Lausanne, Switzerland (215): : 1 - 2
  • [42] INTERPRETATION OF THE AL-ZN-SN PHASE-DIAGRAM - MECHANISM OF DEGENERATION OF ZN-AL ALLOYS BY SN
    VINCENT, D
    SEBAOUN, A
    MEMOIRES ET ETUDES SCIENTIFIQUES DE LA REVUE DE METALLURGIE, 1981, 78 (03): : 165 - 172
  • [43] Effect of Zn content on the vibration fracture behavior of Sn-Zn and Sn-Zn-Bi solders
    Song, Jenn-Ming
    Lui, Truan-Sheng
    Chang, Yea-Luen
    Chen, Li-Hui
    JOURNAL OF ELECTRONIC MATERIALS, 2006, 35 (05) : 929 - 936
  • [44] Effect of Zn content on the vibration fracture behavior of Sn-Zn and Sn-Zn-Bi solders
    Jenn-Ming Song
    Truan-Sheng Lui
    Yea-Luen Chang
    Li-Hui Chen
    Journal of Electronic Materials, 2006, 35 : 929 - 936
  • [45] ENTHALPY OF FORMATION OF LIQUID CD+GA+IN+SN, CD+GA+IN+ZN, GA+IN+SN+ZN AND CD+GA+IN+SN+ZN ALLOYS
    PERONASILHOL, N
    GAMBINO, M
    BROS, JP
    CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 1992, 16 (04): : 363 - 376
  • [46] 稀土元素Nd对Sn-Zn-Ga无铅钎料组织及性能的影响
    罗冬雪
    薛鹏
    薛松柏
    胡玉华
    焊接学报, 2013, (06) : 57 - 60+116
  • [47] ANALYTICAL CALCULATION OF THE TERNARY ZN-IN-CD PHASE-DIAGRAM
    MOSER, Z
    ZAKULSKI, W
    JEDRZEJEK, C
    ZEITSCHRIFT FUR METALLKUNDE, 1979, 70 (06): : 362 - 365
  • [48] Calculation and Experimental Verification of Zn-Al-Mg Phase Diagram
    Li, Zhao
    Li, Yuanpeng
    Jiang, Sheming
    Zhang, Jie
    Liu, Xin
    Zhang, Qifu
    Liu, Qiuyuan
    COATINGS, 2024, 14 (04)
  • [50] Effect of Ga on the Oxidation Properties of Sn-8.5Zn-0.5Ag-0.1Al-xGa Solders
    Liu, Nai-Shuo
    Lin, Kwang-Lung
    OXIDATION OF METALS, 2012, 78 (5-6): : 285 - 294