Constitutive modeling and microstructure change of Ti-6Al-4V during the hot tensile deformation

被引:87
|
作者
Xiao, J. [1 ]
Li, D. S. [1 ]
Li, X. Q. [1 ]
Deng, T. S. [1 ]
机构
[1] Beihang Univ, Sch Mech Engn & Automat, Beijing 100191, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti-6Al-4V alloy; Hot uniaxial tensile test; Arrhenius-type equation; Constitutive models; Microstructure; TITANIUM; FLOW; EQUATIONS; BEHAVIOR; ALLOY;
D O I
10.1016/j.jallcom.2012.07.048
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Uniaxial tensile tests were performed on a Ti-6Al-4V alloy sheet over the temperature range of 923-1023 K with the strain rates of 5 x 10(-4)-5 x 10(-2) s(-1) up to a 25% length elongation of the specimen. The true stress-strain curves reveal that the flow stress decreases with the increase of the temperature and the decrease of the strain rate. In the same process, the accompanying softening role increases. On the basis of these experimental data, the Arrhenius-type equation was investigated to characterize the hot deformational behavior. Four material constants were determined to be the fourth-order polynomial functions of true strain. The equations show that the flow stress depends on strain, strain rate and temperature. Further, the microstructures, the grain sizes and the microhardnesses of the deformed specimens were measured. The observed results show that the microstructures and the microhardnesses have not changed largely and the grain sizes fluctuate around the initial one. Thus the flow stress model is provided for the process route compiling and the finite element simulation of the hot forming process of the thin-wall Ti-6Al-4V alloy component. (C) 2012 Elsevier B. V. All rights reserved.
引用
收藏
页码:346 / 352
页数:7
相关论文
共 50 条
  • [41] Hot deformation mechanisms in ELI grade Ti-6Al-4V
    Seshacharyulu, T
    Medeiros, SC
    Morgan, JT
    Malas, JC
    Frazier, WG
    Prasad, YVRK
    SCRIPTA MATERIALIA, 1999, 41 (03) : 283 - 288
  • [42] Effect of Hydrogenation on the Hot Deformation of Ti-6Al-4V Alloy
    Niu Yong
    Li Xiaohua
    Wang Yaoqi
    Hou Hongliang
    Li Miaoquan
    Lin Yingying
    Li Zhiqiang
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (12) : 2089 - 2093
  • [43] Hot working of Ti-6Al-4V with a complex initial microstructure
    Bodunrin, Michael O.
    Chown, Lesley H.
    van der Merwe, Josias W.
    Alaneme, Kenneth K.
    INTERNATIONAL JOURNAL OF MATERIAL FORMING, 2019, 12 (05) : 857 - 874
  • [44] Effect of hydrogenation on the hot deformation of Ti-6Al-4V alloy
    Northwestern Polytechnical University, Xi'an 710072, China
    不详
    Xiyou Jinshu Cailiao Yu Gongcheng, 2008, 12 (2089-2093):
  • [45] SEM/EBSD Analysis on Globularization Behavior of Lamellar Microstructure in Ti-6Al-4V During Hot Deformation and Annealing
    Ito, Yoshinori
    Murakami, Shogo
    Tsuji, Nobuhiro
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2017, 48A (09): : 4237 - 4246
  • [46] SEM/EBSD Analysis on Globularization Behavior of Lamellar Microstructure in Ti-6Al-4V During Hot Deformation and Annealing
    Yoshinori Ito
    Shogo Murakami
    Nobuhiro Tsuji
    Metallurgical and Materials Transactions A, 2017, 48 : 4237 - 4246
  • [47] Hot working of Ti-6Al-4V with a complex initial microstructure
    Michael O. Bodunrin
    Lesley H. Chown
    Josias W. van der Merwe
    Kenneth K. Alaneme
    International Journal of Material Forming, 2019, 12 : 857 - 874
  • [48] A New Method to Increase the Spheroidization Rate of LamellarαMicrostructure during Hot Deformation of a Ti-6Al-4V Alloy
    Jiang, Yu-Qiang
    Lin, Y. C.
    Zhao, Chun-Yang
    Chen, Ming-Song
    He, Dao-Guang
    ADVANCED ENGINEERING MATERIALS, 2020, 22 (10)
  • [49] Deformation mechanisms of Ti-6Al-4V during tensile behavior at low strain rate
    Vanderhasten, M.
    Rabet, L.
    Verlinden, B.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2007, 16 (02) : 208 - 212
  • [50] Deformation Mechanisms of Ti-6Al-4V During Tensile Behavior at Low Strain Rate
    M. Vanderhasten
    L. Rabet
    B. Verlinden
    Journal of Materials Engineering and Performance, 2007, 16 : 208 - 212