The Substantiation of the Pre-Polymerization Heating Efficiency of the Dental Nanocomposite Material

被引:0
|
作者
Khabadze, Zurab [1 ]
Kulikova, Alena [1 ]
Abdulkerimova, Saida [1 ]
Bakaev, Yusup [1 ]
Bakaev, Yunus [1 ]
Todua, David [1 ]
Mordanov, Oleg [1 ]
Adzhieva, Anzhela [1 ]
Davreshyan, Georgy [1 ]
Solimanov, Shamil [1 ]
Nazhmudinov, Shamil [1 ]
机构
[1] Peoples Friendship Univ Russia, Med Inst, Miklukho Maklaya St 6, Moscow 117198, Russia
关键词
Dental Materials; Composite Resins; Materials Testing; RESIN-COMPOSITES; MONOMER CONVERSION; TEMPERATURE; KINETICS; ACADEMY;
D O I
10.1590/pboci.2020.139
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective: To evaluate the effect of pre-polymerization heating of nanocomposite filling materials on their strength properties within one manufacture group. Material and Methods: Two nanocomposite filling materials Enamel Plus HRi Universal Dentin (R) and Universal Enamel (R) were used. The linear thermal expansion coefficient (LTEC), Young's modulus and penetration depth were determined during the tests. Changes in the structure of materials were evaluated using electron scanning microscopy. Results: Dentin nanocomposite samples after pre-heating and polymerization have higher LTEC after 30 degrees C compared to dentine nanocomposite untreated samples with statistically significance started at 62 degrees C (p<0.05) and higher temperature. Pre-polymerization heated samples had a statistically higher LTEC (p<0.05) at 57 degrees C. It was revealed that Young's modulus of the dentin nanocomposite samples after thermal processing at 55 degrees C was higher in total after the first heating cycle by 15% compared to the untreated dentin nanocomposite samples (p<0.05). The volume of total porosity after pre-heating decreased to 5-7% (p<0.05). Conclusion: The material that has undergone preliminary heat processing is significantly less deformed under load than the material that does not have thermal processing during the research was established and also has a denser structure.
引用
收藏
页码:1 / 9
页数:9
相关论文
共 50 条
  • [31] TOXICITY OF DENTAL RESIN COMPONENTS - MATERIAL AND POLYMERIZATION INFLUENCE
    LEFEBVRE, CA
    TAMARESELVY, K
    SCHUSTER, GS
    RUEGGEBERG, FA
    JOURNAL OF DENTAL RESEARCH, 1994, 73 : 381 - 381
  • [32] Hydrogen bond diversity in the pre-polymerization stage contributes to morphology and MIP-template recognition - MAA versus MMA
    Golker, Kerstin
    Karlsson, Bjorn C. G.
    Wiklander, Jesper G.
    Rosengren, Annika M.
    Nicholls, Ian A.
    EUROPEAN POLYMER JOURNAL, 2015, 66 : 558 - 568
  • [33] The effect of pre-heating on flame propagation in nanocomposite thermites
    Dikici, Birce
    Pantoya, Michelle L.
    Levitas, Valery
    COMBUSTION AND FLAME, 2010, 157 (08) : 1581 - 1585
  • [34] Low shrinkage light curable nanocomposite for dental restorative material
    Chen, MH
    Chen, CR
    Hsu, SH
    Sun, SP
    Su, WF
    DENTAL MATERIALS, 2006, 22 (02) : 138 - 145
  • [35] Photopolymerization of a dental nanocomposite as restorative material using the argon laser
    Mirsasaani, Seyyed Shahabeddin
    Atai, Mohammad M.
    Hasani-Sadrabadi, Mohammad M.
    LASERS IN MEDICAL SCIENCE, 2011, 26 (05) : 553 - 561
  • [36] Photopolymerization of a dental nanocomposite as restorative material using the argon laser
    Seyyed Shahabeddin Mirsasaani
    Mohammad M. Atai
    Mohammad M. Hasani-Sadrabadi
    Lasers in Medical Science, 2011, 26 : 553 - 561
  • [37] Semi-Empirical Quantum Chemistry Method for Pre-Polymerization Rational Design of Ciprofloxacin Imprinted Polymer and Adsorption Studies
    Marestoni, Luiz D.
    Wong, Ademar
    Feliciano, Gustavo T.
    Marchi, Mary R. R.
    Tarley, Cesar R. T.
    Sotomayor, Maria D. P. T.
    JOURNAL OF THE BRAZILIAN CHEMICAL SOCIETY, 2016, 27 (01) : 109 - 118
  • [38] SCANNING ELECTRON-MICROSCOPY OF MICRO-VASCULAR CASTS .1. IMPROVED PENETRATION AND RESOLUTION WITH CONTROLLED PRE-POLYMERIZATION
    YOUNG, PM
    SILVER, IA
    ROBERTSONRINTOUL, J
    SMITH, EH
    JOURNAL OF ANATOMY, 1980, 131 (DEC) : 776 - 777
  • [39] Insight into the effect of pre-polymerization with propylene on the evolution of crystalline texture and mechanical response during high-density polyethylene production
    Farzad Jani
    Abdolhannan Sepahi
    Shahin Hosseini
    Seyyed Kamal Afzali
    Saeed Houshmandmoayed
    Journal of Polymer Research, 2023, 30
  • [40] A Functional Monomer Is Not Enough: Principal Component Analysis of the Influence of Template Complexation in Pre-Polymerization Mixtures on Imprinted Polymer Recognition and Morphology
    Golker, Kerstin
    Karlsson, Bjorn C. G.
    Rosengren, Annika M.
    Nicholls, Ian A.
    INTERNATIONAL JOURNAL OF MOLECULAR SCIENCES, 2014, 15 (11): : 20572 - 20584