Crack behavior of Ti-6Al-4V alloy combined conformal contact fretting, non-conformal contact fretting and simple fatigue

被引:11
|
作者
Gu, Huiqing [1 ]
Jiao, Li [2 ]
Yan, Pei [2 ]
Ma, Binxing [1 ]
Chen, Shiqi [1 ]
Feng, Lvchen [1 ]
Wang, Xibin [2 ]
机构
[1] Beijing Inst Technol, Sch Mech Engn, 5 Zhongguancun South St, Beijing 100081, Peoples R China
[2] Beijing Inst Technol, Key Lab Fundamental Sci Adv Machining, 5 Zhongguancun South St, Beijing 100081, Peoples R China
基金
中国国家自然科学基金;
关键词
Fretting fatigue; Radial fretting; Conformal contact; Crack propagation; CONNECTING ROD; INITIATION; WEAR; PREDICTION; SURFACE; STRESS; DAMAGE; MECHANISMS; NUCLEATION; EVOLUTION;
D O I
10.1016/j.ijfatigue.2020.105741
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper presents the results of fatigue tests combined with conformal contact, non-conformal contact and simple fatigue carried out on Ti-6Al-4V sheet specimens under externally remote bending load. A special fretting fatigue test rig was proposed to focus on two different fretting modes fatigue test simultaneously between non-conformal contact and conformal contact. The test results showed that all the specimens failed at the conformal contact area under external bending load, although the contact stress was lower, residual stress was higher than that with non-conformal contact area. The reason for failure was radial fretting induced fatigue depending upon the nature of conformal geometry. The conformal geometric nature reversed the contact shear stress, accelerated the debris accumulation, redistributed the contact loading and exacerbated the crack nucleation conditions. The mechanisms of fretting fatigue crack formation, including crack nucleation and the three stages of crack propagation were discussed. Furthermore, among the four regions (fretting region, protrusion region, dark inner friction region and fracture region) on fractography, the protrusion region and dark inner friction region were special, rarely reported before. To explain the formation of the protrusion region, dark inner friction region, internal crack and stripped material on the fractography, a friction-based press-push-separate procedure interpretation was proposed. In addition, crack arresting effect exists in the propagation of fretting fatigue cracks due to compression loading on the contact surface with non-conformal contact.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] Effect of dissimilar metals on fretting fatigue behavior of Ti-6Al-4V
    Hutson, Alisha
    Lee, Hyukjae
    Mall, Shankar
    TRIBOLOGY INTERNATIONAL, 2006, 39 (10) : 1187 - 1196
  • [32] Fretting Fatigue Behavior of Cavitation Shotless Peened Ti-6Al-4V
    Lee, Hyukjae
    Mall, Shankar
    Soyama, Hitoshi
    TRIBOLOGY LETTERS, 2009, 36 (02) : 89 - 94
  • [33] Effects of Shot-Peening on Fretting Fatigue Crack Growth Behavior in Ti-6Al-4V
    Mall, S.
    Jain, V. K.
    Fadag, H. A.
    STRAIN, 2011, 47 : E305 - E318
  • [34] Shear force effects on fretting fatigue behavior of Ti-6Al-4V
    Jin, O
    Mall, S
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (01): : 131 - 138
  • [35] Shear force effects on fretting fatigue behavior of Ti-6Al-4V
    O. Jin
    S. Mall
    Metallurgical and Materials Transactions A, 2004, 35 : 131 - 138
  • [36] Progression of fretting fatigue damage in Ti-6Al-4V
    Hutson, Alisha
    Sathish, Shamachary
    Nicholas, Ted
    TRIBOLOGY INTERNATIONAL, 2006, 39 (10) : 1197 - 1205
  • [37] Life prediction of fretting fatigue of Ti-6Al-4V
    Jin, Ohchang
    Calcaterra, Jeffrey Ronald
    Mall, Shankar
    FATIGUE & FRACTURE MECHANICS, 35TH VOLUME, 2007, 35 : 174 - +
  • [38] Fretting fatigue damage analysis in Ti-6Al-4V
    Anton, DL
    Guillemette, R
    Reynolds, J
    Lutian, M
    SURFACE PERFORMANCE OF TITANIUM, 1996, : 187 - 198
  • [39] Characterization of fretting fatigue crack initiation processes in CR Ti-6Al-4V
    Hutson, A
    Neslen, C
    Nicholas, T
    TRIBOLOGY INTERNATIONAL, 2003, 36 (02) : 133 - 143
  • [40] Effects of process variables on fretting fatigue crack initiation in Ti-6Al-4V
    Namjoshi, SA
    Mall, S
    Jain, VK
    Jin, O
    JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN, 2002, 37 (06): : 535 - 547