Effect of long-term aging on the fracture toughness of primary coolant piping material Z3CN20.09M

被引:11
|
作者
Yu, Weiwei [1 ,2 ]
Fan, Minyu [2 ]
Gao, Hongbo [2 ]
Yu, Dunji [1 ]
Xue, Fei [2 ]
Chen, Xu [1 ]
机构
[1] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300072, Peoples R China
[2] Suzhou Nucl Power Res Inst, Suzhou 215004, Peoples R China
基金
中国国家自然科学基金;
关键词
Long-term aging; Primary coolant piping; Spinodal decomposition; Fracture toughness; SZW; Critical crack size; STRETCH-ZONE; DUCTILE FRACTURE; STAINLESS-STEELS; BEHAVIOR; RESISTANCE; WELDS;
D O I
10.1016/j.nucengdes.2017.12.022
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In this study, a series of accelerated thermal aging tests were performed on primary coolant piping materials (Z3CN20.09M) at 400 degrees C for 0, 2000, 5000 and 18,000 h to investigate the resulting microstructure change and fracture toughness. To further assess their fracture toughness, 0.2 mm offset line method and stretch zone width method were both employed to determine the fracture toughness. The results indicated that after long-term thermal aging, round shaped particles and characteristic morphology of spinodal decomposition were found in ferrite, thus resulting in the thermal aging embrittlement of Z3CN20.09M. Subsequently, the J-R curves and J-T curves all decreased significantly with the increasing thermal aging time. Furthermore, the fracture toughness parameters J(50), J(SZW(2D)), J(SZW(3D)) and dJ/d Delta a were first decreased rapidly and then slow saturated. In addition, the J(SZW(2D)) and J(SZW(3D)) values were significantly lower than J(Q) while the reduction of the critical crack size based on J(SZW(2D)) and J(SZW(3D)) parameters was about 30% compared with J(Q), and thus J(SZW) was relatively close to the onset of crack initiation.
引用
收藏
页码:150 / 160
页数:11
相关论文
共 50 条
  • [31] Effect of sigma phase on the low cycle fatigue property of Z3CN20.09M cast duplex stainless steel in high temperature water
    Wu, H. C.
    Yang, B.
    Wang, Y. Q.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2015, 66 (07): : 663 - 669
  • [32] Crack Initiation Mechanism of Z3CN20.09M Duplex Stainless Steel during Corrosion Fatigue in Water and Air at 290 °C
    Wu, H. C.
    Yang, B.
    Shi, Y. Z.
    Gao, Q.
    Wang, Y. Q.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2015, 31 (11) : 1144 - 1150
  • [33] 热老化对核电主管道Z3CN20.09M不锈钢点蚀性能的影响
    王永强
    董芳
    杨滨
    北京科技大学学报, 2014, 36 (05) : 644 - 649
  • [34] Crack Initiation Mechanism of Z3CN20.09M Duplex Stainless Steel during Corrosion Fatigue in Water and Air at 290 °C
    H.C.Wu
    B.Yang
    Y.Z.Shi
    Q.Gao
    Y.Q.Wang
    JournalofMaterialsScience&Technology, 2015, 31 (11) : 1144 - 1150
  • [35] Microstructure evolution and impact fracture behaviors of Z3CN20-09M stainless steels after long-term thermal aging
    Li, S. L.
    Wang, Y. L.
    Zhang, H. L.
    Li, S. X.
    Zheng, K.
    Xue, F.
    Wang, X. T.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 433 (1-3) : 41 - 49
  • [36] DETERMINATION OF INTERGRANULAR CORROSION SUSCEPTIBILITY OF Z3CN20.09M CAST DUPLEX STAINLESS STEEL BY A MODIFIED DOUBLE LOOP ELECTROCHEMICAL POTENTIOKINETIC REACTIVATION METHOD
    Shi, Y. Z.
    Yang, B.
    Zhang, M. X.
    Wu, H. C.
    Wang, S. L.
    ENERGY MATERIALS CONFERENCE PROCEEDINGS 2014, 2014, : 557 - 562
  • [37] Effect of long-term thermo-oxidative aging on weight and fracture toughness of polycyanate neat resin
    Kobayashi, Yoshiyuki
    Kobayashi, Satoshi
    ADVANCED COMPOSITE MATERIALS, 2016, 25 (05) : 471 - 485
  • [38] 核电站主管道Z3CN20.09M不锈钢中金属间相的析出行为
    王永强
    韩军
    杨滨
    武焕春
    王西涛
    金属学报 , 2013, (04) : 415 - 420
  • [39] The effect of long-term isothermal aging on dynamic fracture toughness of type 17-4 PHSS at 350°C
    Wang, J
    Zou, H
    Wu, XY
    Li, C
    Qiu, SY
    Shen, BL
    MATERIALS TRANSACTIONS, 2005, 46 (04) : 846 - 851
  • [40] Effect of long-term aging at 350°C on dynamic fracture toughness of 17-4PH stainless steel
    School of Materials Science and Engineering, Sichuan University, Chengdu 610064, China
    不详
    Yuanzineng Kexue Jishu, 2006, 2 (243-248):