The occurrence of porosity in reline acrylic resins. Effect of microwave disinfection

被引:11
|
作者
Rocha Novais, Polyanna Maria [1 ]
Giampaolo, Eunice Teresinha [2 ]
Vergani, Carlos Eduardo [2 ]
Machado, Ana Lucia [2 ]
Pavarina, Ana Claudia [2 ]
Jorge, Janaina Habib [3 ]
机构
[1] Univ Fortaleza, Dept Dent, Fortaleza, Ceara, Brazil
[2] Sao Paulo State Univ, Araraquara Dent Sch, Dept Dent Mat & Prosthodont, Sao Paulo, Brazil
[3] Univ Estadual Ponta Grossa, Dept Dent, Maringa, Parana, Brazil
关键词
acrylic resins; relining; porosity; microwave; DENTURE BASE POLYMERS; RESIDUAL MONOMER CONTENT; SURFACE-TOPOGRAPHY; CANDIDA-ALBICANS; WATER; ADHESION; STERILIZATION; CONVERSION; ROUGHNESS; STRENGTH;
D O I
10.1111/j.1741-2358.2008.00251.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Microwave energy has proved to be an effective method for disinfecting acrylic dentures. However, the effect of microwave heating on the porosity of autopolymerising denture reline resins has not been investigated. The purpose of the study was to determine the effect of microwave disinfection on the porosity of autopolymerised denture reline materials (Kooliner-K, New Truliner-NT, Tokuso Rebase Fast-TR and Ufi Gel Hard-UGH) and a conventional heat-polymerised denture base resin (Lucitone 550-L). Specimens (10 mm x 20 mm x 1 mm) were obtained from the impression surface of the palatal mucosa in a single person and divided into four groups (n = 5). The porosity was evaluated after polymerisation (C1), after two cycles of microwave disinfection (MW2), after seven cycles of microwave disinfection (MW7) and after 7 days storage in water at 37 degrees C (C2). Specimens from group MW7 were exposed to microwave disinfection daily being stored in water at 37 degrees C between exposures. All the replicas were sputter coated with gold and micrographs/digital images were taken of each replica using scanning electron microscopy at magnification x 100. The SEM micrographs were then examined using an image analyser to determine the number of pores. Comparison between materials and groups were made using Kruskal-Wallis tests. MW7 resulted in a significant increase in the number from the pores of material K, but decreased in number in reline material TR and UGH reline resin. The number of pores in materials NT and L remained unaffected following microwave disinfection. Differences in the porosity amongst the materials and for different experimental conditions were observed following microwave disinfection.
引用
收藏
页码:65 / 71
页数:7
相关论文
共 50 条
  • [1] Effect of a disinfection protocol on the hardness and roughness of reline acrylic resins.
    Azevedo, A
    Machado, AL
    Giampaolo, ET
    Pavarina, AC
    Vergani, CE
    Magnani, R
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A414 - A414
  • [2] Effect of microwave disinfection on the surface hardness and roughness of reline resins.
    Jorge, EG
    Azevedo, A
    Machado, AL
    Vergani, CE
    Pavarina, AC
    Giampaolo, ET
    Sampaio, FSA
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : 161 - 161
  • [3] Effects of microwave disinfection on hardness and roughness of acrylic denture resins.
    Pavan, S
    Sousa, RLS
    Batista, AUD
    Arioli, JN
    Mollo, FA
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : 232 - 232
  • [4] Water sorption, solubility and porosity of hard chairside reline resins.
    Cucci, ALM
    Vergani, CE
    Giampaolo, ET
    Teixeira, CES
    JOURNAL OF DENTAL RESEARCH, 1997, 76 (05) : 999 - 999
  • [5] Effect of microwave disinfection on the flexural strength of hard chairside reline resins
    Pavarina, AC
    Neppelenbroek, KH
    Guinesi, AS
    Vergani, CE
    Machado, AL
    Giampaolo, ET
    JOURNAL OF DENTISTRY, 2005, 33 (09) : 741 - 748
  • [6] The influence of microwave irradiation on the hardness of two autopolymerizing reline resins.
    Reis, JMSN
    Vergani, CE
    Seo, RS
    Machado, AL
    Giampaolo, ET
    Pavarina, AC
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : 167 - 167
  • [7] Effect of repeated cycles of chemical disinfection on the roughness and hardness of hard reline acrylic resins
    Pinto, Luciana de Rezende
    Rodriguez Acosta, Emilio Jose T.
    Fernandes Tavora, Flora Freitas
    Batista da Silva, Paulo Mauricio
    Porto, Vinicius Carvalho
    GERODONTOLOGY, 2010, 27 (02) : 147 - 153
  • [8] Effects of polymerization mode on porosity of acrylic denture resins.
    Terry, GL
    Murchison, DF
    Wofford, DT
    Sarkar, NK
    JOURNAL OF DENTAL RESEARCH, 1996, 75 : 313 - 313
  • [9] Influence of curing cycles on the roughness and porosity of acrylic resins.
    Tanji, M
    Domitti, SS
    Consani, RLX
    Consani, S
    Sinhoreti, MAC
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B132 - B132
  • [10] Adaptation, porosity, flexural and impact strength of acrylic resins.
    Ganzarolli, SM
    Mello, JAN
    Del bel Cury, AA
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B130 - B130