摘要
Gravimetric measurements were made for the kinetics of the carbide formation from reduced iron by preventing the decomposition of iron carbides and the deposition of carbon by utilizing the effect of sulfur. Particles of a hematite ore were completely reduced in the H-2-H2S mixture and converted to iron carbide in a CO-H-2-H2S-CO2-H2O-Ar or CO-CO2-COS-N-2 mixture at 873 to 1073 K. The carbide formation kinetics was drastically accelerated by the addition of a few percent H-2 to CO and reached the maximum at about 20 pct H-2. From morphology observation, it was assumed that the carburization reaction on the surface of pores in the reduced iron determines the carbide formation kinetics, and the carburization rate, df(theta)/dt, is expressed as the product of a function of carburization rate, g(pi, T), and the relative reaction surface area at the time t, 1 - f(theta). Applying the integrated rate equation, -In (1 - f(theta)) = g(p(i), T)t, to the experimental results, the value of g(pi, T) was obtained. By analyzing the carbide formation rate, it was assumed that the elementary reactions determining the carbide formation rate are CO + H(ad) --> [C] + OH(ad) and OH(ad) + H-2 = H2O + H(ad), except in the low ratio Of pH(2)/Pco, where the rate determining elementary reaction shifts to O(ad) + CO - CO2. The overall rate Eq. [22] has been proposed for the carbide formation from the reduced iron in CO-H-2-H2S-CO2-H2O mixtures.
引用
收藏
页码:1161 / 1170
页数:10
相关论文
共 50 条
  • [41] KINETICS AND MECHANISMS OF IRON-CATALYZED COKE GASIFICATION WITH H-2 AND H2-H2O-MIXTURES
    HAHN, R
    HUTTINGER, KJ
    SCHLEICHER, P
    CARBON, 1980, 18 (01) : 45 - 45
  • [42] EFFECT OF H2S ON CARBON DEPOSITION ON IRON IN CO-H2 MIXTURES AT 1203-K
    ANDO, S
    KUROSE, N
    KIMURA, H
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1988, 29 (10): : 820 - 827
  • [43] CONDITIONS FOR THE FORMATION OF DENSE AND POROUS IRON ON REDUCTION OF WUSTITE IN H2/H2O AND CO/CO2 GAS-MIXTURES
    HAYES, PC
    STJOHN, DH
    CIM BULLETIN, 1982, 75 (842): : 112 - 112
  • [44] SOLUBILITY OF H2S IN FES AT 800 DEGREES C IN H2S/H2 GAS MIXTURES AND POSSIBLE EFFECTS ON SULFIDATION KINETICS OF IRON
    ZELOUF, S
    SIMKOVIC.G
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1970, 117 (08) : C252 - &
  • [45] THE CORROSION OF IRON AND OF 3 COMMERCIAL STEELS IN H2-H2S AND IN H2-H2S-CO2 GAS-MIXTURES AT 400-700-DEGREES-C
    GESMUNDO, F
    VIANI, F
    ZNAMIROWSKI, W
    GODLEWSKI, K
    BREGANI, F
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1992, 43 (03): : 83 - 95
  • [46] KINETICS AND MECHANISMS OF THE OXIDATION OF CHROMIUM IN H2-H2O-H2S GAS-MIXTURES
    LABRANCHE, MH
    YUREK, GJ
    OXIDATION OF METALS, 1987, 28 (1-2): : 73 - 98
  • [47] Study on the controlling steps and reduction kinetics of iron oxide briquettes with CO-H2 mixtures
    Liu, Donghui
    Wang, Xiaozhe
    Zhang, Jianliang
    Liu, Zhengjian
    Jiao, Kexin
    Liu, Xingle
    Wang, Rongrong
    METALLURGICAL RESEARCH & TECHNOLOGY, 2017, 114 (06)
  • [48] Carbon formation on the surface during the reduction of iron oxide particles by CO and CO/H2 mixtures
    Lu, Feng
    Wen, Liangying
    Chen, Yangxin
    Zhong, Hong
    Xu, Jian
    Zhang, Shengfu
    Yang, Zhongqing
    CHEMICAL ENGINEERING SCIENCE, 2019, 205 : 238 - 247
  • [49] CARBON DEPOSITION OVER FE, NI, AND CO FOILS FROM CO-H2-CH4-CO2-H2O, CO-CO2, CH4-H2, AND CO-H2-H2O GAS-MIXTURES .2. KINETICS
    JABLONSKI, GA
    GEURTS, FWAH
    SACCO, A
    CARBON, 1992, 30 (01) : 99 - 106
  • [50] KINETICS OF FORMATION OF H2O AND CO2 DURING IRON-OXIDE REDUCTION
    HAYES, PC
    METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1979, 10 (02): : 211 - 217