Micro-arc oxidation was applied to AZ91D magnesium alloy by taking K2Cr2O7 as the colouring salt in the silicate system. It was shown that the green coating obtained through performing micro-arc oxidation on magnesium alloy consisted of Mg, Mg2SiO4, MgO, and MgCr2O4 based on analysis of X-ray diffraction (XRD), and scanning electron microscopy (SEM). Among which, MgCr2O4 was the colouring salt; there were something in the lamellar, pit, and convex forms found on the surface of the coating. The coating consisted of a porous, and a compact, layer from the outside to the inside. As demonstrated, the colour of the coating depended on the K2Cr2O7 concentration: it became gradually deeper with the addition of K2Cr2O7 and the increasing micro-arc oxidation time. The corrosion resistance and hardness of the green coating were greater than that of the matrix.
引用
收藏
页码:36 / 40
页数:5
相关论文
共 50 条
  • [21] EFFECTS OF OXIDATION TIME ON MICRO-ARC OXIDIZED COATINGS OF MAGNESIUM ALLOY AZ91D IN ALUMINATE SOLUTION
    Mu, Weiyi
    Li, Zhengxian
    Du, Jihong
    Luo, Ruixue
    Xi, Zhengping
    MAGNESIUM TECHNOLOGY 2011, 2011, : 537 - 541
  • [22] Corrosion behavior of micro-arc oxidation coating on magnesium alloy AZ91D in Na2SO4 solution
    Guo, Huixia
    Ma, Ying
    Zhang, Yufu
    Dong, Hairong
    Hao, Yuan
    Kuei Suan Jen Hsueh Pao/Journal of the Chinese Ceramic Society, 2013, 41 (03): : 382 - 387
  • [23] Wear resistance of ceramic coating on AZ91 magnesium alloy by micro-arc oxidation
    赵晖
    刘正
    陈立佳
    陈吉
    韩忠
    Transactions of Nonferrous Metals Society of China, 2006, (S3) : 1814 - 1818
  • [24] Wear resistance of ceramic coating on AZ91 magnesium alloy by micro-arc oxidation
    Zhao Hui
    Liu Zheng
    Chen Li-jia
    Chen Ji
    Han Zhong
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1814 - S1818
  • [25] Interaction of heat-treatment and micro-arc oxidation on AZ91D magnesium alloys
    State Key Laboratory of Advanced Non-Ferrous Metal Materials, Lanzhou University of Technology, Lanzhou 730050, China
    不详
    Cailiao Yanjiu Xuebao, 2009, 6 (656-662): : 656 - 662
  • [26] Compactness of micro-arc oxidation coatings on AZ91D magnesium alloys and its effect on coating corrosion resistance
    Dong, Hai-Rong
    Ma, Ying
    Guo, Hui-Xia
    Zhang, Yu-Fu
    Hao, Yuan
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2015, 25 (04): : 844 - 851
  • [27] Improvement on corrosion resistance of micro-arc oxidized AZ91D magnesium alloy by a pore-sealing coating
    Zhu, Jiyuan
    Jia, Haojie
    Liao, Kaijin
    Li, Xianxuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 889
  • [28] Improvement on corrosion resistance of micro-arc oxidized AZ91D magnesium alloy by a pore-sealing coating
    Zhu, Jiyuan
    Jia, Haojie
    Liao, Kaijin
    Li, Xianxuan
    Journal of Alloys and Compounds, 2022, 889
  • [29] Quick forming of coating on AZ91D in AC micro-arc oxidation surface treatment
    Zhang, P. (pzhang1@bjtu.edu.cn), 2013, Science Press (42):
  • [30] PREPARATION OF COMPOSITE COATING ON AZ91D MAGNESIUM ALLOY BY SILICA SOL-MICRO-ARC OXIDATION
    Shao, Zhongcai
    Zhang, Feifei
    Zhao, Ruiqiang
    Shen, Xiaoyi
    SURFACE REVIEW AND LETTERS, 2016, 23 (04)