Application of cyclic upsetting-extrusion to semi-solid processing of AZ91D magnesium alloy

被引:7
|
作者
Tao, Jian-quan [1 ]
Jiang, Ju-fu [2 ]
Chen, Hong [1 ]
Xiao, Yuan-lun [1 ]
Zhang, Rong-chao [1 ]
Hu, Qing-hua [1 ]
Zhao, Jun [1 ]
Zhao, Qiang [1 ]
机构
[1] Southwest Tech & Engn Inst, Chongqing 400039, Peoples R China
[2] Harbin Inst Technol, Sch Mat & Engn, Harbin 150001, Peoples R China
关键词
AZ91D magnesium alloy; semi-solid processing; cyclic upsetting-extrusion; mechanical properties; microstructure; TENSILE MECHANICAL-PROPERTIES; CHANNEL ANGULAR EXTRUSION; MICROSTRUCTURAL EVOLUTION; MG-AL;
D O I
10.1016/S1003-6326(13)62547-9
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The microstructural evolution of AZ91D magnesium alloy prepared by means of the cyclic upsetting-extrusion and partial remelting was investigated. The effects of remelting temperature and holding time on microstructure of semi-solid AZ91D magnesium alloy were studied. Furthermore, tensile properties of thixoextruded AZ91D magnesium alloy components were determined. The results show that the cyclic upsetting-extrusion followed by partial remelting is effective in producing semi-solid AZ91D magnesium alloy for thixoforming. During the partial remelting, with the increase of remelting temperature and holding time, the solid grain size increases and the degree of spheroidization tends to be improved. The tensile mechanical properties of thixoextruded AZ91D magnesium alloy components produced by cyclic upsetting-extrusion and partial remelting are better than those of the same alloy produced by casting.
引用
收藏
页码:909 / 915
页数:7
相关论文
共 50 条
  • [31] Influence of procedure parameters on rheological property of semi-solid AZ91D magnesium alloy
    Jiang, YX
    Xie, SS
    Li, XG
    Li, L
    JOURNAL OF RARE EARTHS, 2004, 22 : 47 - 49
  • [33] Microstructure of electromagnetic stirred semi-solid AZ91D alloy
    Mao, WM
    Zhen, ZS
    Chen, HT
    Zhong, XY
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2004, 14 (05) : 846 - 850
  • [34] Effect of holding time on thixotropic fluidity of semi-solid AZ91D magnesium alloy
    Ji, Zesheng
    Hu, Maoliang
    Zheng, Xiaoping
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2007, 23 (02) : 247 - 252
  • [36] Microstructure of electromagnetic stirred semi-solid AZ91D alloy
    毛卫民
    甄子胜
    陈洪涛
    钟雪友
    TransactionsofNonferrousMetalsSocietyofChina, 2004, (05) : 846 - 850
  • [37] Effects of processing parameters on the microstructure of ECAE-formed AZ91D magnesium alloy in the semi-solid state
    Luo, Shoujing
    Chen, Qiang
    Zhao, Zude
    Journal of Alloys and Compounds, 2009, 477 (1-2): : 602 - 607
  • [38] Effects of processing parameters on the microstructure of ECAE-formed AZ91D magnesium alloy in the semi-solid state
    Luo, Shoujing
    Chen, Qiang
    Zhao, Zude
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 477 (1-2) : 602 - 607
  • [39] Semi-solid billets of AZ91D magnesium alloy prepared by forward extrusion/Equal-Channel Angular Pressing
    Zhang, Guang-An
    Ma, Cui-Yan
    Zhou, Qi
    MATERIALS AND MANUFACTURING, PTS 1 AND 2, 2011, 299-300 : 380 - 384
  • [40] Effects of processing parameters on microstructure of semi-solid slurry of AZ91D magnesium alloy prepared by gas bubbling
    Zhang, Yang
    Wu, Guo-hua
    Liu, Wen-cai
    Zhang, Liang
    Pang, Song
    Ding, Wen-jiang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (07) : 2181 - 2187