A mullite/SiC oxidation protective coating for carbon/carbon composites

被引:86
|
作者
Wang, Kai-Tong [1 ]
Cao, Li-Yun [1 ]
Huang, Jian-Feng [1 ]
Fei, Jie [1 ]
机构
[1] Shaanxi Univ Sci & Technol, Sch Mat Sci & Engn, Key Lab Auxiliary Chem & Technol Chem Ind, Minist Educ, Xian 710021, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
Carbon/carbon composites; Mullite coating; Hydrothermal electrophoretic deposition; Oxidation; C/C-SIC COMPOSITES; HYDROTHERMAL TREATMENT; TEMPERATURES; BEHAVIOR; HA;
D O I
10.1016/j.jeurceramsoc.2012.08.009
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To protect carbon/carbon (C/C) composites against oxidation, a mullite coating was prepared on SiC precoated C/C composites by a hydrothermal electrophoretic deposition process. The phase composition, microstructure and oxidation resistance of the prepared mullite/SiC coatings were investigated. Results show that hydrothermal electrophoretic deposition is an effective route to achieve crack-free mullite coatings. The mullite/SiC coating displays excellent oxidation resistance and can protect C/C composites from oxidation at 1773 K for 322 h with a weight loss rate of only 4.89 x 10(-4) g/cm(2) h. The failure of the multi-layer coatings is considered to be caused by the volatilization of silicate glass layer, the formation of microholes and microcracks on the coating surface and the formation of penetrative holes between the SiC bonding layer and the C/C matrix at 1773 K. The corresponding high temperature oxidation activation energy of the coated C/C composites at 1573-1773 K is calculated to be 111.11 kJ/mol. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:191 / 198
页数:8
相关论文
共 50 条
  • [31] A cordierite-mullite anti-oxidation coating for carbon/carbon composites
    Lan, Feng-tao
    Li, Ke-zhi
    Li, He-jun
    Fu, Qian-gang
    CARBON, 2007, 45 (13) : 2708 - 2710
  • [32] TaB2-SiC-Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites
    Ren, Xuanru
    Li, Hejun
    Fu, Qiangang
    Chu, Yanhui
    Li, Kezhi
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (15-16) : 2953 - 2959
  • [34] Oxidation Protective C/SiC/Si-SiC Multilayer Coating for Carbon/Carbon Composites Applying at 1873 K
    Zhang, Yulei
    Li, Hejun
    Qiang, Xinfa
    Li, Kezhi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2010, 26 (12) : 1139 - 1142
  • [35] Effect of SiC whiskers on the microstructure and oxidation protective ability of SiC-CrSi2 coating for carbon/carbon composites
    Fu, Qian-Gang
    Li, He-Jun
    Li, Ke-Zhi
    Shi, Xiao-Hong
    Huang, Min
    Sun, Guo-Dong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 445 : 386 - 391
  • [36] An oxidation protective Si-Mo-Cr coating for C/SiC coated carbon/carbon composites
    Yu-Lei, Zhany
    He-Jun, Li
    Qian-Gang, Fu
    Xi-Yuan, Yao
    Ke-Zhi, Li
    Geng-Sheny, Jiao
    CARBON, 2008, 46 (01) : 179 - 182
  • [37] Oxidation protective TaB2-SiC gradient coating to protect SiC-Si coated carbon/carbon composites against oxidation
    Ren, Xuanru
    Li, Hejun
    Fu, Qiangang
    Li, Kezhi
    COMPOSITES PART B-ENGINEERING, 2014, 66 : 174 - 179
  • [38] SiC nanowire-toughened SiC-MoSi2-CrSi2 oxidation protective coating for carbon/carbon composites
    Yan-Hui, Chu
    Qian-Gang, Fu
    Cui-Wei, Cao
    He-Jun, Li
    Ke-Zhi, Li
    Qin, Lei
    SURFACE & COATINGS TECHNOLOGY, 2010, 205 (02): : 413 - 418
  • [39] Microstructure and oxidation protective ability of MoSi2-SiC-Si coating toughened with SiC whiskers for carbon/carbon composites
    Fu, Q. -G.
    Li, H. -J.
    Li, K. -Z.
    Shi, X. -H.
    SURFACE ENGINEERING, 2008, 24 (05) : 383 - 387
  • [40] A SiC-Si-ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites
    Yao, Xiyuan
    Li, Hejun
    Zhang, Yulei
    Wu, Heng
    Qiang, Xinfa
    CERAMICS INTERNATIONAL, 2012, 38 (03) : 2095 - 2100