Effect of temperature gradient on the erosion behavior of SiC coating for carbon/carbon composites in a combustion environment

被引:15
|
作者
Zhang, Jia-Ping [1 ]
Fu, Qian-Gang [1 ]
Qu, Jun-Ling [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Temperature gradient; SiC coating; Oxidation behavior; Mechanical property; Wind tunnel; OXIDATION; RESISTANCE; MICROSTRUCTURE; DEGRADATION;
D O I
10.1016/j.ceramint.2016.08.174
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
SiC coating with a thickness of 50-70 mu m was prepared on the surface of C/C composites by in-situ reaction method. The SiC coated C/C composites were then tested in a wind tunnel where a temperature gradient from 200 to 1600 degrees C could be obtained to investigate their erosion behavior. The results of wind tunnel test indicated that the service life of C/C composites was prolonged from 0.5 to 44 h after applying the SiC coating. After the wind tunnel test, three typical oxidation morphologies, including glassy SiO2 layer, porous SiO2 layer and clusters of honeycomb-like SiO2 grains, were found on the SiC coated C/C composites. With the decrease of oxidation temperature, the amount of glassy SiO2 declined and the thermal stress increased, which induced the cracking followed by the degradation of the SiC coating. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:18411 / 18417
页数:7
相关论文
共 50 条
  • [21] Influence of grain size on wear behavior of SiC coating for carbon/carbon composites at elevated temperatures
    Chen Zishan
    Li Hejun
    Li Kezhi
    Shen Qingliang
    Fu Qiangang
    MATERIALS & DESIGN, 2014, 53 : 412 - 418
  • [22] Oxidation behavior and kinetics of SiC/alumina-borosilicate coating for carbon-carbon composites
    Li, Jun
    Luo, Ruiying
    Chen, Yaping
    Xiang, Qiao
    Lin, Chen
    Ding, Peng
    An, Na
    Cheng, Jiwei
    APPLIED SURFACE SCIENCE, 2008, 255 (05) : 1967 - 1974
  • [23] A mullite/SiC oxidation protective coating for carbon/carbon composites
    Wang, Kai-Tong
    Cao, Li-Yun
    Huang, Jian-Feng
    Fei, Jie
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (01) : 191 - 198
  • [24] SiCn/SiC oxidation protective coating for carbon/carbon composites
    Huang Jian-Feng
    Liu Miao
    Wang Bo
    Cao Li-Yun
    Xia Chang-Kui
    Wu Jian-Peng
    CARBON, 2009, 47 (04) : 1198 - 1201
  • [25] Ablation resistance of ZrC/SiC gradient coating for SiC-coated carbon/carbon composites prepared by supersonic plasma spraying
    Yao, Dong-Jia
    Li, He-Jun
    Wu, Heng
    Fu, Qian-Gang
    Qiang, Xin-Fa
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (15) : 3739 - 3746
  • [26] Effects of Cyclic Loading and Temperature on a SiC-Coated Carbon/Carbon Composite in a Combustion Environment
    Liu, Chidong
    Cheng, Laifei
    Luan, Xingang
    Li, Jianghong
    Huang, Hui
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2008, 91 (11) : 3634 - 3637
  • [27] SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites
    Li, HJ
    Fu, QG
    Shi, XH
    Li, KZ
    Hu, ZB
    CARBON, 2006, 44 (03) : 602 - 605
  • [28] Ablation behavior of TaB2-SiC coating for carbon/carbon composites under oxyacetylene torch
    Qu, Jun-Ling
    Fu, Qian-Gang
    Zhang, Jia-Ping
    Zhang, Peng-Fei
    VACUUM, 2016, 131 : 223 - 230
  • [29] The Research of the Carbon Coating on SiC Fiber and the SiCf/SiC Composites
    刘伟峰
    王亦菲
    叶飞
    材料导报, 2007, (S1) : 237 - 238
  • [30] Si-SiC oxidation protective coating for carbon/carbon composites
    Fu, QG
    Li, HJ
    Shi, XH
    Li, KZ
    Sun, GD
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 : 261 - 264