Self-piercing riveting of aluminium-lithium alloy sheet materials

被引:30
|
作者
Zhang, Xianlian [1 ]
He, Xiaocong [1 ]
Gu, Fengshou [2 ]
Ball, Andrew [2 ]
机构
[1] Kunming Univ Sci & Technol, Innovat Mfg Res Ctr, Kunming 650500, Yunnan, Peoples R China
[2] Univ Huddersfield, Ctr Efficiency & Performance Engn, Huddersfield HD1 3DH, W Yorkshire, England
基金
中国国家自然科学基金;
关键词
Self-piercing riveting; Aluminium-lithium alloy; Fretting wear; MECHANICAL-PROPERTIES; PROCESS PARAMETERS; FATIGUE PROPERTIES; FRETTING BEHAVIOR; SPR JOINTS; AEROSPACE; TITANIUM;
D O I
10.1016/j.jmatprotec.2019.01.019
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The self-piercing riveting (SPR) of 1420 aluminium-lithium alloy sheets is investigated. Static tests with lapshear loads and fatigue tests using the tension-tension loading mode were applied to obtain the joint performances and failure modes. The mechanism analysis regarding failure and fretting was employed using a scanning electron microscope (SEM) and an energy dispersive X-ray spectroscopy (EDX). The 1420 Al-Li alloy sheets can be joined effectively using SPR. The fatigue load-fatigue life curve with a 95% confidence level is obtained using a variation coefficient method. The joints failed in the rivet pulled out from the locked sheet in static trials, and the locked sheet fractured during the fatigue tests. The fretting wear can be observed at the contact interface between the rivet tail and the locked sheet or between both sheets at different load levels. The fretting region changes at a high or low load level, and it is highly relevant to the fatigue rupture paths.
引用
收藏
页码:192 / 200
页数:9
相关论文
共 50 条
  • [31] Influence of aluminium sheet surface modification on the self-piercing riveting process and the joint static lap shear strength
    Li, Dezhi
    [J]. INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 93 (5-8): : 2685 - 2695
  • [32] Inversion Model of Maximum Riveting Force in Aluminum Alloy Self-piercing Riveting Processes
    Sun, Xiaoting
    Zeng, Kai
    He, Xiaocong
    Xing, Baoying
    [J]. Zhongguo Jixie Gongcheng/China Mechanical Engineering, 2021, 32 (11): : 1341 - 1345
  • [33] Strength modeling of Al-alloy sheet self-piercing riveting considering different failure modes
    Liu, Yahui
    Zhu, Zhiwang
    Yu, Huipeng
    Wang, Jun
    [J]. INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 127 (5-6): : 2487 - 2503
  • [34] Influence of aluminium sheet surface modification on the self-piercing riveting process and the joint static lap shear strength
    Dezhi Li
    [J]. The International Journal of Advanced Manufacturing Technology, 2017, 93 : 2685 - 2695
  • [35] A Performance Study of Self-piercing Riveting of Aluminum and Copper Alloy Sheets
    Deng, Chengjiang
    He, Xiaocong
    Xing, Baoying
    [J]. RESOURCES AND SUSTAINABLE DEVELOPMENT, PTS 1-4, 2013, 734-737 : 2460 - 2464
  • [36] Strength modeling of Al-alloy sheet self-piercing riveting considering different failure modes
    Yahui Liu
    Zhiwang Zhu
    Huipeng Yu
    Jun Wang
    [J]. The International Journal of Advanced Manufacturing Technology, 2023, 127 : 2487 - 2503
  • [37] Fatigue Performance and Life Prediction of Aluminum Alloy Self-piercing Riveting
    Qiu, Sawei
    Lei, Bei
    Ye, Tuo
    Zhang, Yue
    Jiang, Jiachuan
    Wang, Tao
    [J]. Cailiao Daobao/Materials Reports, 2024, 38 (18):
  • [38] Effects of process parameters on friction self-piercing riveting of dissimilar materials
    Liu, Xun
    Lim, Yong Chae
    Li, Yongbing
    Tang, Wei
    Ma, Yunwu
    Feng, Zhili
    Ni, Jun
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2016, 237 : 19 - 30
  • [39] Friction Self-Piercing Riveting (F-SPR) of Dissimilar Materials
    Ma, YunWu
    Xian, XiRui
    Lou, Ming
    Li, YongBing
    Lin, ZhongQin
    [J]. INTERNATIONAL CONFERENCE ON THE TECHNOLOGY OF PLASTICITY, ICTP 2017, 2017, 207 : 956 - 961
  • [40] An experimental and numerical investigation on self-piercing riveting
    R. Porcaro
    M. Langseth
    S. Weyer
    H. Hooputra
    [J]. International Journal of Material Forming, 2008, 1 : 1307 - 1310