Experimental Study on Intermittent Turning 2.25Cr-1Mo-0.25V Steel with Coated Cemented Carbide Tool

被引:2
|
作者
Liu, Hanlian [1 ]
Lv, Xiang [1 ]
Huang, Chuanzhen [1 ]
Zhu, Hongtao [1 ]
机构
[1] Shandong Univ, Sch Mech Engn, Minist Educ, Ctr Adv Jet Engn Technol CaJET,Key Lab High Effic, Jinan 250061, Peoples R China
来源
关键词
Shell ring material; Intermittent turning; Efficient machining; Failure mechanism;
D O I
10.4028/www.scientific.net/AMR.500.128
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In order to improve the machining efficiency and tool life in manufacturing process of hydrogenation reactor shell components, the cutting performance of quadrate GC4235 coated carbide tool in intermittent turning 2.25Cr-1Mo-0.25V steel was investigated, the optimal cutting parameters were obtained. The empirical mathematical models of relationships among the amount of metal removal, tool life, cutting force and cutting parameters were established. The failure mechanism of the GC4235 carbide coated tools for turning 2.25Cr-1Mo-0.25V steel at lower speed intermittent turning was abrasive wear and the coating peeling; however coating peeling and substrate adhesive wear were the main failure forms at the higher speed.
引用
收藏
页码:128 / 133
页数:6
相关论文
共 50 条
  • [1] Experimental study of temper embrittlement of 2.25Cr-1Mo-0.25V steel weld metals
    Song, L. P.
    Sun, R. L.
    APPLIED SCIENCE, MATERIALS SCIENCE AND INFORMATION TECHNOLOGIES IN INDUSTRY, 2014, 513-517 : 3 - 6
  • [2] Quantitative carbide analysis using the Rietveld method for 2.25Cr-1Mo-0.25V steel
    Zhang Yongtao
    Han Haibo
    Miao Lede
    Zhang Hanqian
    Li Jinfu
    MATERIALS CHARACTERIZATION, 2009, 60 (09) : 953 - 956
  • [3] Evolution Behavior of Carbides in 2.25Cr-1Mo-0.25V Steel
    Zhang Yongtao
    Miao Lede
    Wang Xiaojun
    Zhang Hanqian
    Li Jinfu
    MATERIALS TRANSACTIONS, 2009, 50 (11) : 2507 - 2511
  • [4] Research on Turning 2.25Cr-1Mo-0.25v Force Density Function and Stress
    Li Zhe
    Li Yongfu
    Li Long
    Zheng Minli
    Zhai Quanpeng
    PROCEEDINGS OF 2013 2ND INTERNATIONAL CONFERENCE ON MEASUREMENT, INFORMATION AND CONTROL (ICMIC 2013), VOLS 1 & 2, 2013, : 1425 - 1430
  • [5] Different tempering precipitation behaviors of carbide in 2.25Cr-1Mo-0.25V steel after quenching and normalizing
    Zhang Yongtao
    Song Guobin
    Zhang Hanqian
    Li Jinfu
    TMS 2010 139TH ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 3: GENERAL PAPER SELECTIONS, 2010, : 715 - +
  • [6] Characterization of microstructures of 2.25Cr-1Mo-0.25V steel after quenching and tempering
    Zhong, Yong-Tao
    Gao, Jia-Qiang
    Zhang, Han-Qian
    Li, Jin-Fu
    Cailiao Kexue yu Gongyi/Material Science and Technology, 2008, 16 (SUPPL. 1): : 64 - 67
  • [7] Effect of Hydrogen on Fracture Toughness Behavior of 2.25Cr-1Mo-0.25V Steel
    Chai, Mengyu
    Song, Yan
    Zhang, Zaoxiao
    Duan, Quan
    Cheng, Guangxu
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2018, VOL 1A, 2019,
  • [8] Effect of reheating processes on grain boundary heritance for 2.25Cr-1Mo-0.25V steel
    Wang, C. Y.
    Fu, R. D.
    Zhou, W. H.
    Zhang, W. H.
    Zheng, Y. Z.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 438 (1135-1138): : 1135 - 1138
  • [9] Microstructure and Charpy Impact Toughness of a 2.25Cr-1Mo-0.25V Steel Weld Metal
    Wu, Kefan
    Yan, Yingjie
    Cao, Rui
    Li, Xinyu
    Jiang, Yong
    Yang, Fei
    Jia, Xingwang
    Chen, Jianhong
    MATERIALS, 2020, 13 (13)
  • [10] Characterization of Hydrogen Embrittlement in 2.25cr-1mo-0.25v Steel by Eddy Current Method
    Zhou, Haiting
    Xu, Chi
    Wang, Qingming
    Pan, Hongliang
    Chen, Jianjun
    RESEARCH IN NONDESTRUCTIVE EVALUATION, 2018, 29 (04) : 212 - 220