The effect of chloride concentration and pH on pitting corrosion of AA7075 aluminum alloy coated with phenyltrimethoxysilane

被引:43
|
作者
Younis, A. A. [1 ]
El-Sabbah, M. M. B. [2 ]
Holze, Rudolf [1 ]
机构
[1] Tech Univ Chemnitz, AG Elektrochem, Inst Chem, D-09111 Chemnitz, Germany
[2] Al Azhar Univ, Dept Chem, Fac Sci, Nasr City 11884, Cairo, Egypt
关键词
Aluminum alloy (AA7075); Phenyltrimethoxysilane; Pitting corrosion; Sodium chloride; Harrison's solution; ELECTROCHEMICAL-BEHAVIOR; SUSCEPTIBILITY; COPPER; AA5083; ION;
D O I
10.1007/s10008-011-1476-7
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The effect of chloride ion concentration and pH of solution on the corrosion behavior of aluminum alloy AA7075 coated with phenyltrimethoxysilane (PTMS) immersed in aqueous solutions of NaCl is reported. Potentiodynamic polarization, linear polarization, open circuit potential, and weight loss measurements were performed. The surface of samples was examined using SEM and optical microscopy. Elemental characterization of the coating by secondary ion mass spectrometry indicates an intermediate layer between coating and aluminum alloy surface. The corrosion behavior of the aluminum alloy AA7075 depends on chloride concentration and pH of solution. In acidic or neutral solutions, general and pitting corrosion occur simultaneously. On the contrary, exposure to alkaline solutions results in general corrosion only. Results further reveal that aluminum alloy AA7075 is susceptible to pitting corrosion in all chloride solutions with concentrations between 0.05 M and 2 M NaCl; an increase in the chloride concentration slightly shifted both the pitting and corrosion potentials to more active values. Linear polarization resistance measurements show a substantially improved corrosion resistance value in case of samples coated with PTMS as compared to uncoated samples in both neutral (pH = 7), acidic (pH = 0.85 and 3), and alkaline chloride solutions (pH = 10 and 12.85). The higher corrosion resistance of the aluminum alloy coated with PTMS can be attributed to the hydrophobic coating which acts as a barrier and prevents chloride ion penetration and subsequent reaction with the aluminum alloy.
引用
收藏
页码:1033 / 1040
页数:8
相关论文
共 50 条
  • [41] Effect of Friction Stir Processing on Pitting Corrosion and Intergranular Attack of 7075 Aluminum Alloy
    Navaser, M.
    Atapour, M.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2017, 33 (02) : 155 - 165
  • [42] Effect of Nitriding on the Microstructure and Mechanical Properties of AA7075 Alloy
    Panchenko, I. A.
    Konovalov, S. V.
    Drobyshev, V. K.
    Labinsky, D. N.
    Khusainov, Y. G.
    Nazarov, A. Yu.
    RUSSIAN JOURNAL OF NON-FERROUS METALS, 2024, 65 (03) : 162 - 169
  • [43] Surface Morphology and Hardness Analysis of TiCN Coated AA7075 Aluminium Alloy
    Srinath M.K.
    Ganesha Prasad M.S.
    Journal of The Institution of Engineers (India): Series C, 2019, 100 (01) : 221 - 228
  • [44] Numerical analysis of heat treatment of TiCN coated AA7075 aluminium alloy
    Srinath, M. K.
    Prasad, M. S. Ganesha
    ADVANCES IN MECHANICAL DESIGN, MATERIALS AND MANUFACTURE, 2018, 1943
  • [45] Pitting corrosion evaluation in aluminum alloy AA1050
    Garita-Arce, Luis
    Rodriguez-Yanez, Javier E.
    TECNOLOGIA EN MARCHA, 2014, 27 (03): : 13 - 21
  • [46] Taguchi optimization of PEO process parameters for corrosion protection of AA7075 alloy
    Songur, Fatma
    Arslan, Ersin
    Dikici, Burak
    SURFACE & COATINGS TECHNOLOGY, 2022, 434
  • [47] Double aging and thermomechanical heat treatment of AA7075 aluminum alloy extrusions
    Emani, S. V.
    Benedyk, J.
    Nash, P.
    Chen, D.
    JOURNAL OF MATERIALS SCIENCE, 2009, 44 (23) : 6384 - 6391
  • [48] A difference-imaging technique used to study streaking corrosion of aluminum alloys AA7075 and AA8006 in chloride solution
    Huang, RS
    Lin, CJ
    Isaacs, HS
    ELECTROCHEMICAL AND SOLID STATE LETTERS, 2006, 9 (02) : B11 - B14
  • [49] Effects of Re-Aging on the Fatigue Properties of Aluminum Alloy AA7075
    Fakioglu, Avni
    Oezyuerek, Dursun
    MATERIALS TESTING, 2014, 56 (7-8) : 575 - 582
  • [50] Double aging and thermomechanical heat treatment of AA7075 aluminum alloy extrusions
    S. V. Emani
    J. Benedyk
    P. Nash
    D. Chen
    Journal of Materials Science, 2009, 44 : 6384 - 6391