DEEP DRAWING FORMABILITY OF THE MEASUREMENT OF MAGNESIUM SHEET METALS

被引:0
|
作者
Minami, Akihiro [1 ]
Sakamoto, Hidetoshi [2 ]
Marumo, Yasuo [3 ]
机构
[1] Ariake Natl Coll Technol, Fukuoka, Japan
[2] Doshisha Univ, Kyoto, Japan
[3] Kumamoto Univ, Kumamoto, Japan
关键词
deep drawing; magnesium; formability; limiting drawing ratio;
D O I
10.2495/CMEM170011
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the field of sheet metals forming, the press forming is executed as important method for mass production processing. It is reported that the plastic formability of Mg-alloy improves in the warm working. The warm deep drawing tests was carried out by using the 2 kinds of punch diameter, 30 mm and 50 mm. This paper describes about the optimum deep drawing conditions with forming temperature and lubricant in the magnesium AZ31B alloy and the flame retardant magnesium alloy AMX602. These Mg alloys are difficult to mold at room temperature. However, in forming temperature at 180 degrees C-200 degrees C, Limiting Drawing Ratio (LDR) of AZ31B became 2.65. The optimum forming temperature condition of AZ31B is 180 degrees C-200 degrees C. The value of LDR decreases at 200 degrees C or more. LDR of retardant magnesium alloy AMX602 is also 2.65 at the temperature at 300 degrees C-320 degrees C. The optimum temperature conditions of retardant magnesium alloy AMX602 is assumed to be 300 degrees C or more. After molding, the thickness decreases from the punch shoulder to the part around the sidewall. The magnesium alloys in thickness change is similar to the common deep drawing with the other materials. In AZ31B alloy and AMX602 alloy, the failure pattern is often occurred at sidewall area and punch-shoulder area respectively.
引用
收藏
页码:1 / 10
页数:10
相关论文
共 50 条
  • [21] Orientation and formability of orthotropic sheet metals
    Brunel Univ, Middlesex, United Kingdom
    J Strain Anal Eng Des, 1 (61-81):
  • [22] Orientation and formability of orthotropic sheet metals
    Rees, DWA
    Power, RK
    JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN, 1997, 32 (01): : 61 - 81
  • [23] Ductile fracture criterion for warm deep drawing of magnesium alloy sheet
    Chang, Qunfeng
    Peng, Yinghong
    Du, Zhaohui
    Jixie Gongcheng Xuebao/Journal of Mechanical Engineering, 2009, 45 (10): : 294 - 299
  • [24] Heated hydro-mechanical deep drawing of magnesium sheet metal
    Kurz, G
    MAGNESIUM TECHNOLOGY 2004, 2004, : 67 - 71
  • [25] Forming property of Magnesium Alloy Sheet in Radial Pressure Deep Drawing
    Mao, Xianchang
    Lin, Haiyan
    PROCEEDINGS OF THE 6TH INTERNATIONAL CONFERENCE ON INFORMATION ENGINEERING FOR MECHANICS AND MATERIALS, 2016, 97 : 508 - 513
  • [26] The numerical analysis of the formability of aluminium alloy sheet in complex shape box deep drawing forming
    Yu, Z.Q.
    Lin, Z.Q.
    Zhao, Y.X.
    Key Engineering Materials, 2004, 274-276 (0I) : 619 - 624
  • [27] EXPERIMENTAL ESTIMATION OF SIZE EFFECT AND FORMABILITY IN MICROSCALE DEEP DRAWING PROCESS USING COPPER SHEET
    Nam, Jung Soo
    Lee, Sang Won
    Kim, Hong Seok
    PROCEEDINGS OF THE ASME 9TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE, 2014, VOL 2, 2014,
  • [28] Validation of Formability of Laminated Sheet Metal for Deep Drawing Process using GTN Damage Model
    Lim, Yongbin
    Cha, Wan-gi
    Ko, Sangjin
    Kim, Naksoo
    NUMISHEET 2014: THE 9TH INTERNATIONAL CONFERENCE AND WORKSHOP ON NUMERICAL SIMULATION OF 3D SHEET METAL FORMING PROCESSES: PART A BENCHMARK PROBLEMS AND RESULTS AND PART B GENERAL PAPERS, 2013, 1567 : 607 - 613
  • [29] The numerical analysis of the formability of aluminium alloy sheet in complex shape box deep drawing forming
    Yu, ZQ
    Lin, ZQ
    Zhao, YX
    ADVANCES IN ENGINEERING PLASTICITY AND ITS APPLICATIONS, PTS 1 AND 2, 2004, 274-276 : 619 - 623
  • [30] Effect of Strain Rate on Formability in Warm Deep Drawing of High Tensile Strength Steel Sheet
    Yoshihara, Shoichiro
    Iwamatsu, Go
    INTERNATIONAL CONFERENCE OF COMPUTATIONAL METHODS IN SCIENCES AND ENGINEERING 2014 (ICCMSE 2014), 2014, 1618 : 315 - 318