Spheroidization of Eutectic Silicon in Direct-Electrolytic Al-Si Alloy

被引:9
|
作者
Wang, Ruyao [1 ]
Lu, Weihua [1 ]
机构
[1] Donghua Univ, Dept Mat Sci & Engn, Shanghai 200051, Peoples R China
关键词
SHAPE INSTABILITIES; GROWTH;
D O I
10.1007/s11661-012-1603-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The spheroidization process of direct-electrolytic Al-Si alloy (DEASA) containing Si content in the range of 7 to 12 pct heated at temperatures of 778 K to 803 K (505 A degrees C to 530 A degrees C) was studied. The width, length, and aspect ratio of Si particles were measured to quantitatively analyze the microstructural variety of Si phase during the heating process in terms of chemical composition and remelting. Compared to existing Al-Si alloy, the lower soaking temperature of 778 K to 783 K (505 A degrees C to 510 A degrees C) is required to obtain the full spheroidization of the Si phase of DEASA. When remelting DEASA, a satisfactory granulation rate can be achieved at a higher soak temperature of 788 K to 803 K (515 A degrees C to 530 A degrees C). The origin of the high spheroidizaton rate is attributed to the microstructural characteristic relative to the electrolysis process. It would be expected that high crystallographic defects of Si grain result in the complete spheroidization of Si phase at lower temperatures for a short period.
引用
收藏
页码:2799 / 2809
页数:11
相关论文
共 50 条
  • [21] Influence of silicon on growth process of plasma electrolytic oxidation coating on Al-Si alloy
    He, J.
    Cai, Q. Z.
    Luo, H. H.
    Yu, L.
    Wei, B. K.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 471 (1-2) : 395 - 399
  • [22] Effect of humidity on friction and wear of Al-Si eutectic alloy and Al-Si alloy-graphite composites
    Yen, BK
    Ishihara, T
    WEAR, 1996, 198 (1-2) : 169 - 175
  • [23] Crystal morphology of massive eutectic silicon in unmodified Al-Si eutectic
    Shamsuzzoha, M.
    Hogan, L.M.
    Metallography, 1989, 22 (01): : 37 - 45
  • [24] Morphology transformation of eutectic silicon in Al-Si alloy during solid solution treatment
    Liu, Bingyi
    Xue, Yajun
    Tezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys, 2006, 26 (12): : 802 - 804
  • [25] Investigation on Wear Behavior of Al-Si Eutectic Alloy
    Al-Ethari, Haydar
    Haleem, Ali Hubi
    Hassan, Muhanad Hamid
    2021 12TH INTERNATIONAL CONFERENCE ON MECHANICAL AND AEROSPACE ENGINEERING (ICMAE), 2021, : 176 - 180
  • [26] Modification of silicon in eutectic and hyper-eutectic Al-Si alloys
    Heshmatpour, B
    LIGHT METALS 1997, 1997, : 801 - 808
  • [27] Silicon morphology modification in the eutectic Al-Si alloy using mechanical mold vibration
    Abu-Dheir, N
    Khraisheh, M
    Saito, K
    Male, A
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 393 (1-2): : 109 - 117
  • [28] Effect of silicon content on wear resistance and corrosion behaviour of Al-Si eutectic alloy
    Korkut, M. H.
    Eren, H.
    TRIBOLOGY-MATERIALS SURFACES & INTERFACES, 2007, 1 (03) : 154 - 160
  • [29] Nanocrystalline eutectic Al-Si alloy produced by cryomilling
    Milligan, J.
    Vintila, R.
    Brochu, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 508 (1-2): : 43 - 49
  • [30] CRYSTAL MORPHOLOGY OF MASSIVE EUTECTIC SILICON IN UNMODIFIED AL-SI EUTECTIC
    SHAMSUZZOHA, M
    HOGAN, LM
    METALLOGRAPHY, 1989, 22 (01): : 37 - 45