Thin-Film Deposition of Silicon-Incorporated Diamond-Like Carbon by Plasma-Enhanced Chemical Vapor Deposition Using Monomethylsilane as a Silicon Source

被引:17
|
作者
Nakazawa, Hideki [1 ]
Asai, Yuhki [1 ]
Kinoshita, Takeshi [1 ]
Suemitsu, Maki [2 ]
Abe, Toshimi [3 ]
Yasui, Kanji [4 ]
Itoh, Takashi [2 ]
Endoh, Tetsuo [5 ]
Narita, Yuzuru [6 ]
Konno, Atsushi [2 ]
Enta, Yoshiharu [1 ]
Mashita, Masao [1 ]
机构
[1] Hirosaki Univ, Fac Sci & Technol, Aomori 0368561, Japan
[2] Tohoku Univ, Interdisciplinary Res Ctr, Sendai, Miyagi 9808578, Japan
[3] Tohoku Inst Technol, Sendai, Miyagi 9828577, Japan
[4] Nagaoka Univ Technol, Niigata 9402188, Japan
[5] Tohoku Univ, Res Inst Elect Commun, Sendai, Miyagi 9808577, Japan
[6] Kyushu Inst Technol, Kitakyushu, Fukuoka 8048550, Japan
关键词
diamond-like carbon; chemical vapor deposition; monomethylsilane; methane; argon; structural properties; internal stress;
D O I
10.1143/JJAP.47.8491
中图分类号
O59 [应用物理学];
学科分类号
摘要
We have deposited Si-incorporated diamond-like carbon (DLC) films by radio-frequency plasma-enhanced chemical vapor deposition using methane, argon, and monomethylsilane (MMS: CH3SiH3) as a silicon source, and have investigated the structural and mechanical properties of the films. The deposition rate and Si atomic fraction [Si/(Si + C) in the DLC films increased with increasing MMS flow ratio. The Si fraction was approximately 13% at a MMS flow ratio [MMS/(MMS + CH4)] of 3%, showing that the deposition using a combination of CH4 and MMS produces films with high Si content compared with those deposited using conventional C and Si sources. The Si fraction was also found to increase with a decrease in Ar flow rate under a constant MMS flow ratio. Many particles composed mainly of Si, whose size was 0.3-1 mu m in diameter, were observed on the surface when deposition was carried out at MMS flow ratios of 15 and 30%. Compressive internal stress in the films decreased with the MMS flow ratio and/or with the Ar flow rate. The decrease in internal stress is probably due to the relaxation of a three-dimensional rigid network by the formation of Si-C and Si-H bonds in the films are well as Ar+ ion bombardment. [DOI: 10.1143/JJAP.47.8491]
引用
收藏
页码:8491 / 8497
页数:7
相关论文
共 50 条
  • [21] Surface studies of diamond-like carbon films grown by plasma-enhanced chemical vapor deposition
    Maheswaran, R.
    Sivaraman, R.
    Mahapatra, O.
    Rao, P. C.
    Gopalakrishnan, C.
    Thiruvadigal, D. J.
    [J]. SURFACE AND INTERFACE ANALYSIS, 2010, 42 (12-13) : 1702 - 1705
  • [22] Fluorinated amorphous diamond-like carbon films deposited by plasma-enhanced chemical vapor deposition
    Yu, GQ
    Tay, BK
    Sun, Z
    [J]. SURFACE & COATINGS TECHNOLOGY, 2005, 191 (2-3): : 236 - 241
  • [23] Hydrogen Effects on the Properties of Silicon/Nitrogen-Coincorporated Diamond-Like Carbon Films Prepared by Plasma-Enhanced Chemical Vapor Deposition
    Nakazawa, Hideki
    Okuno, Saori
    Miura, Soushi
    Kamata, Ryosuke
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS, 2012, 51 (07)
  • [24] THIN-FILM DEPOSITION ON INSIDE SURFACES BY PLASMA-ENHANCED CHEMICAL-VAPOR-DEPOSITION
    JANSEN, F
    KROMMENHOEK, S
    [J]. THIN SOLID FILMS, 1994, 252 (01) : 32 - 37
  • [25] Growth of diamond-like carbon thin film using microwave chemical vapor deposition
    Ooi, H. T.
    Ibrahim, K.
    [J]. FUNCTIONAL MATERIALS AND DEVICES, 2006, 517 : 57 - 60
  • [27] High-mobility nanocrystalline silicon thin-film transistors fabricated by plasma-enhanced chemical vapor deposition
    Lee, CH
    Sazonov, A
    Nathan, A
    [J]. APPLIED PHYSICS LETTERS, 2005, 86 (22) : 1 - 3
  • [28] Atomic hydrogen etching of silicon-incorporated diamond-like carbon films prepared by pulsed laser deposition
    Nakazawa, H.
    Sugita, H.
    Enta, Y.
    Suemitsu, M.
    Yasui, K.
    Itoh, T.
    Endoh, T.
    Narita, Y.
    Mashita, M.
    [J]. DIAMOND AND RELATED MATERIALS, 2009, 18 (5-8) : 831 - 834
  • [29] Synthesis and characterization of diamond-like carbon coatings for drill bits using plasma-enhanced chemical vapor deposition
    Vijaykumar S. Jatti
    Eyob Messele Sefene
    Ashwini V. Jatti
    Akshansh Mishra
    Rahul D. Dhabale
    [J]. The International Journal of Advanced Manufacturing Technology, 2023, 127 : 4081 - 4096
  • [30] Synthesis and characterization of diamond-like carbon coatings for drill bits using plasma-enhanced chemical vapor deposition
    Jatti, Vijaykumar S. S.
    Sefene, Eyob Messele
    Jatti, Ashwini V. V.
    Mishra, Akshansh
    Dhabale, Rahul D. D.
    [J]. INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 127 (9-10): : 4081 - 4096