Effect of the Electro-Chemical Hydrogen Charging lime on Hydrogen Embrittlement of X70 Steel Using for Gas Pipeline

被引:3
|
作者
Sung, Chi-Eun [1 ]
Jeon, Hyeon-Jee [1 ]
Lee, Jin-Kyung [2 ]
Son, In-Soo [2 ]
Lee, Sang-Pill [2 ]
Lee, Seok-Cheol [3 ]
Baek, Un-Bong [3 ]
Nahm, Seung-Hoon [3 ]
Bae, Dong-Su [1 ]
机构
[1] Dong Eui Univ, Dept Adv Mat Engn, Pusan 614714, South Korea
[2] Dong Eui Univ, Dept Mech Engn, Pusan 614714, South Korea
[3] KRISS, Ctr Mat Measurements, Taejon 305340, South Korea
来源
关键词
embrittlement; electro-chemical hydrogen charging; alloys; mechanical properties; scanning electron microscopy (SEM); MICROSTRUCTURE; SUSCEPTIBILITY;
D O I
10.3365/KJMM.2013.51.11.813
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigated the effect of the hydrogen charging time under the electro-chemical hydrogen charging condition on hydrogen embrittlement of hot-rolled and then air-cooled API X70 steel. Tensile and V-notch Charpy impact test specimens were held for 0 h, 2 h, 4 h, and 10 h in the electrolyte pot during electro-chemical hydrogen charging processes and then both of tensile and impact tests were completed at room temperature. The microstructure consisted of fine acicular ferrite, coarse polygonal ferrite and pearlite. The yield and tensile strength decreased slightly and elongation decreased rapidly up to 2 h holding time and then decreased slowly with the holding time. The V-notch Charpy impact value decreased continuously up to 4 h holding time and then increased slightly up to 10 h. The morphology of the fracture surface changed from a ductile type to a brittle type with the hydrogen charging time. Secondary cracks were observed in the hydrogen charged specimens. No external cracks were formed at the specimen surface of the tensile tested with 0 h holding time, but many external cracks were observed at the surface of the hydrogen charged specimens. Cracks were observed in the nominal and parallel directions to the tensile direction at the longitudinal cross-section region near the tensile fractured surface with the 2 h held specimen.
引用
收藏
页码:813 / 820
页数:8
相关论文
共 50 条
  • [41] EFFECT OF MICROSTRUCTURAL CONSTITUENTS ON HYDROGEN EMBRITTLEMENT RESISTANCE OF API X60, X70, AND X80 PIPELINE STEELS
    Shin, Seung-Hyeok
    Oh, Dong-Kyu
    Kim, Sang-Gyu
    Hwang, Byoungchul
    ARCHIVES OF METALLURGY AND MATERIALS, 2024, 69 (02) : 415 - 419
  • [42] Manipulating nano-WS2 aggregates in electroplated Ni coating to mitigate hydrogen embrittlement in X70 pipeline steel
    Xue, Jinxin
    Zhou, Chilou
    Dai, Pengzhi
    Liu, Xianhui
    Wu, Hao
    Li, Xinfeng
    Chu, Paul K.
    Corrosion Science, 2024, 241
  • [43] 3D cohesive modelling of hydrogen embrittlement in the heat affected zone of an X70 pipeline steel - Part II
    Alvaro, Antonio
    Olden, Vigdis
    Akselsen, Odd Magne
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2014, 39 (07) : 3528 - 3541
  • [44] Comparative Study on Hydrogen Embrittlement Susceptibility of X60 and X70 Pipeline Steels and Their Welded Joints
    Wang W.
    Chen Y.
    Zhan X.
    Liu J.
    Tang W.
    Surface Technology, 2024, 53 (04): : 117 - 124
  • [45] The effect of hydrogen peroxide on crack growth rate in X70 pipeline steel under static load
    Bogdanov, R. I.
    Ignatenko, V. E.
    Marshakov, A. I.
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2013, 49 (05) : 574 - 579
  • [46] Effect of hydrogen peroxide on crack growth rate in X70 pipeline steel in weak acid solution
    Bogdanov, Roman
    Marshakov, Andrey
    Ignatenko, Vasiliy
    Ryakhovskikh, Ilya
    Bachurina, Diana
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2017, 52 (04) : 294 - 301
  • [47] The effect of hydrogen peroxide on crack growth rate in X70 pipeline steel under static load
    R. I. Bogdanov
    V. E. Ignatenko
    A. I. Marshakov
    Protection of Metals and Physical Chemistry of Surfaces, 2013, 49 : 574 - 579
  • [48] Influence of stress triaxiality on hydrogen assisted ductile damage in an X70 pipeline steel
    Depraetere, Robin
    De Waele, Wim
    Cauwels, Margo
    Depover, Tom
    Verbeken, Kim
    Boone, Matthieu
    Hertele, Stijn
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 864
  • [49] Hydrogen trapping and hydrogen embrittlement (HE) susceptibility of X70 grade high-strength, acid-resistant, submarine pipeline steel with Mg treatment
    Lang, Fengjun
    Huang, Feng
    Yue, Jiangbo
    Li, Liwei
    Xu, Jinqiao
    Liu, Jing
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 24 : 623 - 638
  • [50] Effect of Stress on Hydrogen Permeation for X70 Carbon Steel in Seawater
    Zheng, Chuanbo
    Wang, Cheng
    MATERIALS PERFORMANCE, 2017, 56 (08) : 54 - 58