In situ observation of solidification of undercooled hypoeutectic Ni-Ni3B alloy melt

被引:14
|
作者
Xu, Junfeng [1 ,2 ]
Liu, Feng [1 ,2 ]
Zhang, Di [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Shaanxi, Peoples R China
[2] Xian Technol Univ, Sch Mat & Chem Engn, Dept Met Mat Engn, Xian 710032, Peoples R China
关键词
ANOMALOUS EUTECTIC FORMATION; RAPID SOLIDIFICATION; PHASE SELECTION; NI-B; SOLID FRACTION; HEAT-FLOW; BEHAVIOR; GROWTH; MICROSTRUCTURE; NUCLEATION;
D O I
10.1557/jmr.2013.165
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Solidification of undercooled Ni-3.3 wt% B alloy melt was investigated by glass fluxing. If Delta T-e, < 140 +/- 10 K, two recalescences appear, indicating that stable eutectic reaction occurs; if Delta T-e >= 140 +/- 10 K, three recalescences can be observed, indicating that metastable eutectic reaction occurs. Analysis indicates that the phase fractions of the as-solidified structure can be predicted by the recalescence delay times in the cooling curves. High-speed video images show that the solidification interface of primary solidification changes from single dendritic shape to spherical shape with increasing Delta T-p; the interface of eutectic solidification changes from many small "dendrites" to a single large one with increasing Delta T-e; the interface of residual liquid solidification changes from many small rings to a single large one with increasing Delta T-r. The growth velocity of eutectic solidification suggests a coupled growth at small and moderate undercoolings and decoupled growth at large undercooling, whereas that of residual liquid solidification cannot be interpreted by the available models.
引用
收藏
页码:1891 / 1902
页数:12
相关论文
共 50 条
  • [31] Transition from hypereutectic to hypoeutectic for rapid solidification in an undercooled Co-B alloy
    He, Yixuan
    Li, Jinshan
    Wang, Jun
    Beaugnon, Eric
    JOURNAL OF CRYSTAL GROWTH, 2018, 499 : 98 - 105
  • [32] Solidification behavior of decagonal quasicrystal in the undercooled Al72Ni12Co16 alloy melt
    Liu, XB
    Yang, GC
    Fan, P
    JOURNAL OF MATERIALS SCIENCE, 2003, 38 (05) : 885 - 889
  • [33] Solidification behavior of decagonal quasicrystal in the undercooled Al72Ni12Co16 alloy melt
    Xinbao Liu
    Gencang Yang
    Ping Fan
    Journal of Materials Science, 2003, 38 : 885 - 889
  • [34] Undercooled solidification of Ni-3.3 wt-%B alloy and cooling curve description
    Xu, J. F.
    Liu, F.
    Xu, X. L.
    Dang, B.
    MATERIALS SCIENCE AND TECHNOLOGY, 2013, 29 (01) : 36 - 42
  • [35] Solidification structure of undercooled Ni54.6Pd45.4 alloy
    Lu, S. Y.
    Li, J. F.
    Zhou, Y. H.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 460 : 63 - 68
  • [36] In Situ Observation of the Competition Between Metastable and Stable Phases in Solidification of Undercooled Fe-17at. pctB Alloy Melt
    Zhang, Di
    Xu, Junfeng
    Liu, Feng
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (11): : 5232 - 5239
  • [37] In Situ Observation of the Competition Between Metastable and Stable Phases in Solidification of Undercooled Fe-17at. pctB Alloy Melt
    Di Zhang
    Junfeng Xu
    Feng Liu
    Metallurgical and Materials Transactions A, 2015, 46 : 5232 - 5239
  • [38] Disorder trapping during the solidification of βNi3Ge from its deeply undercooled melt
    Ahmad, R.
    Cochrane, R. F.
    Mullis, A. M.
    JOURNAL OF MATERIALS SCIENCE, 2012, 47 (05) : 2411 - 2420
  • [39] Disorder trapping during the solidification of βNi3Ge from its deeply undercooled melt
    R. Ahmad
    R. F. Cochrane
    A. M. Mullis
    Journal of Materials Science, 2012, 47 : 2411 - 2420
  • [40] In situ observation of phase selection in undercooled Ni-Al melts
    Shuleshova, O.
    Holland-Moritz, D.
    Loeser, W.
    Lindenkreuz, H. -G.
    Buechner, B.
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2009, 22 (1-4) : 286 - 289