Constitutive equations for hot deformation of an Al-6061/20%Al2O3 composite

被引:42
|
作者
Spigarelli, S
Evangelista, E
Cerri, E
Langdon, TG
机构
[1] Univ Ancona, INFM, Dept Mech, I-60131 Ancona, Italy
[2] Univ Lecce, INFM, Dept Ingn Innovaz, I-70131 Lecce, Italy
[3] Univ So Calif, Dept Mat Sci & Engn, Los Angeles, CA 90089 USA
关键词
hot deformation; composites; constitutive equations; torsion testing;
D O I
10.1016/S0921-5093(01)01071-1
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The hot deformation response of an Al-6061 + 20%Al2O3 particulate composite was investigated by means of torsion tests. An analysis of the flow stress dependence on strain rate and temperature gave a stress exponent of n approximate to 5.6 and an activation energy of Q approximate to 150 kJ mol(-1). This value of Q is reasonably close to the anticipated value for self-diffusion in Al. The results are in excellent agreement with other studies carried out on the hot deformation of composites but the phenomenological nature of the constitutive equation does not permit an unambiguous determination of the rate-controlling flow mechanism. Nevertheless, it is shown that an identical constitutive equation may be used to describe the creep of composites under both shear and hot torsion conditions. It is concluded that the mechanism controlling hot deformation and creep at high stresses is the climb of dislocations. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:721 / 725
页数:5
相关论文
共 50 条
  • [11] EFFECT OF HEAT TREATMENT ON FRICTION AND WEAR BEHAVIOR OF Al-6061 COMPOSITE REINFORCED WITH 10% SUBMICRON Al2O3 PARTICLES
    Al-Qutub, Amro M.
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2009, 34 (1B) : 205 - 215
  • [12] Fabrication and Mechanical Behaviour of Al-6061/Al2O3 Metal Matrix Composite Fabricated Through Powder Metallurgy Technique
    Gurusamy, P.
    Muthuraman, V.
    Lokeshkumar, J.
    Hari Krishna Raj, S.
    International Journal of Vehicle Structures and Systems, 2022, 14 (01) : 47 - 49
  • [13] An analysis of hot formability of the 6061+20% Al2O3 composite by means of different stability criteria
    Spigarelli, S
    Cerri, E
    Cavaliere, P
    Evangelista, E
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 327 (02): : 144 - 154
  • [14] AGE-HARDENING IN 6061AL ALLOY AND AL2O3/6061AL COMPOSITE
    YU, D
    CHANDRA, T
    MATERIALS TRANSACTIONS JIM, 1993, 34 (12): : 1184 - 1190
  • [15] Superplasticity in a hot extruded 15%vol. Al2O3 particulate reinforced 6061 Al composite
    Han, LH
    Hu, H
    Northwood, D
    Niu, JT
    ADVANCES IN SUPERPLASTICITY AND SUPERPLASTIC FORMING, 2004, : 185 - 192
  • [16] HOT DEFORMATION MECHANISMS IN A 10-VOL-PERCENT AL2O3 PARTICLE-REINFORCED 6061-AL MATRIX COMPOSITE
    XIA, XX
    MCQUEEN, HJ
    SAKARIS, P
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (08): : 1185 - 1190
  • [17] Mathematical modeling of the extrusion of 6061/Al2O3/20p composite
    Chen, WC
    Davies, CHJ
    Samarasekera, IV
    Brimacombe, JK
    Hawbolt, EB
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (12): : 4095 - 4111
  • [18] Effect of Flyash Treatment on the Properties of Al-6061 Alloy Reinforced with SiC–Al2O3–C Mixture
    R. Govinda Rao
    K. L. Sahoo
    R. I. Ganguly
    R. R. Dash
    N. Narasaiah
    Transactions of the Indian Institute of Metals, 2017, 70 : 2707 - 2717
  • [19] Synthesis of an Al/Al2O3 composite by severe plastic deformation
    Kuncicka, Lenka
    Lowe, Terry C.
    Davis, Casey F.
    Kocich, Radim
    Pohludka, Martin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 646 : 234 - 241
  • [20] Instability map for hot working of 6061 Al-10 vol% Al2O3 metal matrix composite
    Murty, SVSN
    Rao, BN
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 1998, 31 (22) : 3306 - 3311