Convective Drying of Beech Lumber without Color Changes of Wood

被引:0
|
作者
Dzurenda, Ladislav [2 ]
Deliiski, Nencho [1 ]
机构
[1] Univ Forestry, Fac Forest Ind, 10 Kliment Ohridski Blvd, Sofia 1756, Bulgaria
[2] Tech Univ Zvolen, Fac Wood Sci & Technol, Zvolen, Slovakia
关键词
beech lumber; convective drying; regime of drying; color of wood;
D O I
暂无
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
This paper presents the results of analyzing the influence of suggested regimes of chamber drying of beech lumber with the thickness h = 40 mm, h = 60 mm and h = 80 mm from the initial moisture content W-p = 70 % to the final moisture content W-k = 8 %. The regimes ensure the preservation of the natural color of the wood. The study results show that the drying of beech lumber according to the suggested regimes causes no changes in the chromophoric compounds of the wood and the beech lumber preserves its original white-yellow color Quality parameters of the dried lumber such as: difference between the average final moisture content and the required final moisture content, and the range of the final moisture and moisture gradient in dried beech lumber classify this dried lumber into the first quality class. The suggested regimes for drying beech lumber using hot air in the temperature range t(s) = 37 divided by 65 degrees C has a negative impact on the duration of the drying process. In comparison with the regimes of beech lumber drying according to ON 49 0651, carried out at temperatures t = 60 divided by 80 degrees C, the duration of drying beech lumber with the thickness h = 40 mm according to the suggested regime is 1.9 times longer the duration of drying beech lumber with the thickness h = 60 mm is 2.3 times longer and the duration of drying beech lumber with the thickness h = 80 111117 is 2.9 times longer The specific heat energy consumption of beech lumber with the initial moisture content W = 70 % to the final moisture content W-k = 8 % in a chamber type KWC 121, according to the suggested regimes, is equals to Q(TZN) = 514.46 kWh.m(-3) for the thickness h = 40 Q(TZN) = 557.62 kWh.m(-3) for lumber with the thickness h = 60 mm, and Q(TZN) = 643.16 kWh-m(-3) for lumber with the thickness h = 80 mm. The specific heat energy consumption needed for the drying of l m(3) of beech lumber with the thickness h = 60 mm according to the suggested regime is by 26.89% higher than the specific heat energy consumption used to dry beech lumber of the same thickness according to the regime of beech lumber drying by Vzduchotechnika a.s. which does not preserve the natural color of the wood.
引用
收藏
页码:95 / 103
页数:9
相关论文
共 50 条
  • [41] Control of Lumber Drying Process in the Microwave Cavity-Type Wood-Drying Kiln
    Melekhov, V., I
    Shul'gin, V. A.
    LESNOY ZHURNAL-FORESTRY JOURNAL, 2016, (01) : 122 - 130
  • [42] Systematization of Factors Affecting the Cracking of Larch Lumber during Wood Drying
    Zaripov, Sh G.
    LESNOY ZHURNAL-FORESTRY JOURNAL, 2018, (03) : 127 - 136
  • [43] Effects of sub-macroscopic structure of wood in lumber drying process
    Petr, K
    WOOD RESEARCH, 2003, 48 (03) : 17 - 26
  • [44] Natural Variability of the Color of Beech Wood in the Color Space CIE L*a*b*
    Dzurenda, Ladislav
    FORESTS, 2023, 14 (06):
  • [45] Computer Vision for Real-Time Measurements of Shrinkage and Color Changes in Blueberry Convective Drying
    Chen, Yougui
    Martynenko, Alex
    DRYING TECHNOLOGY, 2013, 31 (10) : 1114 - 1123
  • [46] The influence of the drying medium on high temperature convective drying of single wood chips
    Johansson, A
    Rasmuson, A
    DRYING TECHNOLOGY, 1997, 15 (6-8) : 1801 - 1813
  • [47] CHANGES OF CHEMICAL-COMPONENTS AND COLOR OF WOOD OF SUGI, CRYPTOMERIA-JAPONICA, DURING DRYING WITHOUT LOPPING AFTER FELLING IN THE FOREST
    HAYASHI, Y
    OHARA, S
    FURUTA, M
    KUROSU, H
    KITAMURA, Y
    MOKUZAI GAKKAISHI, 1988, 34 (11): : 934 - 941
  • [48] The influence of the drying medium on high temperature convective drying of single wood chips
    Johansson, A
    Rasmuson, A
    DRYING '96, VOL A, 1996, : 671 - 678
  • [49] Changes Caused by Heat Treatment in Color and Dimensional Stability of Beech (Fagus sylvatica L.) Wood
    Mitani, Andromachi
    Barboutis, Ioannis
    DRVNA INDUSTRIJA, 2014, 65 (03) : 225 - 232
  • [50] EFFECT OF DRYING PROCESS ON MARUPA WOOD COLOR
    Goncalez, Joaquim Carlos
    Bezerra Marques, Marcia Helena
    Sousa Karas, Maria Cristina
    Janin, Gerard
    Ribeiro, Patricia Gomes
    MADERAS-CIENCIA Y TECNOLOGIA, 2014, 16 (03): : 337 - 342