Toughening of Ti3SiC2 with 3Y-TZP addition by spark plasma sintering

被引:17
|
作者
Shi, Sui Lin [1 ]
Pan, Wei [1 ]
机构
[1] Tsing Hua Univ, Dept Mat Sci & Engn, State Key Lab New Ceram & Fine Proc, Beijing 100084, Peoples R China
基金
中国国家自然科学基金;
关键词
composite materials; mechanical properties; spark plasma sintering; Ti3SiC2; Y-TZP;
D O I
10.1016/j.msea.2006.10.038
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
3 mol% Yttria-stabilized tetragonal zirconia (3Y-TZP)/Ti3SiC2 composites with different 3Y-TZP content were fabricated by Spark Plasma Sintering (SPS) at 1300 degrees C. The effect of 3Y-TZP content on room-temperature mechanical properties and microstructures of the composites was investigated. The Vickers hardness of the composites increased with the increasing of the 3Y-TZP content. The bending strength and fracture toughness of the composites exhibit the decrease and increase respectively, as the 3Y-TZP content was less than 30 vol.%, whereas they showed the increase and decrease, respectively, as the 3Y-TZP content was higher than 30 vol.%. The maximum fracture toughness of 11.94 MPa m(1/2) was achieved for the composite with 30 vol.% 3Y-TZP. The increased fracture toughness involved multiple-toughening behaviors, in which the phase transformation toughening, the crack deflection, and delamination may all have mainly contributed to the improvement of fracture toughness. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:303 / 306
页数:4
相关论文
共 50 条
  • [21] Synthesis of Ti3SiC2 by spark plasma sintering(SPS) of elemental powders
    朱教群
    梅炳初
    何利萍
    陈艳林
    Transactions of Nonferrous Metals Society of China, 2003, (01) : 46 - 49
  • [22] Stability of Nanocrystalline Spark Plasma Sintered 3Y-TZP
    Chintapalli, Ravikiran
    Mestra, Alvaro
    Marro, Fernando Garcia
    Yan, Haixue
    Reece, Michael
    Anglada, Marc
    MATERIALS, 2010, 3 (02): : 800 - 814
  • [23] Toughening of SiC with Ti3SiC2 particles
    Mogilevsky, P
    Mah, TI
    Parthasarathy, TA
    Cooke, CM
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2006, 89 (02) : 633 - 637
  • [24] Machinable Ti3SiC2/Hydroxyapatite Bioceramic Composites Prepared by Spark Plasma Sintering
    Jing Zhang
    MRS Bulletin, 2007, 32 : 996 - 996
  • [25] Synthesis of fine grain Ti3SiC2 by spark plasma sintering with additive of aluminum
    Han Ruobing
    Pan Wei
    Fang Minghao
    Shi Suilin
    Qi Longhao
    HIGH-PERFORMANCE CERAMICS IV, PTS 1-3, 2007, 336-338 : 1046 - 1049
  • [27] Rapid fabrication of the Ti3SiC2 bonded diamond composite by spark plasma sintering
    Mu, Yunchao
    Guo, Jifeng
    Liang, Baoyan
    Wang, Qinsheng
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2011, 29 (03): : 397 - 400
  • [28] Effect of aluminum on fabrication of Ti3SiC2 by mechanical alloying and spark plasma sintering
    Jin, Songzhe
    Liang, Baoyan
    Li, Jing-Feng
    Li, Li
    High-Performance Ceramics IV, Pts 1-3, 2007, 336-338 : 1065 - 1068
  • [29] In-situ synthesis of TiC/SiC/Ti3SiC2 composite coatings by spark plasma sintering
    Singh, Ashish
    Bakshi, Srinivasa R.
    Virzi, David A.
    Keshri, Anup K.
    Agarwal, Arvind
    Harimkar, Sandip P.
    SURFACE & COATINGS TECHNOLOGY, 2011, 205 (13-14): : 3840 - 3846
  • [30] Effect of CuO addition on the sintering behavior and electrical conductivity of 3Y-TZP
    Hassan, Ahmed A.
    Abdelal A., Omar
    El-Hout, S. M.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2007, 23 (01) : 131 - 134