On the Vickers indentation fracture toughness test

被引:545
|
作者
Quinn, George D. [1 ]
Bradt, Richard C.
机构
[1] Natl Inst Stand & Technol, Gaithersburg, MD 20899 USA
[2] Univ Alabama, Dept Met & Mat Sci, Coll Engn, Tuscaloosa, AL 35487 USA
关键词
D O I
10.1111/j.1551-2916.2006.01482.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Vickers indentation fracture toughness test, or VIF, is addressed by considering its origins and the numerous equations that have been applied along with the technique to estimate the fracture resistance, or the K-Ic of ceramics. Initiation and propagation of cracks during the VIF test are described and contrasted with the pre-cracking and crack growth for internationally standardized fracture toughness tests. It is concluded that the VIF test technique is fundamentally different than standard fracture toughness tests. The VIF test has a complex three-dimensional crack system with substantial deformation residual stresses and damage around the cracks. The VIF test relates to an ill-defined crack arrest condition as opposed to the rapid crack propagation of the standardized fracture toughness tests. Previously published fracture toughness results employing the VIF technique are reviewed. These reveal serious discrepancies in reported VIF fracture toughness values. Finally, recent fracture resistance measurements by the VIF technique for the Standard Reference Material SRM 2100 are presented. These are compared with standardized test results for the same material. It is concluded that the VIF technique is not reliable as a fracture toughness test for ceramics or for other brittle materials. What the VIF actually measures in terms of fracture resistance cannot be readily defined. It is recommended that the VIF technique no longer be acceptable for the fracture toughness testing of ceramic materials.
引用
收藏
页码:673 / 680
页数:8
相关论文
共 50 条
  • [31] Determination of fracture toughness using the area of micro-crack tracks left in brittle materials by Vickers indentation test
    Moradkhani, Alireza
    Baharvandi, Hamidreza
    Tajdari, Mehdi
    Latifi, Hamidreza
    Martikainen, Jukka
    JOURNAL OF ADVANCED CERAMICS, 2013, 2 (01) : 87 - 102
  • [32] INVESTIGATION BY VICKERS INDENTATION OF THE FRACTURE-TOUGHNESS OF EXPERIMENTAL BATCHES OF SINTERED POLYCRYSTALLINE SIC
    MOUSSA, R
    CHERMANT, JL
    OSTERSTOCK, F
    REVUE INTERNATIONALE DES HAUTES TEMPERATURES ET DES REFRACTAIRES, 1982, 19 (03): : 225 - 238
  • [33] An improved Vickers indentation fracture toughness model to assess the quality of thermally sprayed coatings
    Faisal, N. H.
    Ahmed, R.
    Prathuru, A. K.
    Spence, S.
    Hossain, M.
    Steel, J. A.
    ENGINEERING FRACTURE MECHANICS, 2014, 128 : 189 - 204
  • [34] Young's modulus, Vickers hardness and indentation fracture toughness of alumino silicate glasses
    Tiegel, Mirko
    Hosseinabadi, Reza
    Kuhn, Stefan
    Herrmann, Andreas
    Ruessel, Christian
    CERAMICS INTERNATIONAL, 2015, 41 (06) : 7267 - 7275
  • [35] A Study of the Microstructure and Vickers Indentation Fracture Toughness of Silicon Carbide Coatings on TRISO Fuel Particles
    Zhang, Huixing
    Lopez-Honorato, Eddie
    Javed, Athar
    Shapiro, Ian
    Xiao, Ping
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (03) : 1086 - 1092
  • [36] Fracture Toughness of 3Y-TZP Dental Ceramics by Using Vickers Indentation Fracture and SELNB Methods
    Moradkhani, Alireza
    Baharvandi, Hamidreza
    Naserifar, Ali
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2019, 56 (01) : 37 - 48
  • [37] Critical evaluation of indentation fracture toughness measurements with Vickers indenter on ceramic matrix composite tools
    Gatto, A.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2006, 174 (1-3) : 67 - 73
  • [38] USE OF VICKERS INDENTATION METHOD FOR EVALUATION OF FRACTURE-TOUGHNESS OF PHASE-SEPARATED GLASSES
    MIYATA, N
    JINNO, H
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1980, 38-9 (MAY-) : 391 - 396
  • [39] Vickers microhardness and indentation fracture toughness of tantalum sesquinitride, η-Ta2N3
    Bourguille, Judith
    Brinza, Ovidiu
    Zerr, Andreas
    CERAMICS INTERNATIONAL, 2016, 42 (01) : 982 - 985
  • [40] Estimation of fracture toughness of nitride compound layers on tool steel by application of the Vickers indentation method
    Nolan, D.
    Leskovsek, V.
    Jenko, M.
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (1-2): : 182 - 188