被引:545
|
作者
Quinn, George D. [1 ]
Bradt, Richard C.
机构
[1] Natl Inst Stand & Technol, Gaithersburg, MD 20899 USA
[2] Univ Alabama, Dept Met & Mat Sci, Coll Engn, Tuscaloosa, AL 35487 USA
关键词
D O I
10.1111/j.1551-2916.2006.01482.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Vickers indentation fracture toughness test, or VIF, is addressed by considering its origins and the numerous equations that have been applied along with the technique to estimate the fracture resistance, or the K-Ic of ceramics. Initiation and propagation of cracks during the VIF test are described and contrasted with the pre-cracking and crack growth for internationally standardized fracture toughness tests. It is concluded that the VIF test technique is fundamentally different than standard fracture toughness tests. The VIF test has a complex three-dimensional crack system with substantial deformation residual stresses and damage around the cracks. The VIF test relates to an ill-defined crack arrest condition as opposed to the rapid crack propagation of the standardized fracture toughness tests. Previously published fracture toughness results employing the VIF technique are reviewed. These reveal serious discrepancies in reported VIF fracture toughness values. Finally, recent fracture resistance measurements by the VIF technique for the Standard Reference Material SRM 2100 are presented. These are compared with standardized test results for the same material. It is concluded that the VIF technique is not reliable as a fracture toughness test for ceramics or for other brittle materials. What the VIF actually measures in terms of fracture resistance cannot be readily defined. It is recommended that the VIF technique no longer be acceptable for the fracture toughness testing of ceramic materials.
引用
收藏
页码:673 / 680
页数:8
相关论文
共 50 条
  • [1] VICKERS INDENTATION FRACTURE-TOUGHNESS TEST .1. REVIEW OF LITERATURE AND FORMULATION OF STANDARDIZED INDENTATION TOUGHNESS EQUATIONS
    PONTON, CB
    RAWLINGS, RD
    MATERIALS SCIENCE AND TECHNOLOGY, 1989, 5 (09) : 865 - 872
  • [2] A Work Approach to Determine Vickers Indentation Fracture Toughness
    Feng, Yihui
    Zhang, Taihua
    Yang, Rong
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2011, 94 (02) : 332 - 335
  • [3] An investigation into the fracture toughness of nitrided layers by Vickers indentation
    Boniardi, M
    Bozzini, B
    Martinelli, GC
    REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 1999, 96 (02): : 253 - 258
  • [4] New developments for fracture toughness determination by Vickers indentation
    Chicot, D
    Pertuz, A
    Roudet, F
    Staia, MH
    Lesage, J
    MATERIALS SCIENCE AND TECHNOLOGY, 2004, 20 (07) : 877 - 884
  • [5] VICKERS INDENTATION FRACTURE-TOUGHNESS TEST .2. APPLICATION AND CRITICAL-EVALUATION OF STANDARDIZED INDENTATION TOUGHNESS EQUATIONS
    PONTON, CB
    RAWLINGS, RD
    MATERIALS SCIENCE AND TECHNOLOGY, 1989, 5 (10) : 961 - 976
  • [6] Methodology for measuring fracture toughness of ceramic materials by instrumented indentation test with vickers indenter
    Ma, Dejun
    Wang, Jialiang
    Sun, Liang
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2017, 100 (05) : 2296 - 2308
  • [7] FRACTURE-TOUGHNESS TEST OF SILICON NITRIDES WITH DIFFERENT MICROSTRUCTURES USING VICKERS INDENTATION
    Miyazaki, Hiroyuki
    Hyuga, Hideki
    Yoshizawa, Yu-ichi
    Hirao, Kiyoshi
    Ohji, Tatsuki
    MECHANICAL PROPERTIES AND PERFORMANCE OF ENGINEERING CERAMICS AND COMPOSITES III, 2008, 28 (02): : 433 - 442
  • [8] FRACTURE-TOUGHNESS OF GERMANIUM DETERMINED WITH THE VICKERS INDENTATION TECHNIQUE
    LEMAITRE, P
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1988, 7 (08) : 895 - 896
  • [9] Evaluation by Vickers indentation of fracture toughness of a phosphate biodegradable glass
    Clément, J
    Torres, P
    Gil, FJ
    Planell, JA
    Terradas, R
    Martinez, S
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1999, 10 (07) : 437 - 441
  • [10] Fracture Toughness of Alumina Ceramics Determined by Vickers Indentation Technique
    Majic, Marijana
    Curkovic, Lidija
    MATERIALS TESTING, 2012, 54 (04) : 228 - 232