Pitting of AISI 304 stainless steel in bicarbonate and chloride solutions

被引:34
|
作者
Drogowska, M [1 ]
Menard, H [1 ]
Brossard, L [1 ]
机构
[1] INST RECH HYDRO QUEBEC, VARENNES, PQ J3X 1S1, CANADA
基金
加拿大自然科学与工程研究理事会;
关键词
D O I
10.1023/A:1018499823288
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Metastable and stable pitting on 304 stainless steel (SS304) in 0.1-0.5 M NaCl aqueous solution (pH similar to 8) has been investigated using a potentiodynamic, a potentiostatic and a weak anodic current galvanostatic techniques. The addition of bicarbonate (0.025-0.5 M) to the solution had an inhibiting effect manifested by a shift of the pitting potentials to more positive values, a longer induction time for pitting and reduced pit nucleation. The pit nucleation frequency and growth, in the metastable and stable states, decrease as the NaHCO3/NaCl molar concentration increases and pitting is no longer observed for NaHCO3/NaCl molar ratios higher than 3 (four times larger % wt of NaHCO3). Pitting events never occurred at a potential below -0.1 V, fewer metastable events were observed at higher temperature (50 degrees C) and none were observed in chloride free bicarbonate solutions. The inhibiting behaviour of oxyanions is discussed.
引用
收藏
页码:169 / 177
页数:9
相关论文
共 50 条
  • [21] Effect of electrolyte composition on the pitting and repassivation behavior of aisi 304 stainless steel at high temperature
    Japan Soc of Corrosion Engineering; Deutsche Bunsen-Geselschaft fuer Physikalische Chemie; Electrochemical Soc, US; Electrochemical Soc of Japan; Inst of Corrosion Science & Technology; et al
  • [22] Corrosion Behavior of Sensitized AISI 304 Stainless Steel in Acid Chloride Solution
    Zatkalikova, Viera
    Uhricik, Milan
    Markovicova, Lenka
    Kucharikova, Lenka
    MATERIALS, 2022, 15 (23)
  • [23] Kurtosis as a Decisive Topographic Parameter for Pitting Attack of AISI 304L Stainless Steel
    Kalhor, Alireza
    Sohrabi, Mohammad Javad
    Mobasheri, Mohammad
    Rodak, Kinga
    Dehghanian, Changiz
    Mirzadeh, Hamed
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2025,
  • [24] Correlation of hydrogen-facilitated pitting of AISI 304 stainless steel to semiconductivity of passive films
    Yang, MZ
    Luo, JL
    Patchet, BM
    THIN SOLID FILMS, 1999, 354 (1-2) : 142 - 147
  • [25] Effect of Surface Finish on the Pitting Corrosion Behavior of Sensitized AISI 304 Austenitic Stainless Steel Alloys in 3.5% NaCl Solutions
    Ezuber H.
    Alshater A.
    Nisar S.O.
    Gonsalvez A.
    Aslam S.
    Surface Engineering and Applied Electrochemistry, 2018, 54 (1) : 73 - 80
  • [26] Passivity and pitting susceptibility of type 304 stainless steel in acidic sulphate solutions
    El-Egamy, SS
    Badawy, WA
    Shehata, H
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2001, 32 (09) : 737 - 742
  • [27] Research on the Failure Mechanism of Pitting Corrosion of the 304 Stainless Steel in Chloride Ions Environment
    Pan, Yi
    Chen, Rongfa
    Wang, Duxiong
    Cai, Guosheng
    Zhang, Xianliang
    Liu, Tao
    PROGRESS IN NEW MATERIALS AND MECHANICS RESEARCH, 2012, 502 : 12 - +
  • [28] Effect of strain and chloride concentration on pitting susceptibility for type 304 austenitic stainless steel
    Lue Guocheng
    Cheng Haidong
    Xu Chunchun
    He Zonghu
    CHINESE JOURNAL OF CHEMICAL ENGINEERING, 2008, 16 (02) : 314 - 319
  • [29] Development of Pitting Corrosion of Stainless Steel 403 in Sodium Chloride Solutions
    Rybalka, K. V.
    Shaldaev, V. S.
    Beketaeva, L. A.
    Malofeeva, A. N.
    Davydov, A. D.
    RUSSIAN JOURNAL OF ELECTROCHEMISTRY, 2010, 46 (02) : 196 - 204
  • [30] Critical pitting and repassivation temperatures for duplex stainless steel in chloride solutions
    Deng, Bo
    Jiang, Yiming
    Gong, Jia
    Zhong, Cheng
    Gao, Juan
    Li, Jin
    ELECTROCHIMICA ACTA, 2008, 53 (16) : 5220 - 5225