Nanoscale zero-valent iron (nZVI) synthesis in a Mg-aminoclay solution exhibits increased stability and reactivity for reductive decontamination

被引:63
|
作者
Hwang, Yuhoon [1 ]
Lee, Young-Chul [2 ,3 ]
Mines, Paul D. [1 ]
Huh, Yun Suk [3 ]
Andersen, Henrik R. [1 ]
机构
[1] Tech Univ Denmark, Dept Environm Engn, DK-2800 Lyngby, Denmark
[2] Korea Adv Inst Sci & Technol, Dept Civil & Environm Engn, Taejon 305701, South Korea
[3] Inha Univ, Coll Engn, Dept Biol Engn, Inchon 402751, South Korea
基金
新加坡国家研究基金会;
关键词
Mg-aminoclay (MgAC); Nanoscale zero-valent iron (nZVI); Nanotechnology; Colloidal stability; CORE-SHELL NANOWIRES; ORGANO-BUILDING BLOCKS; FUNCTIONALIZED MAGNESIUM PHYLLOSILICATE; OLEAGINOUS CHLORELLA SP; FE-0; NANOPARTICLES; POROUS-MEDIA; HUMIC-ACID; NEUTRAL PH; WATER; DEGRADATION;
D O I
10.1016/j.apcatb.2013.10.017
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Nanoscale zero-valent iron (nZVI) has often been explored as a reductant for detoxification of pollutants in environmental clean-ups. Despite the large surface area and superior reactivity of nZVI, its limited stability is a major obstacle in applying nZVI for in situ subsurface remediation, e.g. for chlorinated solvents hotspots. In this study, water-solubilized magnesium-aminoclay (MgAC) was applied for the first time as a stabilizing agent in the synthesis of nZVI. With increased doses of Mg-aminoclay applied in the synthesis mixture, nZVI particle growth was inhibited and thin sheathed grape-like nZVI particles with higher crystallinity were produced. Stability of nZVI particles were evaluated using a sedimentation test and a dynamic light scattering technique. The characteristic time increased from 6.71 to 83.8 min, and particle (aggregate diameter) size decreased from 5132 to 186 nm with increasing amounts of applied MgAC. The higher stability of MgAC coated nZVI could be explained from the higher zeta potential, which indicates that the stabilization mechanism is increased electrostatic repulsion from the positively charged MgAC coating. The optimal weight ratio between MgAC and iron was found to be 7.5:1. The MgAC coated nZVI exhibited higher reactivity for nitrate reduction with the observed first order rate constants increasing from 1.17 to 42.0h(-1), and Fe(0)-normalized rate constants from 0.124 to 43.8 h(-1) mg-Fe(0)(-1). Consequently, the MgAC coated nZVI showed increased feasibility, compared to uncoated nZVI, for application in remediation of subsurface contaminations; where high stability and mobility as well as high reactivity for degradation of contaminants is desired. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:748 / 755
页数:8
相关论文
共 50 条
  • [41] Strategies to enhance the stability of nanoscale zero-valent iron (NZVI) in continuous BrO3- reduction
    Hamid, Shanawar
    Abudanash, Damira
    Han, Seunghee
    Kim, Jong R.
    Lee, Woojin
    JOURNAL OF ENVIRONMENTAL MANAGEMENT, 2019, 231 : 714 - 725
  • [42] Phosphorous removal by nanoscale zero-valent iron (nZVI) and chitosan-coated nZVI (CS-nZVI)
    Shanableh, A.
    Darwish, N.
    Bhattacharjee, S.
    Al-Khayyat, G.
    Khalil, M.
    Mousa, M.
    Tayara, A.
    Al-Samarai, M.
    DESALINATION AND WATER TREATMENT, 2020, 184 : 282 - 291
  • [43] The influence of polyelectrolyte modification on nanoscale zero-valent iron (nZVI): Aggregation, sedimentation, and reactivity with Ni(II) in water
    Liu, Jing
    Liu, Airong
    Zhang, Wei-xian
    CHEMICAL ENGINEERING JOURNAL, 2016, 303 : 268 - 274
  • [44] Mutual effect of U(VI) and phosphate on the reactivity of nanoscale zero-valent iron (nZVI) for their co-removal
    Zheng, Huiling
    Ren, Xuemei
    Zhang, Xiaodong
    Song, Gang
    Chen, Diyun
    Chen, Changlun
    JOURNAL OF MOLECULAR LIQUIDS, 2020, 297
  • [45] Reactivity of nano zero-valent iron (nZVI) and Ni-modified nano zero-valent iron (Ni-nZVI) stabilized with carboxymethylcellulose towards chlorinated hydrocarbons
    Agrawal, Abinash
    Kimmel, Elizabeth
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2016, 251
  • [46] Degradation of trichloroethene by nanoscale zero-valent iron (nZVI) and nZVI activated persulfate in the absence and presence of EDTA
    Dong, Haoran
    He, Qi
    Zeng, Guangming
    Tang, Lin
    Zhang, Lihua
    Xie, Yankai
    Zeng, Yalan
    Zhao, Feng
    CHEMICAL ENGINEERING JOURNAL, 2017, 316 : 410 - 418
  • [47] Facile Auto-Combustion Synthesis and Characterization of Stable Amorphous Nanoscale Zero-Valent Iron (nZVI)
    R. Pillai
    Ramdas Balan
    I. C. Lekshmi
    K. Milina
    International Journal of Self-Propagating High-Temperature Synthesis, 2021, 30 : 251 - 256
  • [48] Facile Auto-Combustion Synthesis and Characterization of Stable Amorphous Nanoscale Zero-Valent Iron (nZVI)
    Pillai, R.
    Balan, Ramdas
    Lekshmi, I. C.
    Milina, K.
    INTERNATIONAL JOURNAL OF SELF-PROPAGATING HIGH-TEMPERATURE SYNTHESIS, 2021, 30 (04) : 251 - 256
  • [49] Reductive degradation of nitrobenzene in aqueous solution by zero-valent iron
    Mu, Y
    Yu, HQ
    Zheng, JC
    Zhang, SJ
    Sheng, GP
    CHEMOSPHERE, 2004, 54 (07) : 789 - 794
  • [50] Stabilization of nanoscale zero-valent iron (nZVI) with modified biochar for Cr(VI) removal from aqueous solution
    Dong, Haoran
    Deng, Junmin
    Xie, Yankai
    Zhang, Cong
    Jiang, Zhao
    Cheng, Yujun
    Hou, Kunjie
    Zeng, Guangming
    JOURNAL OF HAZARDOUS MATERIALS, 2017, 332 : 79 - 86