Microstructure and oxidation resistance of C-AlPO4-mullite coating prepared by hydrothermal electrophoretic deposition for SiC-C/C composites

被引:26
|
作者
Wang, Kai-Tong [1 ]
Cao, Li-Yun [1 ]
Huang, Jian-Feng [1 ]
Fei, Jie [1 ]
Zhang, Bo-Ye [1 ]
机构
[1] Shaanxi Univ Sci & Technol, Sch Mat Sci & Engn, Minist Educ, Key Lab Auxiliary Chem & Technol Chem Ind, Xian 710021, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
Mullite; Carbon/carbon composites; C-AlPO4; Hydrothermal electrophoretic deposition; CARBON/CARBON COMPOSITES; ANTIOXIDATION PROPERTY; PROTECTION; TEMPERATURES; HA;
D O I
10.1016/j.ceramint.2012.07.024
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Oxidation resistant C-AlPO4-mullite coating for SiC pre-coated carbon/carbon composites (SiC-C/C) was prepared by a novel hydrothermal electrophoretic deposition process. The phase composition, surface and cross-section microstructure of the as-prepared multi-layer coatings were characterized by X-ray Diffraction (XRD), scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). The influence of deposition voltage on phase composition, microstructure and oxidation resistance of the as-prepared coatings was particularly investigated. Results show that the outer layer coating mainly composed of C-AlPO4 and mullite phase can be achieved after the hydrothermal electrophoretic deposition. The thickness, density and anti-oxidation property of the C-AlPO4-mullite coating was improved with the increase of deposition voltage from 160 V to 200 V. The multi-layer coating prepared at a voltage of 200 V exhibit excellent anti-oxidation property, which can effectively protect C/C composites from oxidation in air at 1773 K for 324 h with a weight loss of 1.01%. The failure of the multi-layer coatings is due to the generation of cross-holes in the coating, which cannot be self-cured by the metaphosphate and silicate glass layer after long time oxidation at 1773 K. (C) 2012 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:1037 / 1044
页数:8
相关论文
共 50 条
  • [21] Effects of deposition temperature on microstructure of laminated (SiC-C) matrix composites
    K. A. Appiah
    Z. L. Wang
    W. J. Lackey
    Journal of Materials Science, 2000, 35 : 1979 - 1984
  • [22] Influence of Deposition Voltage on the SiCn-MoSi2 Coating for C/C Composites Prepared by a Hydrothermal Electrophoretic Deposition Process
    Wang Bo
    Huang Jian-Feng
    Liu Miao
    Cao Li-Yun
    Wu Jian-Peng
    JOURNAL OF INORGANIC MATERIALS, 2010, 25 (12) : 1291 - 1297
  • [23] ZrSiO4/SiC Oxidation Protective Coating for Carbon/Carbon Composites Prepared by Hydrothermal Electrophoretic Deposition
    Liu Jia
    Huang Jian-feng
    Cao Li-yun
    Xin Yu
    HIGH-PERFORMANCE CERAMICS VII, PTS 1 AND 2, 2012, 512-515 : 1070 - 1073
  • [24] Electrophoretic deposition of mullite based oxygen diffusion systems on C/C-Si-SiC composites
    Damjanovic, T.
    Argirusis, Chr.
    Jokanovic, B.
    Borchardt, G.
    Moritz, K.
    Mueller, E.
    Herbig, R.
    Weiss, R.
    ELECTROPHORETIC DEPOSITON: FUNDAMENTALS AND APPLICATIONS II, 2006, 314 : 201 - 206
  • [25] Oxidation resistance of SiC nanowires reinforced SiC coating prepared by a CVD process on SiC-coated C/C composites
    Qiang, Xinfa
    Li, Hejun
    Zhang, Nan
    Liu, Yunfan
    Tian, Song
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2018, 15 (05) : 1100 - 1109
  • [26] Microstructure and oxidation behavior of a novel bilayer (c-AlPO4-SiCw-mullite)/SiC coating for carbon fiber reinforced CMCs
    Chen, Pengju
    Xiao, Peng
    Li, Zhuan
    Liu, Zeyan
    Pu, Dongmei
    Li, Yang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (14) : 3988 - 3999
  • [27] Enhancement of the oxidation resistance of C/C composites by depositing SiC nanowires onto carbon fibers by electrophoretic deposition
    Wen, Shiqi
    Li, Kezhi
    Song, Qiang
    Shan, Yucai
    Li, Yunyu
    Li, Hejun
    Ma, Haili
    Journal of Alloys and Compounds, 2015, 618 : 336 - 342
  • [28] Enhancement of the oxidation resistance of C/C composites by depositing SiC nanowires onto carbon fibers by electrophoretic deposition
    Wen, Shiqi
    Li, Kezhi
    Song, Qiang
    Shan, Yucai
    Li, Yunyu
    Li, Hejun
    Ma, Haili
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 618 : 336 - 342
  • [29] Synthesis and electrophoretic deposition of an yttrium silicate coating system for oxidation protection of C/C-Si-SiC composites
    Argirusis, C
    Damjanovic, T
    Stojanovic, M
    Borchardt, G
    CURRENT RESEARCH IN ADVANCED MATERIALS AND PROCESSES, 2005, 494 : 451 - 456
  • [30] Microstructure and oxidation protection of borosilicate glass coating prepared by pulse arc discharge deposition for C/C composites
    Huang Jian-Feng
    Zhang Yong-Liang
    Zhu Kong-Jun
    Li Cui-Yan
    Cao Li-Yun
    Zhou Lei
    Ouyang Hai-Bo
    Zhang Bo-Ye
    Hao Wei
    Yao Chun-Yan
    CERAMICS INTERNATIONAL, 2015, 41 (03) : 4662 - 4667