Sub-surface microstructure of single and polycrystalline tungsten after high flux plasma exposure studied by TEM

被引:21
|
作者
Dubinko, A. [1 ,2 ]
Terentyev, D. [1 ]
Bakaeva, A. [1 ,2 ]
Hernandez-Mayoral, M. [3 ]
De Temmerman, G. [4 ]
Buzi, L. [5 ]
Noterdaeme, J. -M. [2 ]
Unterberg, B. [5 ]
机构
[1] SCK CEN, Inst Nucl Mat Sci, B-2400 Mol, Belgium
[2] Univ Ghent, Dept Appl Phys, B-9000 Ghent, Belgium
[3] CIEMAT, Div Mat, E-28040 Madrid, Spain
[4] ITER Org, Route Vinon Sur Verdon,CS 90 046, F-13067 St Paul Les Durance, France
[5] Forschungszentrum Julich, Inst Energie & Klimaforsch Plasmaphys, D-52425 Julich, Germany
关键词
High flux plasma; Tungsten; Single crystal; Dislocations; DEUTERIUM RETENTION; ENERGY;
D O I
10.1016/j.apsusc.2016.09.071
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
We have performed high flux plasma exposure of tungsten and subsequent microstructural characterization using transmission electron microscopy (TEM) techniques. The aim was to reveal the nanometric features in the sub-surface region as well as to compare the microstructural evolution in tungsten single crystal and ITER-relevant specification. In both types of samples, TEM examination revealed the formation of a dense dislocation network and dislocation tangles. The estimated dislocation density in the sub-surface region was of the order of 10(14) m(-2) and it gradually decreased with a depth position of the examined sample. Besides individual dislocation lines, networks and tangles, the interstitial dislocation loops have been observed in all examined samples only after the exposure. Contrary to that, examination of the pristine single crystal W and backside of the plasma-exposed samples did not reveal the presence of dislocation loops and tangles. This clearly proves that high flux plasma exposure induces severe plastic deformation in the sub-surface region irrespective of the presence of initial dislocations and sub-grains, and the formation of dislocation tangles, networks and interstitial loops is a co-product of thermal stress and intensive plasma particles uptake. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:330 / 339
页数:10
相关论文
共 50 条
  • [21] Surface morphology and deuterium retention in tungsten exposed to high flux D plasma at high temperatures
    Jia, Y. Z.
    De Temmerman, G.
    Luo, G. -N.
    Xu, H. Y.
    Li, C.
    Fu, B. Q.
    Liu, W.
    JOURNAL OF NUCLEAR MATERIALS, 2015, 457 : 213 - 219
  • [22] Effect of Surface Cracks and Texture on Residual Stresses in Tungsten after Exposure to Plasma
    Balash I.I.
    Kazantsev S.R.
    Shmakov A.N.
    Piminov P.A.
    Borin V.M.
    Bulletin of the Russian Academy of Sciences: Physics, 2023, 87 (05) : 611 - 614
  • [23] The effect of high-flux H plasma exposure with simultaneous transient heat loads on tungsten surface damage and power handling
    van Eden, G. G.
    Morgan, T. W.
    van der Meiden, H. J.
    Matejicek, J.
    Chraska, T.
    Wirtz, M.
    De Temmerman, G.
    NUCLEAR FUSION, 2014, 54 (12)
  • [24] Influence of tungsten microstructure and ion flux on deuterium plasma-induced surface modifications and deuterium retention
    Buzi, L.
    De Temmerman, G.
    Unterberg, B.
    Reinhart, M.
    Dittmar, T.
    Matveev, D.
    Linsmeier, Ch.
    Breuer, U.
    Kreter, A.
    Van Oost, G.
    JOURNAL OF NUCLEAR MATERIALS, 2015, 463 : 320 - 324
  • [25] Surface hardening induced by high flux plasma in tungsten revealed by nano-indentation
    Terentyev, D.
    Bakaeva, A.
    Pardoen, T.
    Favache, A.
    Zhurkin, E. E.
    JOURNAL OF NUCLEAR MATERIALS, 2016, 476 : 1 - 4
  • [26] Deuterium accumulation in tungsten under low-energy high-flux plasma exposure
    Grigorev P.Y.
    Dubinko V.I.
    Terentyev D.A.
    Bakaev A.V.
    Zhurkin E.E.
    Journal of Surface Investigation, 2014, 8 (02): : 234 - 238
  • [27] High-flux hydrogen irradiation-induced cracking of tungsten reproduced by low-flux plasma exposure
    Gao, L.
    Manhard, A.
    Jacob, W.
    von Toussaint, U.
    Balden, M.
    Schmid, K.
    NUCLEAR FUSION, 2019, 59 (05)
  • [28] Nanofatigue behaviour of single struts of cast A356.0 foam: cyclic deformation, nanoindent characteristics and sub-surface microstructure
    Schmahl, M.
    Maerten, A.
    Zaslansky, P.
    Fleck, C.
    MATERIALS & DESIGN, 2020, 195
  • [29] Thermal shock behaviour of tungsten after high flux H-plasma loading
    Wirtz, M.
    Linke, J.
    Pintsuk, G.
    De Temmerman, G.
    Wright, G. M.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 443 (1-3) : 497 - 501
  • [30] He2+ irradiation induced microstructure evolution in sub-surface layer of the coarse-grained tungsten accessed by synchrotron GIXRD and GISAXS
    Huang, W. J.
    Sun, M.
    Wen, W.
    Yang, J. F.
    Xie, Z. M.
    Liu, R.
    Wang, X. P.
    Wu, X. B.
    Liu, C. S.
    Fang, Q. F.
    APPLIED SURFACE SCIENCE, 2022, 593