High-Temperature Oxidation and Smelt Deposit Corrosion of Ni-Cr-Ti Arc-Sprayed Coatings

被引:8
|
作者
Matthews, S. [1 ]
Schweizer, M. [2 ,3 ]
机构
[1] Massey Univ, Sch Engn & Adv Technol, Auckland 0745, New Zealand
[2] Univ Auckland, Dept Chem & Mat Engn, Auckland Mail Ctr, Auckland 1142, New Zealand
[3] Aalen Univ Appl Sci, Dept Surface & Mat Technol, D-73430 Aalen, Germany
关键词
arc-sprayed microstructure; black liquor recovery boiler; high-temperature oxidation; Ni-Cr-Ti; smelt deposit corrosion;
D O I
10.1007/s11666-013-9939-2
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
High Cr content Ni-Cr-Ti arc-sprayed coatings have been extensively applied to mitigate corrosion in black liquor recovery boilers in the pulp and paper industry. In a previous article, the effects of key spray parameters on the coating's microstructure and its composition were investigated. Three coating microstructures were selected from that previous study to produce a dense, oxidized coating (coating A), a porous, low oxide content coating (coating B), and an optimized coating (coating C) for corrosion testing. Isothermal oxidation trials were performed in air at 550 and 900 A degrees C for 30 days. Additional trials were performed under industrial smelt deposits at 400 and 800 A degrees C for 30 days. The effect of the variation in coating microstructure on the oxidation and smelt's corrosion response was investigated through the characterization of the surface corrosion products, and the internal coating microstructural developments with time at high temperature. The effect of long-term, high-temperature exposure on the interaction between the coating and substrate was characterized, and the mechanism of interdiffusion was discussed.
引用
收藏
页码:932 / 946
页数:15
相关论文
共 50 条
  • [31] Effect of Al content on high temperature erosion properties of arc-sprayed FeMnCrAl/Cr3C2 coatings
    罗来马
    刘少光
    俞佳
    罗娟
    郦剑
    Transactions of Nonferrous Metals Society of China, 2010, 20 (02) : 201 - 206
  • [32] High temperature erosion properties of arc-sprayed coatings using various cored wires containing Ti-Al intermetallics
    Liu, Shao-Guang
    Wu, Jin-Ming
    Zhang, Sheng-Cai
    Rong, Shu-Jie
    Li, Zhi-Zhang
    WEAR, 2007, 262 (5-6) : 555 - 561
  • [33] High-Temperature Corrosion of HVAF-Sprayed Ni-Based Coatings for Boiler Applications
    Eklund, J.
    Phother, J.
    Sadeghi, E.
    Joshi, S.
    Liske, J.
    OXIDATION OF METALS, 2019, 91 (5-6): : 729 - 747
  • [34] High-Temperature Corrosion of HVAF-Sprayed Ni-Based Coatings for Boiler Applications
    J. Eklund
    J. Phother
    E. Sadeghi
    S. Joshi
    J. Liske
    Oxidation of Metals, 2019, 91 : 729 - 747
  • [35] Hot Corrosion Behavior of a High Velocity Arc-Sprayed Fe-Cr-B-C Coating
    Guo Wenmin
    Wu Yuping
    Li Gaiye
    Wang Qian
    He Zhihua
    Hong Sheng
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 : 456 - 459
  • [36] Hot Corrosion Behavior of a High Velocity Arc-Sprayed Fe-Cr-B-C Coating
    Guo WenminWu YupingLi GaiyeWang QianHe ZhihuaHong Sheng Hohai UniversityNanjing China
    稀有金属材料与工程, 2012, 41(S1) (S1) : 456 - 459
  • [37] Study of High Temperature Oxidation Behavior of Wire Arc Sprayed Coatings
    Kant, Shashi
    Kumar, Manoj
    Chawla, Vikas
    Singh, Supreet
    MATERIALS TODAY-PROCEEDINGS, 2020, 21 : 1741 - 1748
  • [38] High-temperature Oxidation Behavior and Mechanism of Hybrid Twin-wire Supersonic Arc Sprayed Coatings
    Ren D.
    Tang X.
    Li L.
    Zhang Y.
    Jiang X.
    Xu Z.
    Zeng J.
    Surface Technology, 2024, 53 (04): : 78 - 88
  • [39] Corrosion, oxidation and high-temperature tribological properties of Ti-B-N coatings
    Asempah, Isaac
    Yu, Lihua
    Ju, Hongbo
    Yu, Dian
    Xu, Junhua
    Miao, Ran
    SURFACE ENGINEERING, 2019, 35 (08) : 661 - 669
  • [40] Microstructure and high-temperature oxidation behavior of wire-arc sprayed Fe-based coatings
    Li, Ran
    Zhou, Zheng
    He, Dingyong
    Zhao, Lidong
    Song, Xiaoyan
    SURFACE & COATINGS TECHNOLOGY, 2014, 251 : 186 - 190